US4947372A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Optical information memory medium for recording and erasing information
Assignee: Fujitsu Ltd
•
Filing: 1989-11-30
•
Granted: 1990-08-07
•
Expires: 2009-11-30
Abstract
Abstract Recording and erasing optical information can be done by using an alloy film capable of forming two stable crystalline states differing in crystal texture and optical characteristics by being irradiated with optical energies under different conditions. The memory film includes 35-45 atom % of Indium (In) and 55-65 atom % of antimony (Sb).
Inventors
- 👤 Nagaaki Koshino
- 👤 Miyozo Maeda
- 👤 Yasuyuki Goto
- 👤 Itaru Shibata
- 👤 Kenichi Utsumi
- 👤 Akira Ushioda
- 👤 Ken-ichi Itoh
- 👤 Kozo Sueishi
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-03 10:56
CPC Classifications
G; G11; G11B; G11B7/00; G11B7/24; G11B7/241; G11B7/242; G11B7/243; G11B7/2433; G11B7/252; G11B7/257; G11B7/004; G11B2007/24302; G11B2007/2431; G11B2007/24314; G11B7/254; G11B7/2542; G11B7/2572; G11B7/2578; Y; Y10; Y10S; Y10S430/00; Y10S430/146; Y10S430/165
Claims Analysis
Total Claims: 9
Claim 1
Independent Claim
150 words
An optical information memory medium including a substrate, comprising: a thin memory film, formed on the substrate including 35-45 atom% of Indium (In) and 55-65 atom% of antimony (Sb), capable of selectively forming two stable crystalline states, the memory film having a first crystalline state when information has been recorded and a second crystalline state when information has been erased, the first crystalline state having a first reflectivity by irradiating the memory film with an optical energy beam having a first intensity for a first time period such that the entire thickness of the memory film is fused at the portion irradiated , and the second crystalline state having a second reflectivity lower than the first reflectivity by irradiating the memory film with an optical energy beam having a second intensity less than or equal to the first intensity for a second time period longer than the first time period.
Claim 2
Dependent Claim
150 words
An optical information memory medium including a substrate, comprising: a thin memory film, formed on the substrate including 35-45 atom% of Indium (In) and 55-65 atom% of antimony (Sb), capable of selectively forming two stable crystalline states, the memory film having a first crystalline state when information has been recorded and a second crystalline state when information has been erased, the first crystalline state having a first reflectivity by irradiating the memory film with an optical energy beam having a first intensity for a first time period such that the entire thickness of the memory film is fused at the portion irradiated , and the second crystalline state having a second reflectivity lower than the first reflectivity by irradiating the memory film with an optical energy beam having a second intensity less than or equal to the first intensity for a second time period longer than the first time period.
Claim 3
Dependent Claim
63 words
An optical information memory medium according to claim 1, wherein said memory film comprises at least one element M selected from the group consisting of Al, Si, P, S, Zn, Ga, Ge, As, Se, Ag, Cd, Sn, Te, Tl, Pb, and Bi, and wherein said memory film has a composition of (In x Sb 1-x ) 1-y M y where 0.35≦×≦0.45 and y≦0.20.
Claim 4
Dependent Claim
63 words
An optical information memory medium according to claim 1, wherein said memory film further comprises at least one element M selected from the group consisting of Se, Si, P, S, Ge, As, Zn, Al, Ag, Cd, Sn, Pb, Te, Bi, and Ga, and wherein said memory film has a composition of (In x Sb 1-x ) 1-y M y where 0.35≦×≦0.45 and y≦0.20.
Claim 5
Dependent Claim
22 words
An optical information memory medium according to claim 1, wherein the thickness of said memory film is not more than 90 nm.
Claim 6
Dependent Claim
30 words
An optical information memory medium according to claim 1, wherein the memory film having said first and second crystalline states comprise crystallites having a size of 5 nm or larger.
Claim 7
Dependent Claim
19 words
An optical information memory medium according to claim 5, wherein the size of crystallites is larger than 20 nm.
Claim 8
Dependent Claim
29 words
An optical information memory medium according to claim 1, wherein said memory film is formed on a substrate and wherein said memory film is covered with a protective film.
Claim 9
Dependent Claim
43 words
An optical information medium according to claim 7, wherein said protective film includes one or more elements selected from the group consisting of SiO 2 , CeO 2 , SnO 2 , ZnS, PMMA, polystyrene, an epoxy resin, and a UV curable resin.
References Cited (Backward Citations)
US3271591A
Cited
US3530441A
Cited
US3868651A
Cited
US4237468A
Cited
US4373004A
Cited
US4460636A
Cited
US4653024A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1993-08-06 | 1994-02-05 | 1994-08-07 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1997-08-06 | 1998-02-05 | 1998-08-07 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2001-08-06 | 2002-02-05 | 2002-08-07 | $7700.00 | Window Closed / Lapsed |