Abstract

Abstract The invention relates to ceramic composite articles formed by infiltration of a particulate, permeable bed or permeable preform with a polycrystalline matrix a metal-oxidant reaction product. The bed or preform includes a dross material.

Inventors

  • 👤 S. K. Nadkarni
  • 👤 Narasimha S. Raghavan

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 22:43
CPC Classifications
C; C04; C04B; C04B35/00; C04B35/622; C04B35/64; C04B35/65; C04B35/652

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 253 words
A self-supporting ceramic composite body produced by a method comprising the steps of: (a) providing at least one comminuted dross material as at least a portion of a permeable mass of filler material, said dross material being obtained from a metal melting operation; (b) orienting a parent metal and said permeable mass of filler material containing dross relative to each other so that formation of an oxidation reaction product will occur in a direction towards and into said permeable mass of filler material; and (c) heating said parent metal to a temperature above its melting point but below the melting point of said oxidation reaction product to form a body of molten parent metal and reacting the molten parent metal with at least one oxidant at said temperature to form said oxidation reaction product, and at said temperature maintaining at least a portion of said oxidation reaction product in contact with and extending between said body of molten metal and said at least one oxidant, to draw molten metal through the oxidation reaction product towards said at least one oxidant and towards and into the permeable mass of filler material containing dross so that fresh oxidation reaction product continues to form within the permeable mass of filler material containing dross at an interface between said at least one oxidant and previously formed oxidation reaction product, and continuing said reacting for a time sufficient to infiltrate at least a portion of said permeable mass of filler material containing dross with said oxidation reaction product.
Claim 2
Dependent Claim 253 words
A self-supporting ceramic composite body produced by a method comprising the steps of: (a) providing at least one comminuted dross material as at least a portion of a permeable mass of filler material, said dross material being obtained from a metal melting operation; (b) orienting a parent metal and said permeable mass of filler material containing dross relative to each other so that formation of an oxidation reaction product will occur in a direction towards and into said permeable mass of filler material; and (c) heating said parent metal to a temperature above its melting point but below the melting point of said oxidation reaction product to form a body of molten parent metal and reacting the molten parent metal with at least one oxidant at said temperature to form said oxidation reaction product, and at said temperature maintaining at least a portion of said oxidation reaction product in contact with and extending between said body of molten metal and said at least one oxidant, to draw molten metal through the oxidation reaction product towards said at least one oxidant and towards and into the permeable mass of filler material containing dross so that fresh oxidation reaction product continues to form within the permeable mass of filler material containing dross at an interface between said at least one oxidant and previously formed oxidation reaction product, and continuing said reacting for a time sufficient to infiltrate at least a portion of said permeable mass of filler material containing dross with said oxidation reaction product.
Claim 3
Dependent Claim 31 words
A self-supporting ceramic composite body comprising: a polycrystalline oxidation reaction product that is interconnected in at least one direction, which incorporates a filler material, wherein said filler material comprises comminuted dross.
Claim 4
Dependent Claim 31 words
A self-supporting ceramic composite body comprising: a polycrystalline oxidation reaction product that is interconnected in at least one direction, which incorporates a filler material, wherein said filler material comprises comminuted dross.
Claim 5
Dependent Claim 30 words
The self-supporting ceramic composite body according to claim 2, wherein said oxidation reaction product comprises at least one material selected from the group consisting of oxides, nitrides, borides, and carbides.
Claim 6
Dependent Claim 25 words
The self-supporting ceramic composite body according to claim 2, wherein said filler material comprises an admixture of comminuted dross and at least one other material.
Claim 7
Dependent Claim 37 words
The self-supporting ceramic composite body according to claim 4, wherein said at least one other material comprises at least one material selected from the group consisting of powder, particulates, aggregates, refractory fiber, tubules, whiskers, spheres, and platelets.
Claim 8
Dependent Claim 28 words
The self-supporting ceramic composite body according to claim 2, wherein said comminuted dross is present in a quantity sufficient to affect the morphology of said ceramic composite body.
Claim 9
Dependent Claim 33 words
The self-supporting ceramic composite body according to claim 2, wherein said filler material comprises a dross of at least one metal selected from the group consisting of aluminum, bronze, brass, nickel, and iron.
Claim 10
Dependent Claim 33 words
The self-supporting ceramic composite body according to claim 2, wherein said filler material comprises a nitride dross of at least one metal selected from the group consisting of aluminum, silicon, titanium, and zirconium.
Claim 11
Dependent Claim 30 words
The self-supporting ceramic composite body according to claim 1, wherein said parent metal comprises at least one material selected from the group consisting of aluminum, tin, silicon, titanium and zirconium.
Claim 12
Dependent Claim 42 words
The self-supporting ceramic composite body according to claim 2, wherein said self-supporting ceramic composite body comprises a polycrystalline oxidation reaction product of a parent metal comprising at least one material selected from the group consisting of aluminum, tin, silicon, titanium and zirconium.
Claim 13
Dependent Claim 15 words
The self-supporting ceramic composite body according to claim 10, wherein said parent metal comprises aluminum.
Claim 14
Dependent Claim 32 words
The self-supporting ceramic composite body according to claim 4, wherein said at least one other material comprises at least one material selected from the group consisting of metal oxides, nitrides and carbides.
Claim 15
Dependent Claim 25 words
The self-supporting ceramic composite body according to claim 1, wherein said filler material comprises an admixture of comminuted dross and at least one other material.
Claim 16
Dependent Claim 32 words
The self-supporting ceramic composite body according to claim 13, wherein said at least one other material comprises at least one material selected from the group consisting of metal oxides, nitrides and carbides.

References Cited (Backward Citations)

US3296002A Cited
US3669695A Cited
US4851375A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-01-14 1994-07-16 1995-01-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-01-14 1998-07-16 1999-01-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-01-14 2002-07-16 2003-01-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag