Patent US4906538A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4906538A Expired / Lapsed US ⏱️ 0.0 years remaining

Non-aqueous secondary cell

Assignee: Bridgestone Corp
•
Filing: 1988-03-18
•
Granted: 1990-03-06
•
Expires: 2008-03-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A non-aqueous secondary cell comprising a positive electrode, a negative electrode and a non-aqueous electrolyte is provided wherein the positive electrode comprises as an active material polyaniline containing 15 to 30% by weight of BF 4 .

Inventors

  • 👤 Shinichi Toyosawa
  • 👤 Shigeru Kijima
  • 👤 Hideharu Daifuku
  • 👤 Yuko Maeda
  • 👤 Katsuhiko Arai
  • 👤 Takahiro Kawagoe

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 21:50
CPC Classifications
H; H01; H01M; H01M10/00; H01M10/05; C; C08; C08G; C08G73/00; C08G73/02; C08G73/026; C08G73/0266; H01M4/00; H01M4/02; H01M4/04; H01M4/0438; H01M4/0464; H01M4/0466; H01M4/36; H01M4/60; H01M4/602; H01M4/64; H01M4/70; H01M4/72; H01M4/74; H01M4/742; H01M2004/026; H01M2004/028; H01M2300/00; H01M2300/0017; H01M2300/0025; H01M4/66; H01M4/661; H01M4/663; H01M4/669; Y; Y02; Y02E; Y02E60/00; Y02E60/10

Claims Analysis

Total Claims: 11
Claim 1
Independent Claim 71 words
A non-aqueous secondary cell comprising a positive electrode, a negative electrode and an non-aqueous electrolyte solution, wherein the positive electrode comprises as an active material polyaniline film which has been purified by continuously passing 2 to 20 ml/cm 2 of water per 1 mm thickness of the polyaniline film through the film in a thickness direction thereof at a flow rate of 0.1 to 10 ml/cm 2 min to remove impurities.
Claim 2
Dependent Claim 71 words
A non-aqueous secondary cell comprising a positive electrode, a negative electrode and an non-aqueous electrolyte solution, wherein the positive electrode comprises as an active material polyaniline film which has been purified by continuously passing 2 to 20 ml/cm 2 of water per 1 mm thickness of the polyaniline film through the film in a thickness direction thereof at a flow rate of 0.1 to 10 ml/cm 2 min to remove impurities.
Claim 3
Dependent Claim 17 words
The cell of claim 1 wherein the polyaniline film is deposited on a planar network electroconductive material.
Claim 4
Dependent Claim 16 words
The cell of claim 2 wherein the planar network electroconductive material is a stainless steel mesh.
Claim 5
Dependent Claim 69 words
The cell of claim 1 wherein said polyaniline is prepared by immersing a polymerization electrode and a counter electrode comprising a plurality of spaced-apart segments in an electrolytic polymerization solution in an electrolysis tank, and conducting electricity across the electrodes to carry out electrolytic polymerization to deposit a polyaniline film on the polymerization electrode while independently controlling the current or voltage applied to the plurality of counter electrode segments.
Claim 6
Dependent Claim 20 words
The cell of claim 4 wherein a shield partition is disposed between two adjoining ones of the counter electrode segments.
Claim 7
Dependent Claim 24 words
The cell of claim 1 wherein the negative electrode comprises as an active material a lithium-aluminum alloy containing 25 to 65 atom% of lithium.
Claim 8
Dependent Claim 41 words
The cell of claim 1 wherein said electrolyte solution comprises a mixture of 35 to 65% by volume of propylene carbonate and the balance of dimethoxyethane having dissolved therein from more than 1 mol/liter to 3 mol/liter of LiBF 4 .
Claim 9
Dependent Claim 23 words
The cell of claim 1, wherein said polyaniline film has been purified by passing water through the film under super- or sub-atmospheric pressure.
Claim 10
Dependent Claim 42 words
The cell of claim 1, wherein the polyaniline film is washed with water such that when 1 gram of polyaniline is extracted with 200 ml of water, the extract water has an equilibrium pH in the range of from 2.4 to 4.
Claim 11
Dependent Claim 25 words
The cell of claim 1, wherein the polyaniline film which has been washed with water contains 15% to 30% by weight of BF 4 .

References Cited (Backward Citations)

US4740436A Cited
US4717634A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-03-05 1993-09-04 1994-03-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-03-05 1997-09-04 1998-03-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-03-05 2001-09-04 2002-03-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag