Abstract

Abstract An anodized aluminum part is wear tested by forcing a ball point stylus against the part and rotating the part about an axis spaced from the stylus. A turntable driven by a motor rotates the part at a desired speed. Weights are used to determine the force on the stylus. A layer of nonconductive oil on the test area helps clear wear debris from the circular wear path due to the motion of the ball through the oil. An ohm meter is connected between the stylus and the aluminum substrate to monitor electrical continuity and thus detect when the stylus wears through the anodized coating. The time required to achieve the wear through is a measure of the wear resistance of the coating.

Inventors

  • 👤 Leon Marcus

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 20:24
CPC Classifications
G; G01; G01N; G01N3/00; G01N3/56; G01N3/567

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 101 words
The method of wear testing the anodized surface coating of an electrically conductive part comprising the steps of: rotating the part about an axis of rotation at a set speed, pressing a stylus against the anodized surface coating of the part at a fixed load and at a given distance from the axis of rotation, whereby a circular path is worn in the surface, testing for electrical continuity between the stylus and the conductive part while the part is rotating, and measuring the time required to attain electrical continuity, wherein the time is a measure of the anodized surface coating quality.
Claim 2
Independent Claim 101 words
The method of wear testing the anodized surface coating of an electrically conductive part comprising the steps of: rotating the part about an axis of rotation at a set speed, pressing a stylus against the anodized surface coating of the part at a fixed load and at a given distance from the axis of rotation, whereby a circular path is worn in the surface, testing for electrical continuity between the stylus and the conductive part while the part is rotating, and measuring the time required to attain electrical continuity, wherein the time is a measure of the anodized surface coating quality.
Claim 3
Dependent Claim 19 words
The method as defined in claim 1 including the step of coating the anodized surface coating with nonconductive oil.
Claim 4
Dependent Claim 51 words
The method as defined in claim 1 wherein the surface wear mechanism is the crushing of the anodized surface coating by forceful point contact of the stylus on the anodized surface coating; including the step of assuring the integrity of the wear mechanism by continually clearing wear debris from the path.
Claim 5
Dependent Claim 46 words
The method as defined in claim 3 wherein the step of assuring the integrity of the wear mechanism comprises coating the anodized surface coating with a layer of nonconductive oil, whereby the wear debris is swept away by the motion of the stylus through the oil.
Claim 6
Dependent Claim 39 words
The method as defined in claim 1 wherein the step of pressing the stylus against the anodized surface coating comprises exerting sufficient force on the stylus to crush the anodized surface coating upon repeated traversing of the circular path.
Claim 7
Dependent Claim 104 words
A wear test apparatus for testing the anodized surface coating on an electrically conductive substrate comprising: means for rotating the substrate about an axis, a stylus for contacting the anodized surface coating at a point spaced from the axis of rotation, means for applying force to the anodized surface coating through the stylus so that during part rotation the stylus wears a path through the surface coating, electrical means for testing continuity between the stylus and the conductive substrate to determine when the stylus contacts the substrate, and means for measuring the time required by the stylus to wear through the anodized surface coating.
Claim 8
Dependent Claim 104 words
A wear test apparatus for testing the anodized surface coating on an electrically conductive substrate comprising: means for rotating the substrate about an axis, a stylus for contacting the anodized surface coating at a point spaced from the axis of rotation, means for applying force to the anodized surface coating through the stylus so that during part rotation the stylus wears a path through the surface coating, electrical means for testing continuity between the stylus and the conductive substrate to determine when the stylus contacts the substrate, and means for measuring the time required by the stylus to wear through the anodized surface coating.
Claim 9
Dependent Claim 35 words
The apparatus as defined in claim 6 wherein the means for rotating the substrate comprises a rotatable stage, a motor for rotating the stage, and a speed reducing mechanism coupling the motor to the stage.
Claim 10
Dependent Claim 37 words
The apparatus as defined in claim 6 wherein the stylus comprises a hardened steel ball and a holder for holding the ball against rotation so that sliding contact occurs between the ball and the anodized surface coating.
Claim 11
Dependent Claim 41 words
The apparatus as defined in claim 6 wherein the means for applying force comprises a support connected to the stylus and weight means mounted on the support directly above the locus of contact of the stylus and the anodized surface coating.
Claim 12
Dependent Claim 58 words
The apparatus as defined in claim 6 wherein the means for rotating the substrate includes clamp means to hold the substrate and also provide an electrical coupling to the substrate, and the said electrical means for testing continuity comprises means coupled to the stylus and to the means for rotating the substrate for monitoring the electrical resistance therebetween.

References Cited (Backward Citations)

GB497306A Cited
US2414439A Cited
US2962890A Cited
US3041868A Cited
US3834219A Cited
US4791807A Cited
US4864852A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-09-24 1994-03-26 1994-09-25 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-09-24 1998-03-26 1998-09-25 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-09-24 2002-03-26 2002-09-25 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag