Reservoir feed method of making ceramic composite structures and structures made thereby

Assignee: Lanxide Technology Co LP
•
Filing: 1988-03-15
•
Granted: 1990-04-17
•
Expires: 2008-03-15
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for producing a self-supporting ceramic composite structure comprising a ceramic matrix embedding a filler, includes oxidizing a parent metal to form a polycrystalline material comprising the oxidation reaction product of the parent metal and, optionally, one or more metallic constituents. The method includes heating the parent metal to provide a source of molten parent metal and a reservoir of molten metal which is in communication with the parent metal having a chemical composition which is different from the parent metal and contacting the molten parent metal with a permeable bedding of filler. The molten parent metal reacts with the oxidant to form the oxidation reaction product and is replenished by the reservoir as the reacting continues for a time sufficient to grow the oxidation reaction product to a desired extent and thereby embed at least a portion of the bedding of filler within the oxidation reaction product to form the ceramic composite structure. The bedding of filler may have any suitable shape, including that of a hollow body, the interior of which is contacted by the molten parent metal to grow the oxidation reaction product through the shaped, hollow body of filler.

Inventors

  • 👤 Jerry G. Weinstein
  • 👤 Robert C. Kantner
  • 👤 Marc S. Newkirk

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 03:27
CPC Classifications
C; C04; C04B; C04B35/00; C04B35/622; C04B35/64; C04B35/65; C04B35/652; B; B28; B28B; B28B7/00; B28B7/34; B28B7/342; B28B7/344

Claims Analysis

Total Claims: 24
Claim 1
Independent Claim 329 words
A method for producing a self-supporting ceramic composite structure comprising a ceramic matrix obtained by an oxidation reaction of at least a first parent metal with an oxidant to form a polycrystalline material which comprises an oxidation reaction product of said first parent metal and said oxidant and a filler infiltrated by said matrix, the method comprising: (a) orienting a source comprising said first parent metal and a permeable mass of filler relative to each other so that formation of an oxidation reaction product will occur in a direction towards and into said mass of filler, wherein the quantity of said source of first parent metal provided is insufficient to embed substantially completely said permeable mass; (b) communicating a reservoir comprising a second metal having a chemical composition which is different from said source of first parent metal with said source of first parent metal; (c) heating said source of first parent metal to a temperature which is above the melting points of the first parent metal and the second metal, but below the melting point of said oxidation reaction product of said first parent metal to form a source comprising molten first parent metal and reacting said source of molten first parent metal with an oxidant to form said oxidation reaction product by maintaining at least a portion of said oxidation reaction product in contact with and extending between said source of molten first parent metal and said oxidant to progressively draw molten parent metal through the oxidation reaction product towards the oxidant and into said mass of filler so that fresh oxidation reaction product continues to form within said mass of filler at an interface between said oxidant and previously formed oxidation reaction product; and (d) at said temperature, replenishing said source of first parent metal with said second metal in said reservoir as said oxidation reaction continues such that said permeable mass is substantially completely embedded, to permit the formation of said self-supporting ceramic composite structure.
Claim 2
Independent Claim 329 words
A method for producing a self-supporting ceramic composite structure comprising a ceramic matrix obtained by an oxidation reaction of at least a first parent metal with an oxidant to form a polycrystalline material which comprises an oxidation reaction product of said first parent metal and said oxidant and a filler infiltrated by said matrix, the method comprising: (a) orienting a source comprising said first parent metal and a permeable mass of filler relative to each other so that formation of an oxidation reaction product will occur in a direction towards and into said mass of filler, wherein the quantity of said source of first parent metal provided is insufficient to embed substantially completely said permeable mass; (b) communicating a reservoir comprising a second metal having a chemical composition which is different from said source of first parent metal with said source of first parent metal; (c) heating said source of first parent metal to a temperature which is above the melting points of the first parent metal and the second metal, but below the melting point of said oxidation reaction product of said first parent metal to form a source comprising molten first parent metal and reacting said source of molten first parent metal with an oxidant to form said oxidation reaction product by maintaining at least a portion of said oxidation reaction product in contact with and extending between said source of molten first parent metal and said oxidant to progressively draw molten parent metal through the oxidation reaction product towards the oxidant and into said mass of filler so that fresh oxidation reaction product continues to form within said mass of filler at an interface between said oxidant and previously formed oxidation reaction product; and (d) at said temperature, replenishing said source of first parent metal with said second metal in said reservoir as said oxidation reaction continues such that said permeable mass is substantially completely embedded, to permit the formation of said self-supporting ceramic composite structure.
Claim 3
Dependent Claim 19 words
The method of claim 1, wherein said reservoir of second metal communicates with said parent metal by gravity flow.
Claim 4
Dependent Claim 19 words
The method of claim 1 or claim 2, wherein said mass of filler comprises at least one shaped preform.
Claim 5
Dependent Claim 18 words
The method of claim 1 or claim 2, wherein said ceramic composite structure comprises an interconnected metallic component.
Claim 6
Dependent Claim 15 words
The method of claim 3, wherein said ceramic composite structure comprises an interconnected metallic component.
Claim 7
Dependent Claim 32 words
The method of claim 1 or claim 2, wherein said reservoir of a second metal is maintained at a temperature less than a temperature utilized for the growth of oxidation reaction product.
Claim 8
Dependent Claim 29 words
The method of claim 3, wherein said reservoir of a second metal is maintained at a temperature less than a temperature utilized for the growth of oxidation reaction product.
Claim 9
Dependent Claim 98 words
The method of claim 1 or claim 2, wherein said first source of parent metal comprises a solid ingot of parent metal having a pattern formed thereon, and said mass of filler material comprises a filler which is in conforming engagement with said pattern, whereby after said reacting is completed by infiltrating the filler material to a desired amount to form said self-supporting ceramic composite structure, any excess parent metal which did not form oxidation reaction product is removed from said filler material and said self-supporting ceramic composite structure contains an inversely replicated geometry of said pattern therein.
Claim 10
Dependent Claim 25 words
The method of claim 3, wherein at least a portion of a surface of said at least one preform is defined by a barrier means.
Claim 11
Dependent Claim 64 words
The method of claim 1 or claim 2, further comprising a barrier means at least partially spaced from said first source of parent metal for establishing at least one surface of said mass of filler material, whereby said reacting occurs until said oxidation reaction product confronts said barrier means, thereby producing a ceramic composite structure having an exterior surface established by said barrier means.
Claim 12
Dependent Claim 55 words
The method of claim 1 or claim 2, further comprising maintaining said reservoir source of molten parent metal at an elevation at or above the highest elevation of said body of molten parent metal from said first source to maintain a static pressure head on said body of molten parent metal from said first source.
Claim 13
Dependent Claim 52 words
The method of claim 3, further comprising maintaining said reservoir source of molten parent metal at an elevation at or above the highest elevation of said body of molten parent metal from said first source to maintain a static pressure head on said body of molten parent metal from said first source.
Claim 14
Dependent Claim 36 words
The method of claim 1 or claim 2, wherein said mass of filler material comprises a plurality of masses of filler material each of said plurality of masses of filler material contacting said molten parent metal.
Claim 15
Dependent Claim 27 words
The method of claim 3, wherein said at least one preform comprises a plurality of preforms each of said plurality of preforms contacting said molten parent metal.
Claim 16
Dependent Claim 51 words
The method of claim 1 or claim 2, further comprising maintaining molten parent metal in contact with said mass of filler material and after said reacting is completed, permitting unreacted metal to solidify in contact with said self-supporting ceramic composite structure so as to provide a metal substrate integrally formed therewith.
Claim 17
Dependent Claim 49 words
The method of claim 3, further comprising maintaining molten parent metal in contact with said at least one shaped preform and after said reacting is completed, permitting unreacted metal to solidify in contact with said self-supporting ceramic composite structure so as to provide a metal substrate integrally formed therewith.
Claim 18
Dependent Claim 30 words
The method of claim 1 or claim 2, wherein said parent metal comprises at least one metal selected from the group consisting of aluminum, titanium, silicon, zirconium, hafnium and tin.
Claim 19
Dependent Claim 33 words
The method of claim 9, wherein said barrier means comprises at least one material selected from the group consisting of stainless steel, plaster of paris, calcium silicate, calcium sulfate, wollastonite and portland cement.
Claim 20
Dependent Claim 33 words
The method of claim 10, wherein said barrier means comprises at least one material selected from the group consisting of stainless steel, plaster of paris, calcium silicate, calcium sulfate, wollastonite and portand cement.
Claim 21
Independent Claim 333 words
A method for producing a self-supporting ceramic composite structure comprising a ceramic matrix obtained by an oxidation reaction of at least a first parent metal with an oxidant to form a polycrystalline material which comprises an oxidation reaction product of said first parent metal and said oxidant and a filler infiltrated by said matrix, the method comprising: (a) orienting at least a source comprising a first parent metal and a permeable mass of filler relative to each other so that formation of an oxidation reaction product will occur in a direction towards and into said mass of filler, wherein the quantity of said source of first parent metal provided is insufficient to embed substantially completely said permeable mass; (b) communicating a reservoir comprising a second metal which is maintained at a temperature which is less than a temperature of said first source of parent metal with said first source of parent metal; (c) heating said source of first parent metal to a temperature which is above the melting points of the first parent metal and the second metal, but below the melting point of said oxidation reaction product of said parent metal to form a source comprising first molten parent metal and reacting said molten first parent metal with an oxidant to form said oxidation reaction product by maintaining at least a portion of said oxidation reaction product in contact with and extending between said source of first molten parent metal and said oxidant to progressively draw molten parent metal through the oxidation reaction product towards the oxidant and into said mass of filler so that fresh oxidation reaction product continues to form within said mass of filler at an interface between said oxidant and previously formed oxidation reaction product; and (d) at said temperature, replenishing said source of first parent metal with said second metal in said reservoir as said oxidation reaction continues such that said permeable mass is substantially completely embedded, to permit the formation of said self-supporting ceramic composite structure.
Claim 22
Independent Claim 333 words
A method for producing a self-supporting ceramic composite structure comprising a ceramic matrix obtained by an oxidation reaction of at least a first parent metal with an oxidant to form a polycrystalline material which comprises an oxidation reaction product of said first parent metal and said oxidant and a filler infiltrated by said matrix, the method comprising: (a) orienting at least a source comprising a first parent metal and a permeable mass of filler relative to each other so that formation of an oxidation reaction product will occur in a direction towards and into said mass of filler, wherein the quantity of said source of first parent metal provided is insufficient to embed substantially completely said permeable mass; (b) communicating a reservoir comprising a second metal which is maintained at a temperature which is less than a temperature of said first source of parent metal with said first source of parent metal; (c) heating said source of first parent metal to a temperature which is above the melting points of the first parent metal and the second metal, but below the melting point of said oxidation reaction product of said parent metal to form a source comprising first molten parent metal and reacting said molten first parent metal with an oxidant to form said oxidation reaction product by maintaining at least a portion of said oxidation reaction product in contact with and extending between said source of first molten parent metal and said oxidant to progressively draw molten parent metal through the oxidation reaction product towards the oxidant and into said mass of filler so that fresh oxidation reaction product continues to form within said mass of filler at an interface between said oxidant and previously formed oxidation reaction product; and (d) at said temperature, replenishing said source of first parent metal with said second metal in said reservoir as said oxidation reaction continues such that said permeable mass is substantially completely embedded, to permit the formation of said self-supporting ceramic composite structure.
Claim 23
Dependent Claim 19 words
The method of claim 20, wherein said heating of said first source of parent metal occurs within a furnace.
Claim 24
Dependent Claim 23 words
The method of claim 21, wherein at least a portion of said second metal is located, at least initially, external to said furnace.

References Cited (Backward Citations)

US3709096A Cited
US4824008A Cited
US4833110A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-04-16 1993-10-16 1994-04-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-04-16 1997-10-16 1998-04-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-04-16 2001-10-16 2002-04-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag