Impact resistant thermoplastic resin composition

Assignee: Mitsubishi Chemical Corp
•
Filing: 1990-01-17
•
Granted: 1991-06-25
•
Expires: 2010-01-17
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A composition comprising a polyphenylene ether, a polyamide resin and a compound having an unsaturated group and a polar group in combination in the same molecule kneaded therein, and optionally an impact resistance improving material kneaded in said kneaded product. Impact resistance can be greatly improved as compared with the composition having the all components kneaded at the same time.

Inventors

  • 👤 Kiyoji Takagi
  • 👤 Koji Nishida

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 22:55
CPC Classifications
C; C08; C08L; C08L71/00; C08L71/08; C08L71/10; C08L71/12; C08L71/123; C08L77/00; Y; Y10; Y10S; Y10S525/00; Y10S525/905

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 109 words
A resin composition comprising: (A) 10 to 70% by weight of an intermediate composition obtained by melting and kneading: (A 1 ) 75 to 99% by weight of a polyphenylene ether resin; (A 2 ) 0.1 to 19.9% by weight of a polyamide resin; (A 3 ) 0.01 to 10% by weight of a compound having an unsaturated group and a polar group in the same molecule in combination, and (A 4 ) 0 to 20% by weight of an impact resistance improving material, (B) 30 to 90% by weight of a polyamide resin, and (C) 0 to 35% by weight of an impact resistance improving material kneaded therein.
Claim 2
Dependent Claim 109 words
A resin composition comprising: (A) 10 to 70% by weight of an intermediate composition obtained by melting and kneading: (A 1 ) 75 to 99% by weight of a polyphenylene ether resin; (A 2 ) 0.1 to 19.9% by weight of a polyamide resin; (A 3 ) 0.01 to 10% by weight of a compound having an unsaturated group and a polar group in the same molecule in combination, and (A 4 ) 0 to 20% by weight of an impact resistance improving material, (B) 30 to 90% by weight of a polyamide resin, and (C) 0 to 35% by weight of an impact resistance improving material kneaded therein.
Claim 3
Dependent Claim 53 words
The resin composition according to claim 1, wherein the compound (A 3 ) having an unsaturated group and a polar group within the same molecule is at least one selected from unsaturated carboxylic acids, unsaturated esters, unsaturated acid anhydrides, unsaturated amines, unsaturated amides, unsaturated epoxy compounds, unsaturated alcohols and unsaturated isocyanic acid esters.
Claim 4
Dependent Claim 40 words
The resin composition according to claim 1, wherein the compound (A 3 ) having an unsaturated group and a polar group in the same molecule is at least one selected from maleic anhydride, maleic acid, itaconic anhydride and itaconic acid.
Claim 5
Dependent Claim 109 words
A resin composition comprising: (A) 10 to 70% by weight of an intermediate composition obtained by melting and kneading: (A 1 ) 75 to 99% by weight of a polyphenylene ether resin; (A 2 ) 0.1 to 19.9% by weight of a polyamide resin; (A 3 ) 0.01 to 10% by weight of a compound having an unsaturated group and a polar group in the same molecule in combination; and (A 4 ) 1 to 18% by weight of an impact resistance improving material, (B) 20 to 70% by weight of a polyamide resin, and (C) 1 to 30% by weight of an impact resistance improving material kneaded therein.
Claim 6
Dependent Claim 109 words
A resin composition comprising: (A) 10 to 70% by weight of an intermediate composition obtained by melting and kneading: (A 1 ) 75 to 99% by weight of a polyphenylene ether resin; (A 2 ) 0.1 to 19.9% by weight of a polyamide resin; (A 3 ) 0.01 to 10% by weight of a compound having an unsaturated group and a polar group in the same molecule in combination; and (A 4 ) 1 to 18% by weight of an impact resistance improving material, (B) 20 to 70% by weight of a polyamide resin, and (C) 1 to 30% by weight of an impact resistance improving material kneaded therein.
Claim 7
Dependent Claim 30 words
The resin composition according to claim 4, wherein the impact resistance improving materials (A 4 ) and (C) are elastomers having a tensile modulus of 5000 Kg/cm 2 or less.
Claim 8
Dependent Claim 53 words
The resin composition according to claim 4, wherein the compound (A 3 ) having an unsaturated group and a polar group within the same molecule is at least one selected from unsaturated carboxylic acids, unsaturated esters, unsaturated acid anhydrides, unsaturated amines, unsaturated amides, unsaturated epoxy compounds, unsaturated alcohols and unsaturated isocyanic acid esters.
Claim 9
Dependent Claim 40 words
The resin composition according to claim 4, wherein the compound (A 3 ) having an unsaturated group and a polar group in the same molecule is at least one selected from maleic anhydride, maleic acid, itaconic anhyride and itaconic acid.
Claim 10
Dependent Claim 20 words
A resin composition according to claim 4 wherein component A 4 is present in an amount of 2-15% by weight.

References Cited (Backward Citations)

US4839425A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-06-24 1994-12-24 1995-06-25 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-06-24 1998-12-24 1999-06-25 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-06-24 2002-12-24 2003-06-25 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag