Optical recording media

Assignee: Mitsui Chemicals Inc
•
Filing: 1989-10-27
•
Granted: 1991-02-19
•
Expires: 2009-10-27
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Optical recording media disclosed herein are excellent in recording sensitivity as well as in the adhesion of the substrate to the recording layer, said substrate consisting of a random copolymer of ethylene and a cycloolefin and having a specific structure.

Inventors

  • 👤 Hisaharu Toibana
  • 👤 Mitsuyuki Kuroiwa
  • 👤 Takeshi Minoda
  • 👤 Akira Todo

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 11:28
CPC Classifications
G; G11; G11B; G11B7/00; G11B7/24; G11B7/241; G11B7/242; G11B7/243; G11B7/2433; G11B7/252; G11B7/253; G11B7/2533; G11B7/2538; G11B2007/24302; G11B2007/24306; G11B2007/24316; G11B2007/24318; G11B2007/24328; Y; Y10; Y10S; Y10S430/00; Y10S430/146

Claims Analysis

Total Claims: 30
Claim 1
Independent Claim 161 words
An optical recording medium comprising a substrate and a recording layer formed thereon, in which the recording layer is irradiated with beam of energy to form thereon pits corresponding to given pieces of information and thereby record the pieces of information, said recording layer being a thin film consisting essentially of Te and additionally containing Cr, C and H and said substrate comprising a cycloolefin random copolymer composed of a ethylene unit and a cycloolefin unit derived from the following general formula [I] ##STR84## wherein n is 0 or a positive integer, R 1 to R 12 are the same or difference, and represent each hydrogen atom, a halogen atom or a hydrocarbon group, provided that R 9 to R 12 , when taken together, may form a mono-or poly-cyclic hydrocarbon ring which may optionally have double bond or bonds, or R 9 and R 10 or R 11 and R 12 , when taken together, may form an alkylidene group.
Claim 2
Dependent Claim 161 words
An optical recording medium comprising a substrate and a recording layer formed thereon, in which the recording layer is irradiated with beam of energy to form thereon pits corresponding to given pieces of information and thereby record the pieces of information, said recording layer being a thin film consisting essentially of Te and additionally containing Cr, C and H and said substrate comprising a cycloolefin random copolymer composed of a ethylene unit and a cycloolefin unit derived from the following general formula [I] ##STR84## wherein n is 0 or a positive integer, R 1 to R 12 are the same or difference, and represent each hydrogen atom, a halogen atom or a hydrocarbon group, provided that R 9 to R 12 , when taken together, may form a mono-or poly-cyclic hydrocarbon ring which may optionally have double bond or bonds, or R 9 and R 10 or R 11 and R 12 , when taken together, may form an alkylidene group.
Claim 3
Dependent Claim 28 words
The optical recording medium as claimed in claim 1 wherein the substrate comprises a cycloolefin random copolymer having a softening temperature (TMA) of not lower than 70° C.
Claim 4
Dependent Claim 35 words
The optical recording medium as claimed in claim 1 wherein the contents of Cr in the recording layer is from 0.1 to 40 atom % based on the total atoms present in the recording layer.
Claim 5
Dependent Claim 34 words
The optical recording medium as claimed in claim 1 wherein the contents of C in the recording layer is less than 40 atom % based on the total atoms present in the recording layer.
Claim 6
Dependent Claim 35 words
The optical recording medium as claimed in claim 1 wherein the contents of H in the recording layer is from 1 to 40 atom % based on the total atoms present in the recording layer.
Claim 7
Dependent Claim 24 words
The optical recording medium as claimed in claim 1 wherein the film thickness of the recording layer is from 100 Å to 1 μm.
Claim 8
Dependent Claim 277 words
An optical recording medium comprising a substrate and a recording layer formed thereon, in which the recording layer is irradiated with beam of energy to form thereon pits corresponding to given pieces of information and thereby record the pieces of information, said recording layer being a thin film consisting essentially of Te and additionally containing Cr, C and H and said substrate consisting of a cycloolefin random copolymer composition comprising: [A] a cycloolefin random copolymer composed of an ethylene unit and a cycloolefin unit derived from the following general formula [I] and having an intrinsic viscosity [72 ] of from 0.05 to 10 dl/g as measured at 135° C. in decalin and a softening temperature (TMA) of not lower than 70° C., and [B] a cycloolefin random copolymer composed of an ethylene unit and a cycloolefin unit derived from the following general formula [I] and having an intrinsic viscosity [η] of from 0.05 to 5 dl/g as measured at 135° C. in decalin and a softening temperature (TMA) of below 70° C., in such a proportion that the ratio by weight of the component [A] to the component [B] is in the range of from 100/0.1 to 100/10, ##STR85## wherein n is 0 or a positive integer, R 1 to R 12 are the same or difference, and represent each hydrogen atom, a halogen atom or a hydrocarbon group, provided that R 9 to R 12 , when taken together, may form a mono- or poly-cyclic hydrocarbon ring which may optionally have double bond or bonds, or R 9 and R 10 or R 11 and R 12 , when taken together, may form an alkylidene group.
Claim 9
Dependent Claim 277 words
An optical recording medium comprising a substrate and a recording layer formed thereon, in which the recording layer is irradiated with beam of energy to form thereon pits corresponding to given pieces of information and thereby record the pieces of information, said recording layer being a thin film consisting essentially of Te and additionally containing Cr, C and H and said substrate consisting of a cycloolefin random copolymer composition comprising: [A] a cycloolefin random copolymer composed of an ethylene unit and a cycloolefin unit derived from the following general formula [I] and having an intrinsic viscosity [72 ] of from 0.05 to 10 dl/g as measured at 135° C. in decalin and a softening temperature (TMA) of not lower than 70° C., and [B] a cycloolefin random copolymer composed of an ethylene unit and a cycloolefin unit derived from the following general formula [I] and having an intrinsic viscosity [η] of from 0.05 to 5 dl/g as measured at 135° C. in decalin and a softening temperature (TMA) of below 70° C., in such a proportion that the ratio by weight of the component [A] to the component [B] is in the range of from 100/0.1 to 100/10, ##STR85## wherein n is 0 or a positive integer, R 1 to R 12 are the same or difference, and represent each hydrogen atom, a halogen atom or a hydrocarbon group, provided that R 9 to R 12 , when taken together, may form a mono- or poly-cyclic hydrocarbon ring which may optionally have double bond or bonds, or R 9 and R 10 or R 11 and R 12 , when taken together, may form an alkylidene group.
Claim 10
Dependent Claim 35 words
The optical recording medium as claimed in claim 7 wherein the contents of Cr in the recording layer is from 0.1 to 40 atom % based on the total atoms present in the recording layer.
Claim 11
Dependent Claim 34 words
The optical recording medium as claimed in claim 7 wherein the contents of C in the recording layer is less than 40 atom % based on the total atoms present in the recording layer.
Claim 12
Dependent Claim 35 words
The optical recording medium as claimed in claim 7 wherein the contents of H in the recording layer is from 1 to 40 atom % based on the total atoms present in the recording layer.
Claim 13
Dependent Claim 24 words
The optical recording medium as claimed in claim 7 wherein the film thickness of the recording layer is from 100 Å to 1 μm.
Claim 14
Dependent Claim 248 words
An optical recording medium of improved sensitivity comprising a substrate and a recording layer in which the recording layer has improved adhesion to the substrate and improved oxidation resistance and in which the recording layer is irradiated with a beam of energy to form thereon pits corresponding to given pieces of information and thereby record the pieces of information, said recording layer being a thin film consisting essentially of Te, Cr, C and H, wherein Cr is present in an amount of from 0.1 to 40%, based on the total atoms present in the recording layer, C is present in an amount of less than 40 atom %, based on the total atoms present in the recording layer, and H is present in an amount of from 1 to 40 atom %, based on the total atoms present in the recording layer, and said substrate comprises a cycloolefin random copolymer composed of an ethylene unit and a cycloolefin unit from a cycloolefin of the general formula (I) ##STR86## wherein n is 0 or a positive integer, R 1 to R 12 are the same or different and each represents a hydrogen atom, a halogen atom or a hydrocarbon group, provided that R 9 to R 12 , when taken together, may form a mono- or poly-cyclic hydrocarbon ring which may optionally have a double bond or bonds, or R 9 and R 10 or R 11 and R 12 , when taken together, may form an alkylidene group.
Claim 15
Dependent Claim 248 words
An optical recording medium of improved sensitivity comprising a substrate and a recording layer in which the recording layer has improved adhesion to the substrate and improved oxidation resistance and in which the recording layer is irradiated with a beam of energy to form thereon pits corresponding to given pieces of information and thereby record the pieces of information, said recording layer being a thin film consisting essentially of Te, Cr, C and H, wherein Cr is present in an amount of from 0.1 to 40%, based on the total atoms present in the recording layer, C is present in an amount of less than 40 atom %, based on the total atoms present in the recording layer, and H is present in an amount of from 1 to 40 atom %, based on the total atoms present in the recording layer, and said substrate comprises a cycloolefin random copolymer composed of an ethylene unit and a cycloolefin unit from a cycloolefin of the general formula (I) ##STR86## wherein n is 0 or a positive integer, R 1 to R 12 are the same or different and each represents a hydrogen atom, a halogen atom or a hydrocarbon group, provided that R 9 to R 12 , when taken together, may form a mono- or poly-cyclic hydrocarbon ring which may optionally have a double bond or bonds, or R 9 and R 10 or R 11 and R 12 , when taken together, may form an alkylidene group.
Claim 16
Dependent Claim 28 words
The optical recording medium as claimed in claim 12 wherein the substrate comprises a cycloolefin random copolymer having a softening temperature (TMA) of not lower than 70° C.
Claim 17
Dependent Claim 35 words
The optical recording medium as claimed in claim 1 wherein the content of Cr in the recording layer is from 0.5 to 10 atom %, based on the total atoms present in the recording layer.
Claim 18
Dependent Claim 35 words
The optical recording medium as claimed in claim 14 wherein the content of Cr in the recording layer is from 1 to 4 atom %, based on the total atoms present in the recording layer.
Claim 19
Dependent Claim 35 words
The optical recording medium as claimed in claim 12 wherein the content of C in the recording layer is from 3 to 20 atom %, based on the total atoms present in the recording layer.
Claim 20
Dependent Claim 35 words
The optical recording medium as claimed in claim 12 wherein the content of H in the recording layer is from 3 to 25 atom %, based on the total atoms present in the recording layer.
Claim 21
Dependent Claim 24 words
The optical recording medium as claimed in claim 12 wherein the film thickness of the recording layer is from 100 Å to 1 μm.
Claim 22
Dependent Claim 34 words
The optical recording medium as claimed in claim 12 wherein the content of Te in the recording layer is at least 87 atom %, based on the total atoms present in the recording layer.
Claim 23
Dependent Claim 364 words
An optical recording medium of improved sensitivity comprising a substrate and a recording layer in which the recording layer has improved adhesion to the substrate and improved oxidation resistance and in which the recording layer is irradiated with a beam of energy to form thereon pits corresponding to given pieces of information and thereby record the pieces of information, said recording layer being a thin film consisting essentially of Te, Cr, C and H, wherein Cr is present in an amount of from 0.1 to 40 atom %, based on the total atoms present in the recording layer, C is present in an amount of less than 40 atom %, based on the total atoms present in the recording layer, and H is present in an amount of from 1 to 40 atom %, based on the total atoms present in the recording layer, and said substrate comprises a cycloolefin random copolymer composition comprising: [A] a cycloolefin random copolymer composed of an ethylene unit and a cycloolefin unit from a cycloolefin of the general formula (I) ##STR87## wherein n is 0 or a positive integer, R 1 to R 12 are the same or different and each represents a hydrogen atom, a halogen atom or a hydrocarbon group, provided that R 9 to R 12 , when taken together, may form a mono- or poly-cyclic hydrocarbon ring which may optionally have a double bond or bonds, or R 9 and R 10 or R 11 and R 12 , when taken together, may form an alkylidene group, and having an intrinsic viscosity [η] of from 0.05 to 10 dl/g as measured at 135° C. in decalin and a softening temperature (TMA) of not lower than 70° C., and (B) a cycloolefin random copolymer composed of an ethylene unit and a cycloolefin unit from a cycloolefin of said general formula (I), and having an intrinsic viscosity [η] of from 0.05 to 5 dl/g as measured at 135° C. in decalin and a softening temperature (TMA) of below 70° C., in such a proportion that the ratio by weight of the component (A) to the component (B) is in the range of from 100/0.1 to 100/10.
Claim 24
Dependent Claim 364 words
An optical recording medium of improved sensitivity comprising a substrate and a recording layer in which the recording layer has improved adhesion to the substrate and improved oxidation resistance and in which the recording layer is irradiated with a beam of energy to form thereon pits corresponding to given pieces of information and thereby record the pieces of information, said recording layer being a thin film consisting essentially of Te, Cr, C and H, wherein Cr is present in an amount of from 0.1 to 40 atom %, based on the total atoms present in the recording layer, C is present in an amount of less than 40 atom %, based on the total atoms present in the recording layer, and H is present in an amount of from 1 to 40 atom %, based on the total atoms present in the recording layer, and said substrate comprises a cycloolefin random copolymer composition comprising: [A] a cycloolefin random copolymer composed of an ethylene unit and a cycloolefin unit from a cycloolefin of the general formula (I) ##STR87## wherein n is 0 or a positive integer, R 1 to R 12 are the same or different and each represents a hydrogen atom, a halogen atom or a hydrocarbon group, provided that R 9 to R 12 , when taken together, may form a mono- or poly-cyclic hydrocarbon ring which may optionally have a double bond or bonds, or R 9 and R 10 or R 11 and R 12 , when taken together, may form an alkylidene group, and having an intrinsic viscosity [η] of from 0.05 to 10 dl/g as measured at 135° C. in decalin and a softening temperature (TMA) of not lower than 70° C., and (B) a cycloolefin random copolymer composed of an ethylene unit and a cycloolefin unit from a cycloolefin of said general formula (I), and having an intrinsic viscosity [η] of from 0.05 to 5 dl/g as measured at 135° C. in decalin and a softening temperature (TMA) of below 70° C., in such a proportion that the ratio by weight of the component (A) to the component (B) is in the range of from 100/0.1 to 100/10.
Claim 25
Dependent Claim 34 words
The optical recording medium as claimed in claim 20 wherein the content of Cr in the recording layer is from 0.5 to 10 atom %, based on the total atoms in the recording layer.
Claim 26
Dependent Claim 34 words
The optical recording medium as claimed in claim 21 wherein the content of Cr in the recording layer is from 1 to 4 atom %, based on the total atoms in the recording layer.
Claim 27
Dependent Claim 35 words
The optical recording medium as claimed in claim 20 wherein the content of C in the recording layer is from 3 to 20 atom %, based on the total atoms present in the recording layer.
Claim 28
Dependent Claim 35 words
The optical recording medium as claimed in claim 20 wherein the content of H in the recording layer is from 3 to 25 atom %, based on the total atoms present in the recording layer.
Claim 29
Dependent Claim 24 words
The optical recording medium as claimed in claim 20 wherein the film thickness of the recording layer is from 100 Å to 1 μm.
Claim 30
Dependent Claim 34 words
The optical recording medium as claimed in claim 20, wherein the content of Te in the recording layer is at least 87 atom %, based on the total atoms present in the recording layer.

References Cited (Backward Citations)

US4388400A Cited
US4433340A Cited
US4702991A Cited
US4874808A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-02-18 1994-08-20 1995-02-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-02-18 1998-08-20 1999-02-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-02-18 2002-08-20 2003-02-19 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag