Patent US4927480A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4927480A Expired / Lapsed US ⏱️ 0.0 years remaining

Method and clamping device for bonding thin lens wafers

Assignee: Sanwa Business Credit Corp
•
Filing: 1989-02-27
•
Granted: 1990-05-22
•
Expires: 2009-02-27
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A clamping device for bonding lens wafers, the device having a resilient stamp and an oppositely-disposed resilient mold. The stamp surface is slightly more curved than the concave surface of the top wafer and the mold surface is slightly more planar than the convex surface of the bottom wafer. As the wafers are squeezed between the stamp and mold, the stamp and mold deform and bonding material is squeezed evenly outwardly between the wafers.

Inventors

  • 👤 Thomas L. Vaughan

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 03:09
CPC Classifications
B; B29; B29C; B29C66/00; B29C66/80; B29C66/83; B29C66/832; B29C66/8322; B29C65/00; B29C65/48; B29C66/01; B29C66/05; B29C66/10; B29C66/11; B29C66/112; B29C66/1122; B29C66/50; B29C66/51; B29C66/54; B29C66/545; B29C66/82; B29C66/824; B29C66/8242; B29C66/90; B29C66/92; B29C66/922; B29C66/9221; B29C66/924; B29C66/9241; B29D; B29D11/00; B29D11/0073; B30; B30B; B30B15/00; B30B15/02; B30B15/022; B30B15/024; B29C65/4805; B29C65/483; B29C66/40; B29C66/41; B29C66/45; B29C66/452; B29L; B29L2009/00; B29L2011/00; B29L2011/0016

Claims Analysis

Total Claims: 19
Claim 1
Independent Claim 155 words
A clamping device for squeezing a quantity of bonding material between a first bonding surface of a first lens wafer and a second bonding surface of a second lens wafer, said first lens wafer comprising a convex outer surface and said second lens wafer comprising a concave outer surface, said clamping device comprising: a deformable, resilient mold; said mold comprising a concave surface that is slightly more planar than said convex outer surface of said first lens wafer; a deformable, resilient stamp disposed opposite said mold; said stamp comprising a convex surface that is slightly more curved than said concave outer surface of said second lens wafer; and piston means for simultaneously exerting pressure on said convex and concave outer surfaces of said lens wafers through said concave surface of said mold and said convex surface of said stamp, respectively, thereby squeezing said quantity of bonding material between said bonding surfaces of said lens wafers.
Claim 2
Dependent Claim 155 words
A clamping device for squeezing a quantity of bonding material between a first bonding surface of a first lens wafer and a second bonding surface of a second lens wafer, said first lens wafer comprising a convex outer surface and said second lens wafer comprising a concave outer surface, said clamping device comprising: a deformable, resilient mold; said mold comprising a concave surface that is slightly more planar than said convex outer surface of said first lens wafer; a deformable, resilient stamp disposed opposite said mold; said stamp comprising a convex surface that is slightly more curved than said concave outer surface of said second lens wafer; and piston means for simultaneously exerting pressure on said convex and concave outer surfaces of said lens wafers through said concave surface of said mold and said convex surface of said stamp, respectively, thereby squeezing said quantity of bonding material between said bonding surfaces of said lens wafers.
Claim 3
Dependent Claim 19 words
A clamping device as recited in claim 1, wherein: said stamp and said mold are made of silicone rubber.
Claim 4
Dependent Claim 41 words
A clamping device as recited in claim 1, wherein said piston means comprises: an air cylinder; a pressure gauge for measuring the air pressure directed to said air cylinder; and means for adjusting said air pressure directed to said air cylinder.
Claim 5
Dependent Claim 51 words
A clamping device as recited in claim 1 wherein: said mold is fixed to a base with said concave surface facing upward; said stamp is mounted above said mold with said convex surface facing downward; and said clamping device comprises means mounting said stamp for vertical movement relative to said mold.
Claim 6
Dependent Claim 37 words
A clamping device as recited in claim 4 wherein: said mold comprises raised centering means around the periphery of said concave surface for centering and aligning said first lens wafer on said concave surface below said stamp.
Claim 7
Dependent Claim 33 words
A clamping device as recited in claim 1 wherein: said piston means comprises means for moving said mold and said stamp towards one another at a rate of about one inch per second.
Claim 8
Dependent Claim 15 words
A clamping device as recited in claim 1 wherein said concave mold surface is paraboloidal.
Claim 9
Dependent Claim 30 words
A clamping device as recited in claim 7, wherein: said mold surface measures at least about 1/2 smaller in diopter than said convex outer surface of said first lens wafer.
Claim 10
Dependent Claim 15 words
A clamping device as recited in claim 1 wherein said convex stamp surface is paraboloidal.
Claim 11
Dependent Claim 30 words
A clamping device as recited in claim 9, wherein: said stamp surface measures at least about 1/2 larger in diopter than said concave outer surface of said second lens wafer.
Claim 12
Independent Claim 170 words
A method for bonding a first lens wafer comprising both a first bonding surface and a convex outer surface to a second lens wafer comprising both a second bonding surface and a concave outer surface, said method comprising the steps of: applying a quantity of bonding material to a center portion of one of said bonding surfaces; placing the other of said bonding surfaces in contact with said quantity of bonding material; providing a deformable, resilient mold comprising a concave surface that is slightly more planar than said convex outer surface of said first lens wafer; providing a deformable, resilient stamp disposed opposite said mold and comprising a convex surface that is slightly more curved than said concave outer surface of said second lens wafer; and simultaneously exerting pressure on said convex and concave outer surfaces of said lens wafers through said concave surface of said mold and said convex surface of said stamp, respectively, thereby squeezing said quantity of bonding material between said bonding surfaces of said lens wafers.
Claim 13
Independent Claim 170 words
A method for bonding a first lens wafer comprising both a first bonding surface and a convex outer surface to a second lens wafer comprising both a second bonding surface and a concave outer surface, said method comprising the steps of: applying a quantity of bonding material to a center portion of one of said bonding surfaces; placing the other of said bonding surfaces in contact with said quantity of bonding material; providing a deformable, resilient mold comprising a concave surface that is slightly more planar than said convex outer surface of said first lens wafer; providing a deformable, resilient stamp disposed opposite said mold and comprising a convex surface that is slightly more curved than said concave outer surface of said second lens wafer; and simultaneously exerting pressure on said convex and concave outer surfaces of said lens wafers through said concave surface of said mold and said convex surface of said stamp, respectively, thereby squeezing said quantity of bonding material between said bonding surfaces of said lens wafers.
Claim 14
Dependent Claim 23 words
A method as recited in claim 11, comprising the additional step of: curing said quantity of bonding material after said pressure exerting step.
Claim 15
Dependent Claim 25 words
A method as recited in claim 11, comprising the additional step of: waiting about one minute between said pressure exerting step and said curing step.
Claim 16
Dependent Claim 30 words
A method as recited in claim 11, wherein: the refractive index of said bonding material applied in said application step is similar to the refractive indices of said lens wafers.
Claim 17
Dependent Claim 30 words
A method as recited in claim 11, wherein: said lens wafers are being bonded to form a lens for eyeglasses; and said quantity of bonding material is about 0.2 ml.
Claim 18
Dependent Claim 48 words
A method as recited in claim 11, comprising the additional steps of: centering said convex outer surface of said first lens wafer on said concave surface of said mold; and moving said convex surface of said stamp downwardly against said concave outer surface of said second lens wafer.
Claim 19
Dependent Claim 26 words
A method as recited in claim 16, wherein: said convex surface of said stamp is moved downwardly at a rate of about one inch per second.

References Cited (Backward Citations)

JPS4811588A Cited
US4564408A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-05-21 1993-11-20 1994-05-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-05-21 1997-11-20 1998-05-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-05-21 2001-11-20 2002-05-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag