Method to make microcavities and its application to an electrochemical sensor
Assignee: Thales SA
•
Filing: 1988-09-19
•
Granted: 1990-09-11
•
Expires: 2008-09-19
Abstract
Abstract A method for making a microcavity in an enamel layer is disclosed. For this purpose, a layer of a carbon-based material with the dimensions of the microcavity to be obtained is provided. This layer is coated with an enamel except in a limited zone. The unit is heated to high temperature so as to cause combustion of the carbon-based material. The combustion gases escape through the reduced zone.
Inventors
- 👤 Didier Pribat
- 👤 Joel Perret
- 👤 Jean-Claude Rouffy
- 👤 Gonzalo Velasco
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-04 22:00
CPC Classifications
G; G01; G01N; G01N27/00; G01N27/26; G01N27/403; G01N27/406; G01N27/407; G01N27/4071; G01N30/00; G01N30/02; G01N30/60; G01N30/6095; G01N30/6052; G01N30/6073; G01N30/6078
Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
152 words
A method for making an electrochemical sensor having a microcavity comprising the steps of: forming on a substrate at least one element made of solid electrolyte; partially covering said electrolyte element with a first electrode; partially covering said electrolyte element with a second electrode; making, on said second electrode, an element made of a material which is combustible and/or volatile at high temperature and which has the shape, thickness and position of said microcavity to be formed; making a sheath fully covering said first and second electrodes, said electrolyte element and said element made of combustible and/or volatile material, said sheath being made of an amorphous material which is impervious to a fluid mixture and, for making, in said sheath an axis hole to said element made of combustible and/or volatile materials; and heating at least said element made of combustible and/or volatile materials so as to cause its evaporation and/or consumption.
Claim 2
Independent Claim
152 words
A method for making an electrochemical sensor having a microcavity comprising the steps of: forming on a substrate at least one element made of solid electrolyte; partially covering said electrolyte element with a first electrode; partially covering said electrolyte element with a second electrode; making, on said second electrode, an element made of a material which is combustible and/or volatile at high temperature and which has the shape, thickness and position of said microcavity to be formed; making a sheath fully covering said first and second electrodes, said electrolyte element and said element made of combustible and/or volatile material, said sheath being made of an amorphous material which is impervious to a fluid mixture and, for making, in said sheath an axis hole to said element made of combustible and/or volatile materials; and heating at least said element made of combustible and/or volatile materials so as to cause its evaporation and/or consumption.
Claim 3
Dependent Claim
19 words
A manufacturing method according to claim 1 wherein the element made of volatile or combustible material is carbon based.
Claim 4
Dependent Claim
15 words
A manufacturing method according to claim 1 wherein said element is made of pure carbon.
Claim 5
Dependent Claim
25 words
A manufacturing method according to claim 1 wherein the thickness of the element made of combustible and/or volatile material ranges between 1 and 5 micrometers.
Claim 6
Dependent Claim
32 words
A manufacturing method according to claim 1 wherein the element made of combustible and/or volatile material is located on that part of the second electrode which covers the element made of electrolyte.
Claim 7
Dependent Claim
200 words
An electrochemical sensor for the measurement of relative concentrations of species contained in a fluid mixture, made according to the method of claim 1, comprising: at least one solid electrolyte which is an ion conductor of one of the species of the fluid mixture or of an ion capable of reacting with this species; at least one first partial pressure internal reference electrode in contact, by one of its faces, entirely or partly, with the solid electrolyte; at least one second measuring electrode in contact, by one of its faces, entirely or partially, with the solid electrolyte and receiving the fluid mixture to be analyzed; a layer of an encapsulating material made of an inert material which is impervious to the species present in the fluid mixture, coating the first electrode, the second electrode and the solid electrolyte, and having one access hole enabling the fluid mixture to reach the second electrode; said electrochemical sensor comprising at least one microcavity partially covering the second measuring electrode in that zone which covers the electrolyte, said microcavity communicating through the access hole with the fluid mixture to be analyzed and having a thickness enabling a diffusion of a molecular type of fluid.
Claim 8
Dependent Claim
19 words
An electrochemical sensor according to claim 6 wherein the thickness of the cavity ranges between 1 and 5 micrometers.
References Cited (Backward Citations)
US4271000A
Cited
US4272350A
Cited
EP0047687A2
Cited
EP0052542A1
Cited
US4741817A
Cited
US4488920A
Cited
EP0140295A2
Cited
EP0144057A2
Cited
EP0203351A1
Cited
EP0218357A2
Cited
US4668374A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1993-09-10 | 1994-03-12 | 1994-09-11 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1997-09-10 | 1998-03-12 | 1998-09-11 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2001-09-10 | 2002-03-12 | 2002-09-11 | $7700.00 | Window Closed / Lapsed |