Claims Analysis
Total Claims: 33
Claim 1
Independent Claim
123 words
A method of coating small solid particles with a conformal coating of a protective material, said method comprising the steps of: (a) contacting the small particles with a vapor phase precursor coating material in a first multi-stage fluid bed reactor, such that the particles adsorb at least a portion of said precursor coating material; (b) passing the particles having precursor coating material adsorbed thereon to a second multi-stage fluid bed reactor wherein said precursor coating material is oxidized to a protective material; (c) passing said coated particles to a cooling zone; and (d) recirculating the solids through the first and second multi-stage fluid bed reactors and the cooling zone, an appropriate number of times, to achieve a thicker coating of the protective material.
Claim 2
Independent Claim
123 words
A method of coating small solid particles with a conformal coating of a protective material, said method comprising the steps of: (a) contacting the small particles with a vapor phase precursor coating material in a first multi-stage fluid bed reactor, such that the particles adsorb at least a portion of said precursor coating material; (b) passing the particles having precursor coating material adsorbed thereon to a second multi-stage fluid bed reactor wherein said precursor coating material is oxidized to a protective material; (c) passing said coated particles to a cooling zone; and (d) recirculating the solids through the first and second multi-stage fluid bed reactors and the cooling zone, an appropriate number of times, to achieve a thicker coating of the protective material.
Claim 3
Dependent Claim
18 words
The process of claim 1 wherein the fluidizing gas in the first multi-stage fluid bed reactor is nitrogen.
Claim 4
Dependent Claim
15 words
The process of claim 1 wherein the precursor coating material is a precursor of alumina.
Claim 5
Dependent Claim
13 words
The process of claim 3 wherein the precursor of alumina is trimethyl aluminum.
Claim 6
Dependent Claim
30 words
The process of claim 3 wherein the precursor of alumina is AlR x (OR') 3-x wherein 0<2x<3 and x is an integer, and R and R' are lower alkyl groups.
Claim 7
Dependent Claim
37 words
The process of claim 1 wherein each stage of the first multi-stage fluid bed reactor is essentially isothermal, with temperatures ranging from about 25° C. in the first stage to about 500° C. in the last stage.
Claim 8
Dependent Claim
18 words
The process of claim 1 wherein the fluidizing gas in the second multi-stage fluid bed reactor is air.
Claim 9
Dependent Claim
37 words
The process of claim 1 wherein each stage of the second multi-stage fluid bed reactor is essentially isothermal, with temperatures ranging from about 25° C. in the first stage to about 750° C. in the last stage.
Claim 10
Dependent Claim
61 words
The process cf claim 1 wherein the cooling zone is a duct where the hot powder from the last stage of the second reactor is contacted with a cocurrent stream of cool air of controlled psychrometric properties, the residence time of the solids in the duct being sufficient to cool them to about 25° C. at the exit of the duct.
Claim 11
Dependent Claim
30 words
The process cf claim 9 wherein the duct is lined with a material of a low coefficient of friction at positions where the gas-solids mixture undergoes a change in direction.
Claim 12
Dependent Claim
15 words
The process of claim 1 wherein the cooling zone is a multi-stage fluid bed reactor.
Claim 13
Dependent Claim
13 words
The process of claim 11 wherein the fluidizing gas is room temperature air.
Claim 14
Dependent Claim
14 words
The process of claim 1 wherein the solids are transported between reactors using eductors.
Claim 15
Dependent Claim
90 words
A continuous process of coating small particles with a conformal coating of protective material, optionally doped with a metal, said process comprising the steps of: (a) feeding solids at a controlled rate to a first multi-stage fluid bed reactor, wherein the solids are contacted with a precursor material with or without a dopant; and (b) passing the solids to a second multi-stage fluid bed reactor, wherein the solids are cooled; and (c) collecting the coated and cooled solids from the exit of the last stage of the second multi-stage reactor.
Claim 16
Dependent Claim
90 words
A continuous process of coating small particles with a conformal coating of protective material, optionally doped with a metal, said process comprising the steps of: (a) feeding solids at a controlled rate to a first multi-stage fluid bed reactor, wherein the solids are contacted with a precursor material with or without a dopant; and (b) passing the solids to a second multi-stage fluid bed reactor, wherein the solids are cooled; and (c) collecting the coated and cooled solids from the exit of the last stage of the second multi-stage reactor.
Claim 17
Dependent Claim
29 words
The process of claim 14 wherein solids are fed at a constant mass rate to bed #1 of the first reactor using a microprocessor controlled loss in weight feeder.
Claim 18
Dependent Claim
28 words
The process of claim 14 which further comprises means for cooling the distributor plate of the first reactor to a temperature below the decomposition temperature of the precursor.
Claim 19
Dependent Claim
25 words
The process of claim 14 wherein the cooling means is a set of pipes in the distributor plate through which a coolant fluid is circulated.
Claim 20
Dependent Claim
24 words
The process of claim 14 wherein temperature control means are used to maintain essentially isothermal behavior in each stage of the first multi-stage reactor.
Claim 21
Dependent Claim
46 words
The process of claim 18 wherein the temperature of the solids in the first reactor is progressively increased from room temperature to about 500° C. in a certain number of stages, and maintained at that temperature in the remaining number of stages of the first reactor.
Claim 22
Dependent Claim
21 words
The process of claim 19 wherein the fluidizing gas for the stages leading to a temperature of 500° C. is nitrogen.
Claim 23
Dependent Claim
25 words
The process of claim 19 wherein the fluidizing gas for the balance of the stages contains in addition a coating material or a precursor thereto.
Claim 24
Dependent Claim
25 words
The process of claim 21 wherein the fluidizing gas for the balance of the stages contains in addition a dopant material or a precursor thereto.
Claim 25
Dependent Claim
37 words
The process of claim 22 wherein the dopant is selected from the elements of Groups IA, IIA, IIIA, IVA, VA, VIA, VIIA, VIIIA, IB, IIB, IIIB, IVB VB, VIB and VIIB of the Periodic Table of Elements.
Claim 26
Dependent Claim
14 words
The process of claim 23 wherein the dopant is iron or a precursor therefor.
Claim 27
Dependent Claim
13 words
The process of claim 24 wherein the iron precursor is Fe(CO) 5 .
Claim 28
Dependent Claim
15 words
The process of claim 21 wherein the precursor coating material is a precursor of alumina.
Claim 29
Dependent Claim
13 words
The process of claim 26 wherein the precursor of alumina is aluminum isopropoxide.
Claim 30
Dependent Claim
36 words
The process of claim 14 wherein hot and coated solids are transferred from the first reactor to the second reactor by a tube inclined at an angle greater than the angle of repose for the material.
Claim 31
Dependent Claim
23 words
The process of claim 14 wherein temperature control means are used to maintain essentially isothermal behavior in each stage of the second reactor.
Claim 32
Dependent Claim
21 words
The process of claim 14 wherein the solids are cooled from about 500° C. to 60° C. in the second reactor.
Claim 33
Dependent Claim
19 words
The process of claim 30 wherein the cooling is achieved by air fluidizing the stages of the second reactor.