Abstract

Abstract A process for continuously producing a copper-clad laminate by double belt pressing which comprises heating a laminating material comprising at least one resin-impregnated base of continuous length and a copper foil of continuous length superposed on at least one of the outer surfaces of the base(s) between a pair of belts under pressure, wherein a laminating material having been continuously heat-fused under reduced pressure in a vacuum chamber is used. The pressure applied to the laminating material during heating under pressure can be reduced to a range of from 10 to 30 kg/cm 2 .

Inventors

  • 👤 Kazuo Noguchi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 07:30
CPC Classifications
B; B32; B32B; B32B15/00; B32B15/14; B32B15/04; B32B15/08; B32B15/20; B32B37/00; B32B37/02; B32B37/04; H; H05; H05K; H05K3/00; H05K3/02; H05K3/022; B29; B29L; B29L2031/00; B29L2031/34; B29L2031/3425; B32B2260/00; B32B2260/02; B32B2260/021; B32B2260/04; B32B2260/046; B32B2262/00; B32B2262/10; B32B2262/101; B32B2309/00; B32B2309/60; B32B2311/00; B32B2311/12; B32B2315/00; B32B2315/08; B32B2315/085; H05K1/00; H05K1/02; H05K1/03; H05K1/0313; H05K1/0353; H05K1/0366; H05K2203/00; H05K2203/06; H05K2203/068; H05K2203/15; H05K2203/1545

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 216 words
A process for continuously producing a copper-clad laminate, comprising the steps of: (A) pre-heating at least one resin-impregnated base of continuous length and at least one copper foil of continuous length under reduced pressure in a vacuum chamber so as to produce a pre-fused laminate material; (B) heat fusing the resulting pre-fused laminate material of Step ()) under reduced pressure in said vacuum chamber so as to form a laminate material; and (C) heating the resulting laminate material of Step (B) between a pair of belts of a double belt press under pressure so as to form said copper-clad laminate, wherein in Step (A), said copper foil is superimposed on at least one outer surface of said base, and wherein said laminate material has a temperature of T 1 , before Step (C); and said laminate material has a maximum temperature of T 2 , during Step (C); and said copper-clad laminate has a temperature T 3 , after Step (C); and wherein the range of temperature change T 2 -T 1 ≦100° C. and T 2 -T 3 ≦100° C., and wherein said copper-clad laminate, while being delivered out of a pressurized cooling zone of said double belt press, has a temperature at least 20° C. higher than a glass transition temperature of said resin.
Claim 2
Dependent Claim 216 words
A process for continuously producing a copper-clad laminate, comprising the steps of: (A) pre-heating at least one resin-impregnated base of continuous length and at least one copper foil of continuous length under reduced pressure in a vacuum chamber so as to produce a pre-fused laminate material; (B) heat fusing the resulting pre-fused laminate material of Step ()) under reduced pressure in said vacuum chamber so as to form a laminate material; and (C) heating the resulting laminate material of Step (B) between a pair of belts of a double belt press under pressure so as to form said copper-clad laminate, wherein in Step (A), said copper foil is superimposed on at least one outer surface of said base, and wherein said laminate material has a temperature of T 1 , before Step (C); and said laminate material has a maximum temperature of T 2 , during Step (C); and said copper-clad laminate has a temperature T 3 , after Step (C); and wherein the range of temperature change T 2 -T 1 ≦100° C. and T 2 -T 3 ≦100° C., and wherein said copper-clad laminate, while being delivered out of a pressurized cooling zone of said double belt press, has a temperature at least 20° C. higher than a glass transition temperature of said resin.
Claim 3
Dependent Claim 21 words
The process as claimed in claim 1, wherein said Steps (A) and (B) said pressure is not more han 500 mmHg.
Claim 4
Dependent Claim 47 words
The process as claimed in claim 1, wherein air in the vicinity of an inlet and an outlet of said vacuum chamber of Steps (A) and (B), through which the resin-impregnated bases and copper foils are introduced and delivered, has a cleanness class of 100,000 or less.
Claim 5
Dependent Claim 35 words
The process as claimed in claim 1, wherein said pair of belts at an inlet for supplying said resin-impregnated base and said copper foil, are heated to a temperature of not less than 100° C.
Claim 6
Dependent Claim 24 words
The process as claimed in claim 1, wherein Step (C) is carried out at a pressure of from 10 to 30 kg/cm 2 .

References Cited (Backward Citations)

US3305416A Cited
US3960635A Cited
US4579612A Cited
US4670080A Cited
US4659425A Cited
JPS63118242A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-03-19 1993-09-18 1994-03-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-03-19 1997-09-18 1998-03-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-03-19 2001-09-18 2002-03-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag