Patent US4944823A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4944823A Expired / Lapsed US ⏱️ 0.0 years remaining

Composition for bonding solid lignocellulosic materials

Assignee: Carbocol Systems Inc
•
Filing: 1985-09-26
•
Granted: 1990-07-31
•
Expires: 2005-09-26
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Wood surfaces are bonded together by heating and pressing using a preferably dry binder formulation constituting a thorough mixture of an isocyanate and a sugar or starch, the binder formulation also preferably containing a stabilizer and optionally a catalyst and a release agent. The binder formulation may be used with good results in an amount equal to the amount of straight isocyanate resin which would normally be used, i.e. the sugar or starch replaces a quantity of the isocyanate which would normally have been used, thereby reducing the total quantity of isocyanate, thus reducing cost without any disadvantage.

Inventors

  • 👤 John Stofko

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 21:10
CPC Classifications
C; C09; C09J; C09J175/00; C09J175/04; C08; C08G; C08G18/00; C08G18/06; C08G18/28; C08G18/30; C08G18/32; C08G18/3203; C08G18/3218; C08G18/40; C08G18/64; C08G18/6484; C08L; C08L97/00; C08L97/02; Y; Y10; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31971; Y10T428/31989

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 133 words
A method of bonding wood surfaces together and thereby producing a consolidated wood product, which comprises contacting said wood surfaces with an amount of bonding material of 1-15 grams per square foot area or 1-12% by weight based on the weight of wood, said bonding material consisting essentially of a homogeneous mixture, initially reacted in the substantial absence of water, of 50-95% by weight of starch or sugar or other active material, 5-50% of liquid isocyanate, 0-10% catalyst, 0-50% stabilizing agent and 0-10% release agent, or a glucourethane reaction product thereof, the total quantity of said liquid isocyanate being 0.25-2% by weight based on the weight of the wood; pressing the coated wood surfaces together at an elevated temperature and for a time sufficient to effect bonding to produce said bonded wood product.
Claim 2
Independent Claim 133 words
A method of bonding wood surfaces together and thereby producing a consolidated wood product, which comprises contacting said wood surfaces with an amount of bonding material of 1-15 grams per square foot area or 1-12% by weight based on the weight of wood, said bonding material consisting essentially of a homogeneous mixture, initially reacted in the substantial absence of water, of 50-95% by weight of starch or sugar or other active material, 5-50% of liquid isocyanate, 0-10% catalyst, 0-50% stabilizing agent and 0-10% release agent, or a glucourethane reaction product thereof, the total quantity of said liquid isocyanate being 0.25-2% by weight based on the weight of the wood; pressing the coated wood surfaces together at an elevated temperature and for a time sufficient to effect bonding to produce said bonded wood product.
Claim 3
Dependent Claim 37 words
A method according to claim 1 wherein said bonding material comprises a mixture of said liquid isocyanate and said carbohydrate, a glucourethane reaction product of said liquid isocyanate and said starch or sugar, or a mixture thereof.
Claim 4
Dependent Claim 36 words
A method according to claim 1 wherein said bonding material contains said other active material, and wherein said other active material is selected from the group consisting of weak acids, acidic salts, carbonates and mixtures thereof.
Claim 5
Dependent Claim 13 words
A method according to claim 1 wherein said liquid isocyanate is 4,4'-diphenylmethane diisocyanate.
Claim 6
Dependent Claim 26 words
A method according to claim 1 wherein said bonding material is a liquid and comprises 40-90% of said isocyanate and 60-10% of said starch or sugar.
Claim 7
Dependent Claim 59 words
A method according to claim 1 wherein said bonding material is a liquid containing at least 50% starch or sugar based on the mixture of isocyanate and starch or sugar, and further comprises a small quantity of inert, polar, nonaqueous solvent, or water added after an initial reaction has been effected between said isocyanate and said starch or sugar.
Claim 8
Dependent Claim 36 words
A method according to claim 1 wherein said bonding material is in the form of a homogeneous wet powdery or pasty mixture containing about 20-40% liquid isocyanate and about 80-60% of active material, starch or sugar.
Claim 9
Dependent Claim 20 words
A method according to claim 1 wherein said bonding material comprises at least 3% by weight of said liquid isocyanate.
Claim 10
Dependent Claim 29 words
A method according to claim 5 wherein said bonding material comprises said starch or sugar present in an amount of about 4-8% based on the weight of the wood.
Claim 11
Dependent Claim 36 words
A method according to claim 5 wherein said bonding material comprises 50-65% by weight of sugar or starch powder, 5-15% of isocyanate, 20-45% sodium sulfate stabilizer, up to 5% catalyst and up to 10% release agent.
Claim 12
Dependent Claim 25 words
A method according to claim 5 wherein said bonding material is applied at the rate of about 3-10% based on the weight of the wood.
Claim 13
Dependent Claim 15 words
A method according to claim 5 wherein said pressing is carried out in two stages.
Claim 14
Dependent Claim 19 words
A method according to claim 12 wherein, after the first stage of pressing, the product is sprayed with water.
Claim 15
Dependent Claim 26 words
A method according to claim 1 wherein pressing is carried out for less than one minute per 1/8 inch of board thickness at about 100°-200° C.
Claim 16
Independent Claim 132 words
A method of bonding wood surfaces together and thereby producing a consolidated wood product, comprising contacting said wood surfaces with a homogeneous dry powdery bonding material in an amount of 1-15 grams per square foot area or 1-12% by weight based on the weight of the wood, said dry powdery bonding material consisting essentially of a homogeneous mixture of 80-98% by weight of starch or sugar or other active material, 2-20% of liquid isocyanate, 0-10% catalyst, 0-50% stabilizing agent and 0-10% release agent, or a glucourethane reaction product thereof, the total quantity of said liquid isocyanate being 0.25-2% by weight based on the weight of the wood; and pressing the coated wood surfaces together at an elevated temperature and for a time sufficient to effect bonding to produce said bonded wood product.
Claim 17
Independent Claim 132 words
A method of bonding wood surfaces together and thereby producing a consolidated wood product, comprising contacting said wood surfaces with a homogeneous dry powdery bonding material in an amount of 1-15 grams per square foot area or 1-12% by weight based on the weight of the wood, said dry powdery bonding material consisting essentially of a homogeneous mixture of 80-98% by weight of starch or sugar or other active material, 2-20% of liquid isocyanate, 0-10% catalyst, 0-50% stabilizing agent and 0-10% release agent, or a glucourethane reaction product thereof, the total quantity of said liquid isocyanate being 0.25-2% by weight based on the weight of the wood; and pressing the coated wood surfaces together at an elevated temperature and for a time sufficient to effect bonding to produce said bonded wood product.

References Cited (Backward Citations)

No citation records indexed.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-07-30 1994-01-29 1994-07-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-07-30 1998-01-29 1998-07-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-07-30 2002-01-29 2002-07-31 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag