Abstract

Abstract An anti-reflective film for synthetic resin optical parts of elements. The film comprises a first SiO layer, a second SiO2 layer, a third CeO2 layer and a fourth SiO2 layer, each layer having a particular optical thickness at a wavelength of lambda =400-700 nm.

Inventors

  • 👤 Hajime Ichikawa

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 03:03
CPC Classifications
G; G02; G02B; G02B1/00; G02B1/10; G02B1/11; G02B1/113; G02B1/115

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 110 words
An anti-reflective film comprising: a synthetic resin optical substrate, and four film layers laminated on the substrate, the four film layers comprising, for a wavelength of λ=400-700 nm, a first film layer on a surface of the substrate composed of SiO and having an optical thickness of 0.06-0.125 λ, a second film layer composed of SiO 2 on the first layer and having an optical thickness of 0.043-0.125 λ, a third film layer composed of CeO 2 on the second layer and having an optical thickness of 0.06-0.625 λ, and a fourth film layer composed of SiO 2 on the third layer and having an optical thickness of 0.165-0.34 λ.
Claim 2
Dependent Claim 110 words
An anti-reflective film comprising: a synthetic resin optical substrate, and four film layers laminated on the substrate, the four film layers comprising, for a wavelength of λ=400-700 nm, a first film layer on a surface of the substrate composed of SiO and having an optical thickness of 0.06-0.125 λ, a second film layer composed of SiO 2 on the first layer and having an optical thickness of 0.043-0.125 λ, a third film layer composed of CeO 2 on the second layer and having an optical thickness of 0.06-0.625 λ, and a fourth film layer composed of SiO 2 on the third layer and having an optical thickness of 0.165-0.34 λ.
Claim 3
Dependent Claim 34 words
The anti-reflective film according to claim 1, wherein said synthetic resin of the substrate is selected from a group consisting of acrylic resin, polycarbonate resin, diethyleneglycol bisacrylcarbonate, acrylonitrile-styrene copolymer resin, polystyrene and polysulfonic resin.
Claim 4
Dependent Claim 111 words
An anti-reflective film for use on a synthetic resin optical element, comprising: a first layer composed of SiO and disposable on a surface of a synthetic resin optical element and having an optical thickness of 0.06 to 0.125 λ where λ=400-700 nm, a second layer composed of CeO 2 on the first layer and having an optical thickness of 0.043-0.125 λ where λ=400-700 nm; a third layer composed of CeO 2 on the second layer and having an optical thickness of 0.06 to 0.625 λ where λ=400-700 nm; and a fourth layer composed of SiO 2 on the third layer and having an optical thickness of 0.165-0.34 λ where λ=400-700 nm.
Claim 5
Dependent Claim 111 words
An anti-reflective film for use on a synthetic resin optical element, comprising: a first layer composed of SiO and disposable on a surface of a synthetic resin optical element and having an optical thickness of 0.06 to 0.125 λ where λ=400-700 nm, a second layer composed of CeO 2 on the first layer and having an optical thickness of 0.043-0.125 λ where λ=400-700 nm; a third layer composed of CeO 2 on the second layer and having an optical thickness of 0.06 to 0.625 λ where λ=400-700 nm; and a fourth layer composed of SiO 2 on the third layer and having an optical thickness of 0.165-0.34 λ where λ=400-700 nm.
Claim 6
Dependent Claim 42 words
The film according to claim 3, wherein the first layer has an optical thickness of from 40 to 50 nm, the second from 30 to 50 nm, the third from 40 to 250 nm and the fourth from 115 to 135 nm.

References Cited (Backward Citations)

US3811753A Cited
US3799653A Cited
US4130672A Cited
US4609267A Cited
US4497539A Cited
US4599272A Cited
JPS60225101A Cited
US4784467A Cited
JPS6381404A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-01-28 1994-07-30 1995-01-29 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-01-28 1998-07-30 1999-01-29 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-01-28 2002-07-30 2003-01-29 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag