Abstract

Abstract A method of producing glass fiber mat reinforced plastic panels having at least one smooth appearance surface in a set of two matched mold members having interior mold surfaces defining a mold cavity contained therein of which at least one interior surface is the mirror image of the appearance surface of the panel. The method includes the steps of placing at least one layer of glass fiber mat in a mold cavity, pouring a polymeric material into the cavity saturating the glass fiber mat, closing the two mold members together with at least one layer of a flexible sheeting material disposed over and adjacent to the interior mold surface opposing the interior mold surface producing the appearance surface of the panel, clamping the two mold members together, curing the polymeric material for a sufficient time into a hard plastic panel, and opening the matched mold members and demold a finished panel having at least one smooth appearance surface.

Inventors

  • 👤 Hamid G. Kia

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 09:33
CPC Classifications
B; B29; B29C; B29C70/00; B29C70/04; B29C70/28; B29C70/40; B29C70/42; B29C70/46; B29C33/00; B29C33/56

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 186 words
In a method of compression molding glass fiber mat reinforced plastic panels having at least one appearance surface in a set of two matched mold member of which at least one member having an interior mold surface being the mirror image of the appearance surface of said panel, of the type wherein at least one glass fiber mat is first placed in the mold cavity defined by the interior mold surfaces of said mold members and a polymeric material is introduced into the cavity saturating said mat and curing into a panel under heat and pressure transmitted through said mold members clamped together, the improvement comprising placing at least one layer of a reusable flexible sheeting material immediately adjacent to the interior mold surface opposing the mold surface produces the appearance surface of said molded panel prior to clamping the two mold members together and applying pressure on said mold members whereby said at least one layer of flexible sheeting material acts as a stress relief layer to prevent the formation of fiber readout defects and remains in said mold members after the compression molding process.
Claim 2
Dependent Claim 186 words
In a method of compression molding glass fiber mat reinforced plastic panels having at least one appearance surface in a set of two matched mold member of which at least one member having an interior mold surface being the mirror image of the appearance surface of said panel, of the type wherein at least one glass fiber mat is first placed in the mold cavity defined by the interior mold surfaces of said mold members and a polymeric material is introduced into the cavity saturating said mat and curing into a panel under heat and pressure transmitted through said mold members clamped together, the improvement comprising placing at least one layer of a reusable flexible sheeting material immediately adjacent to the interior mold surface opposing the mold surface produces the appearance surface of said molded panel prior to clamping the two mold members together and applying pressure on said mold members whereby said at least one layer of flexible sheeting material acts as a stress relief layer to prevent the formation of fiber readout defects and remains in said mold members after the compression molding process.
Claim 3
Independent Claim 238 words
A method of producing glass fiber mat reinforced plastic panels having at least one smooth appearance surface in a set of two matched mold members having interior mold surfaces defining a mold cavity contained therein of which at least one said interior surface being the mirror image of the appearance surface of said panel, said matched mold members being equipped with an injection port for the injection of a polymeric material into said mold cavity, said method comprising: placing at least one layer of glass fiber mat in said mold cavity, closing said two mold members together with at least one layer of a reusable flexible sheeting material disposed over and adjacent to the interior mold surface opposing said interior mold surface producing the appearance surface of said panel, clamping said two mold members together under sufficient clamping pressure such that no leaking of the polymeric materials occurs when injected into said mold cavity, injecting a sufficient amount of a polymeric material into said mold cavity through said injection port in said mold, curing said polymeric material for a sufficient time into a hard plastic panel, and opening said matched mold members and demold a finished panel having at least one smooth appearance surface whereby said at least one layer of flexible sheeting material acts as a stress relief layer to prevent the formation of fiber readout defects and remains in said mold members after the molding process.
Claim 4
Independent Claim 238 words
A method of producing glass fiber mat reinforced plastic panels having at least one smooth appearance surface in a set of two matched mold members having interior mold surfaces defining a mold cavity contained therein of which at least one said interior surface being the mirror image of the appearance surface of said panel, said matched mold members being equipped with an injection port for the injection of a polymeric material into said mold cavity, said method comprising: placing at least one layer of glass fiber mat in said mold cavity, closing said two mold members together with at least one layer of a reusable flexible sheeting material disposed over and adjacent to the interior mold surface opposing said interior mold surface producing the appearance surface of said panel, clamping said two mold members together under sufficient clamping pressure such that no leaking of the polymeric materials occurs when injected into said mold cavity, injecting a sufficient amount of a polymeric material into said mold cavity through said injection port in said mold, curing said polymeric material for a sufficient time into a hard plastic panel, and opening said matched mold members and demold a finished panel having at least one smooth appearance surface whereby said at least one layer of flexible sheeting material acts as a stress relief layer to prevent the formation of fiber readout defects and remains in said mold members after the molding process.
Claim 5
Independent Claim 240 words
A method of producing glass fiber mat reinforced plastic panels having at least one smooth appearance surface in a set of two matched mold members having interior mold surfaces defining a mold cavity contained therein of which at least one said interior surface being the mirror image of the appearance surface of said panel, said matched mold members being equipped with an injection port for the injection of a polymeric material into said mold cavity, said method comprising: placing at least one layer of glass fiber mat in said mold cavity, closing said two mold members together with a layer of reusable flexible sheeting material having a thickness of no less than 0.01 inch disposed over and adjacent to the interior mold surface opposing said interior mold surface producing the appearance surface of said panel, clamping said two mold members together under sufficient clamping pressure that no leaking of the polymeric materials occurs when injected into said mold cavity, injecting a sufficient amount of a polymeric material into said mold cavity through said injection port in said mold, curing said polymeric material for a sufficient time into a hard plastic panel, and opening said matched mold members and demold a finished panel having at least one smooth appearance surface whereby said layer of flexible sheeting material acts as a stress relief layer to prevent the formation of fiber readout defects and remains in said mold members after the molding process.
Claim 6
Independent Claim 240 words
A method of producing glass fiber mat reinforced plastic panels having at least one smooth appearance surface in a set of two matched mold members having interior mold surfaces defining a mold cavity contained therein of which at least one said interior surface being the mirror image of the appearance surface of said panel, said matched mold members being equipped with an injection port for the injection of a polymeric material into said mold cavity, said method comprising: placing at least one layer of glass fiber mat in said mold cavity, closing said two mold members together with a layer of reusable flexible sheeting material having a thickness of no less than 0.01 inch disposed over and adjacent to the interior mold surface opposing said interior mold surface producing the appearance surface of said panel, clamping said two mold members together under sufficient clamping pressure that no leaking of the polymeric materials occurs when injected into said mold cavity, injecting a sufficient amount of a polymeric material into said mold cavity through said injection port in said mold, curing said polymeric material for a sufficient time into a hard plastic panel, and opening said matched mold members and demold a finished panel having at least one smooth appearance surface whereby said layer of flexible sheeting material acts as a stress relief layer to prevent the formation of fiber readout defects and remains in said mold members after the molding process.
Claim 7
Independent Claim 251 words
A method of producing glass fiber mat reinforced plastic panels having at least one smooth appearance surface in a set of two matched mold members having interior mold surfaces defining a mold cavity contained therein of which at least one said interior surface being the mirror image of the appearance surface of said panel, said matched mold members being equipped with an injection port for the injection of a polymeric material into said mold cavity, said method comprising: placing at least one layer of glass fiber mat in said mold cavity, closing said two mold members together with at least one layer of a reusable flexible sheeting material having a Shore "A" durometer of no larger than 60 as determined by ASTMD-2240 over and adjacent to the interior mold surface opposing said interior mold surface producing the appearance surface of said panel, clamping said two mold members together under sufficient clamping pressure such that no leaking of the polymeric materials occurs when injected into said mold cavity, injecting a sufficient amount of a polymeric material into said mold cavity through said injection port in said mold, curing said polymeric material for a sufficient time into a hard plastic panel, and opening said matched mold member and demold a finished panel having at least one smooth appearance surface whereby said at least one layer of flexible sheeting material acts as a stress relief layer to prevent the formation of fiber readout defects and remains in said mold members after the molding process.
Claim 8
Independent Claim 251 words
A method of producing glass fiber mat reinforced plastic panels having at least one smooth appearance surface in a set of two matched mold members having interior mold surfaces defining a mold cavity contained therein of which at least one said interior surface being the mirror image of the appearance surface of said panel, said matched mold members being equipped with an injection port for the injection of a polymeric material into said mold cavity, said method comprising: placing at least one layer of glass fiber mat in said mold cavity, closing said two mold members together with at least one layer of a reusable flexible sheeting material having a Shore "A" durometer of no larger than 60 as determined by ASTMD-2240 over and adjacent to the interior mold surface opposing said interior mold surface producing the appearance surface of said panel, clamping said two mold members together under sufficient clamping pressure such that no leaking of the polymeric materials occurs when injected into said mold cavity, injecting a sufficient amount of a polymeric material into said mold cavity through said injection port in said mold, curing said polymeric material for a sufficient time into a hard plastic panel, and opening said matched mold member and demold a finished panel having at least one smooth appearance surface whereby said at least one layer of flexible sheeting material acts as a stress relief layer to prevent the formation of fiber readout defects and remains in said mold members after the molding process.
Claim 9
Independent Claim 191 words
A method of producing glass fiber mat reinforced plastic panels having at least one smooth appearance surface in a set of two matched mold members having interior mold surfaces defining a mold cavity contained therein of which at least one said interior surface being the mirror image of the appearance surface of said panel, said method comprising: placing at least one layer of glass fiber mat in said mold cavity, pouring a polymeric material into said cavity saturating said glass fiber mat, closing said two mole member together with at least one layer of a reusable flexible sheeting material disposed over and adjacent to the interior mold surface opposing said interior mold surface producing the appearance surface of said panel, clamping said two mold members together, curing said polymeric material for a sufficient time into a hard plastic panel, and opening said matched mold members and demold a finished panel having at least one smooth appearance surface whereby said at least one layer of flexible sheeting material acts as a stress relief layer to prevent the formation of fiber readout defects and remains in said mold members after the molding process.
Claim 10
Independent Claim 191 words
A method of producing glass fiber mat reinforced plastic panels having at least one smooth appearance surface in a set of two matched mold members having interior mold surfaces defining a mold cavity contained therein of which at least one said interior surface being the mirror image of the appearance surface of said panel, said method comprising: placing at least one layer of glass fiber mat in said mold cavity, pouring a polymeric material into said cavity saturating said glass fiber mat, closing said two mole member together with at least one layer of a reusable flexible sheeting material disposed over and adjacent to the interior mold surface opposing said interior mold surface producing the appearance surface of said panel, clamping said two mold members together, curing said polymeric material for a sufficient time into a hard plastic panel, and opening said matched mold members and demold a finished panel having at least one smooth appearance surface whereby said at least one layer of flexible sheeting material acts as a stress relief layer to prevent the formation of fiber readout defects and remains in said mold members after the molding process.
Claim 11
Independent Claim 194 words
A method of producing glass fiber mat reinforced plastic panels having at least one smooth appearance surface in a set of two matched mold members having interior mold surfaces defining a mold cavity contained therein of which at least one said interior surface being the mirror image of the appearance surface of said panel, said method comprising: placing at least one layer of glass fiber mat in said mold cavity, pouring a polymeric material into said cavity saturating said glass fiber mat, closing said two mold members together with a layer of reusable flexible sheeting material having a thickness of no less than 0.01 inch disposed over and adjacent to the interior mold surface opposing said interior mold surface producing the appearance surface of said panel, clamping said two mold members together, curing said polymeric material for a sufficient time into a hard plastic panel, and opening said matched mold members and demold a finished panel having at least one smooth appearance surface whereby said layer of flexible sheeting material acts as a stress relief layer to prevent the formation of fiber readout defects and remains in said mold members after the molding process.
Claim 12
Independent Claim 194 words
A method of producing glass fiber mat reinforced plastic panels having at least one smooth appearance surface in a set of two matched mold members having interior mold surfaces defining a mold cavity contained therein of which at least one said interior surface being the mirror image of the appearance surface of said panel, said method comprising: placing at least one layer of glass fiber mat in said mold cavity, pouring a polymeric material into said cavity saturating said glass fiber mat, closing said two mold members together with a layer of reusable flexible sheeting material having a thickness of no less than 0.01 inch disposed over and adjacent to the interior mold surface opposing said interior mold surface producing the appearance surface of said panel, clamping said two mold members together, curing said polymeric material for a sufficient time into a hard plastic panel, and opening said matched mold members and demold a finished panel having at least one smooth appearance surface whereby said layer of flexible sheeting material acts as a stress relief layer to prevent the formation of fiber readout defects and remains in said mold members after the molding process.
Claim 13
Independent Claim 206 words
A method of producing glass fiber mat reinforced plastic panels having at least one smooth appearance surface in a set of two matched mold members having interior mold surfaces defining a mold cavity contained therein of which at least one said interior surface being the mirror image of the appearance surface of said panel, said method comprising: placing at least one layer of glass fiber mat in said mold cavity, pouring a polymeric material into said cavity saturating said glass fiber mat, closing said two mold members together with at least one layer of a reusable flexible sheeting material having a Shore A durometer of no greater than 60 as determined by ASTM D-2240 disposed over and adjacent to the interior mold surface opposing said interior mold surface producing the appearance surface of said panel, clamping said two mold members together, curing said polymeric material for a sufficient time into a hard plastic panel, and opening said matched mold members and demold a finished panel having at least one smooth appearance surface whereby said at least one layer of flexible sheeting material acts as a stress relief layer to prevent the formation of fiber readout defects and remains in said mold members after the molding process.
Claim 14
Independent Claim 206 words
A method of producing glass fiber mat reinforced plastic panels having at least one smooth appearance surface in a set of two matched mold members having interior mold surfaces defining a mold cavity contained therein of which at least one said interior surface being the mirror image of the appearance surface of said panel, said method comprising: placing at least one layer of glass fiber mat in said mold cavity, pouring a polymeric material into said cavity saturating said glass fiber mat, closing said two mold members together with at least one layer of a reusable flexible sheeting material having a Shore A durometer of no greater than 60 as determined by ASTM D-2240 disposed over and adjacent to the interior mold surface opposing said interior mold surface producing the appearance surface of said panel, clamping said two mold members together, curing said polymeric material for a sufficient time into a hard plastic panel, and opening said matched mold members and demold a finished panel having at least one smooth appearance surface whereby said at least one layer of flexible sheeting material acts as a stress relief layer to prevent the formation of fiber readout defects and remains in said mold members after the molding process.

References Cited (Backward Citations)

US3663341A Cited
US3755031A Cited
US4123488A Cited
US4201823A Cited
US4379103A Cited
US4517323A Cited
US4548861A Cited
US4714575A Cited
US4891176A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-09-17 1994-03-19 1994-09-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-09-17 1998-03-19 1998-09-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-09-17 2002-03-19 2002-09-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag