Patent US5031127A successfully refreshed from Google Patents.
← Back to Patent Explorer
US5031127A Expired / Lapsed US ⏱️ 0.0 years remaining

Molten injection-molding method

Assignee: Shibaura Machine Co Ltd
•
Filing: 1988-11-18
•
Granted: 1991-07-09
•
Expires: 2008-11-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A molten injection-molding method is applicable to any system of dividing a molded product form model into micro-elements and analyzing a molten material flow behavior within the mold by the use of numerical analytic techniques that include the finite element method, boundary element method, difference method, and FAN method, among others. First, the entire length of time required for the process of filling the mold with a molten material is divided into an arbitrary number of intervals, representing the filling progress in each individual time interval in an equitime curve diagram. This is followed by next not only deriving the distance segmented by each pair of adjacent equitime curves based on interrelations of the divided micro-element and equitime curves, but also computing the individual filling speeds, and then making a graphic display on display equipment of the variations in these filling speeds over an entire filling cycle, in order to evaluate, and find, the filling speeds at which an optimum mold filling cycle may be achieved.

Inventors

  • 👤 Shigeru Fujita
  • 👤 Susumu Harada

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 15:16
CPC Classifications
B; B29; B29C; B29C45/00; B29C45/17; B29C45/76; B29C45/77; B29C45/7693; B29C45/766; G; G01; G01N; G01N11/00; G01N11/02

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 151 words
A method for injection molding a product, comprising the steps of: (a) simulating an injection-molded product formed in a mold filled at a filling speed during a fill cycle with molten material by forming a model of the product; (b) generating a model pattern of the model by subdividing the model into a plurality of elements; (c) dividing the fill cycle into a plurality of successive time intervals; (d) generating a fill pattern of equitime curves, each representative of the advancement over time of the molten material through the mold for respective successive time intervals; (e) superimposing the fill pattern over the model pattern; (f) generating from the superimposed patterns on individual filling speed for each time interval; (g) visually displaying the individual filling speed over the fill cycle to determine optimum filling speed conditions; and (h) controlling an injection molding operation in accordance with the determined optimum filling speed conditions.
Claim 2
Independent Claim 151 words
A method for injection molding a product, comprising the steps of: (a) simulating an injection-molded product formed in a mold filled at a filling speed during a fill cycle with molten material by forming a model of the product; (b) generating a model pattern of the model by subdividing the model into a plurality of elements; (c) dividing the fill cycle into a plurality of successive time intervals; (d) generating a fill pattern of equitime curves, each representative of the advancement over time of the molten material through the mold for respective successive time intervals; (e) superimposing the fill pattern over the model pattern; (f) generating from the superimposed patterns on individual filling speed for each time interval; (g) visually displaying the individual filling speed over the fill cycle to determine optimum filling speed conditions; and (h) controlling an injection molding operation in accordance with the determined optimum filling speed conditions.
Claim 3
Dependent Claim 33 words
The method according to claim 1, wherein step (b) is performed by forming each element with linear boundary lines, and wherein step (d) is performed by forming each equitime curve with linear segments.
Claim 4
Dependent Claim 46 words
The method according to claim 1, wherein step (f) is performed by generating a filling flow curve over the superimposed patterns, said filling flow curve representing the flow of the molten material from a mold gate through the mold to a selected location in the mold.
Claim 5
Dependent Claim 91 words
The method according to claim 3, wherein step (f) is performed by selecting a first starting point within a first element associated with a first equitime curve having a first linear segment; determine points of intersection on boundary lines of adjacent second and third elements by extending a normal line through said first point and perpendicular to said first linear segment; interconnecting the intersection points; and repeating said determining step with each intersection point as a starting point until a point of intersection corresponds to the location of the mold gate.
Claim 6
Dependent Claim 51 words
The method according to claim 4, wherein step (f) is further performed by locating crossover points between the filling flow curve and the equitime curves; measuring individual mean linear distances between adjacent pairs of cross-over points; and determining individual filling speeds from the individual means linear distances and the time intervals.
Claim 7
Dependent Claim 68 words
The method according to claim 3, wherein step (f) is performed by determining each area bounded between each adjacent pair of equitime curves; determining each means length of individual equitime curves; determining individual mean linear distances between each adjacent pair of equitime curves as a function of each area and each mean length; and determining individual filling speeds from the individual mean linear distances and the time intervals.
Claim 8
Dependent Claim 110 words
The method according to claim 3, wherein step (f) is further performed by selecting a first gate point in a first element associated with a first equitime curve having a first linear segment; selecting a second point in a second element associated with a second equitime curve having a second linear segment; interconnecting the first and second points; determining a point of intersection with a third element by extending a normal line through said second point and perpendicular to said first segment; and repeating said determining step with each intersection point as a starting point until a point on the superimposed patterns corresponds to said selected location in the mold.
Claim 9
Dependent Claim 129 words
The method according to claim 3, wherein step (f) is further performed by selecting a first starting point on a first linear segment of a first equitime curve; extending a first normal line through said first point and perpendicular to an adjacent second linear segment of a second equitime curve; extending a second normal line through said first point and perpendicular to said first linear segment; determining a second point of intersection on the second equitime curve by extending a bisecting line that bisects the angle included between said first and second normal lines; interconnecting the first and second points; and repeating said extending steps with each point of intersection as a starting point until a point on the superimposed patterns corresponds to said selected location in the mold.
Claim 10
Dependent Claim 32 words
The method according to claim 1; and further comprising the step of visually displaying, simultaneously with step (g), a profile of input filling speed settings for the mold over the fill cycle.
Claim 11
Dependent Claim 29 words
The method according to claim 1; and further comprising the step of visually displaying, simultaneously with step (g), wall thickness variations at all the elements over the fill cycle.
Claim 12
Dependent Claim 31 words
The method according to claim 1; and further comprising the step of visually displaying, simultaneously with step (g), temperature settings of mold plates at all the elements over the fill cycle.

References Cited (Backward Citations)

US4326255A Cited
US4797842A Cited
US4787057A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-07-08 1995-01-07 1995-07-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-07-08 1999-01-07 1999-07-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-07-08 2003-01-07 2003-07-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag