US4892786A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Ceramic articles with a polymer component and methods of making same
Assignee: Lanxide Technology Co LP
•
Filing: 1987-06-26
•
Granted: 1990-01-09
•
Expires: 2007-06-26
Abstract
Abstract A method of producing self-supporting ceramic or ceramic composite bodies having a polymer component, which includes first providing a self-supporting ceramic or ceramic composite body comprising (i) a polycrystalline oxidation reaction product formed upon oxidation of a molten parent metal with an oxidant, and (ii) interconnected porosity at least partially accessible from one or more surfaces of said ceramic body. The polymer is disposed or formed within the interconnected porosity. The polymer is situated so as to alter, modify or contribute to the properties of the ceramic or ceramic composite body originally formed.
Inventors
- 👤 Marc S. Newkirk
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-03 21:05
CPC Classifications
C; C04; C04B; C04B35/00; C04B41/00; C04B41/009; C04B35/622; C04B35/64; C04B35/65; C04B35/652; C04B41/45; C04B41/46; C04B41/48; C04B41/80; C04B41/81; C04B41/82; C04B41/83; Y; Y10; Y10T; Y10T428/00; Y10T428/12; Y10T428/12014; Y10T428/12028; Y10T428/12042; Y10T428/12063; Y10T428/12104; Y10T428/12111; Y10T428/12153; Y10T428/1216; Y10T428/12167; Y10T428/249921; Y10T428/249953; Y10T428/249955; Y10T428/249956; Y10T428/249971; Y10T428/249972
Claims Analysis
Total Claims: 25
Claim 1
Independent Claim
79 words
A method of producing a self-supporting ceramic body containing a polymer component, comprising the steps of: (a) providing a self-supporting ceramic body comprising (i) a polycrystalline oxidation reaction product formed upon oxidation of a molten parent metal with an oxidant, and (ii) interconnected porosity at least partially accessible from at least one surface of said ceramic body; and (b) disposing a polymer in at least a portion of said porosity to form a ceramic body containing a polymer component.
Claim 2
Independent Claim
79 words
A method of producing a self-supporting ceramic body containing a polymer component, comprising the steps of: (a) providing a self-supporting ceramic body comprising (i) a polycrystalline oxidation reaction product formed upon oxidation of a molten parent metal with an oxidant, and (ii) interconnected porosity at least partially accessible from at least one surface of said ceramic body; and (b) disposing a polymer in at least a portion of said porosity to form a ceramic body containing a polymer component.
Claim 3
Independent Claim
118 words
A method of producing a self-supporting ceramic body containing a polymer component comprising the steps of: (a) providing a self-supporting ceramic body comprising (i) a polycrystalline oxidation reaction product formed upon oxidation of a molten parent metal with an oxidant, and (ii) interconnected porosity at least partially accessible from at least one surface of said ceramic body; (b) contacting said at least one surface of said ceramic body with a quantity of a polymer which is capable of infiltrating at least a portion of said interconnected porosity; and (c) infiltrating at least a portion of said interconnected porosity with at least a portion of said quantity of said polymer to form a ceramic body containing a polymer component.
Claim 4
Independent Claim
118 words
A method of producing a self-supporting ceramic body containing a polymer component comprising the steps of: (a) providing a self-supporting ceramic body comprising (i) a polycrystalline oxidation reaction product formed upon oxidation of a molten parent metal with an oxidant, and (ii) interconnected porosity at least partially accessible from at least one surface of said ceramic body; (b) contacting said at least one surface of said ceramic body with a quantity of a polymer which is capable of infiltrating at least a portion of said interconnected porosity; and (c) infiltrating at least a portion of said interconnected porosity with at least a portion of said quantity of said polymer to form a ceramic body containing a polymer component.
Claim 5
Independent Claim
81 words
A method of producing a self-supporting ceramic body containing a polymer component comprising the steps of: (a) providing a self-supporting ceramic body comprising (i) a polycrystalline oxidation reaction product formed upon oxidation of a molten parent metal with an oxidant, and (ii) interconnected porosity at least partially accessible from at least one surface of said ceramic body; and (b) forming a polymer in situ in at least a portion of said porosity to produce a ceramic body containing a polymer component.
Claim 6
Independent Claim
81 words
A method of producing a self-supporting ceramic body containing a polymer component comprising the steps of: (a) providing a self-supporting ceramic body comprising (i) a polycrystalline oxidation reaction product formed upon oxidation of a molten parent metal with an oxidant, and (ii) interconnected porosity at least partially accessible from at least one surface of said ceramic body; and (b) forming a polymer in situ in at least a portion of said porosity to produce a ceramic body containing a polymer component.
Claim 7
Independent Claim
117 words
A method of producing a self-supporting ceramic body containing a polymer component comprising the steps of: (a) providing a self-supporting ceramic body comprising (i) a polycrystalline oxidation reaction product formed upon oxidation of a molten parent metal with an oxidant, and (ii) interconnected porosity at least partially accessible from at least one surface of said ceramic body; (b) positioning the ceramic body in a reaction zone; (c) infiltrating at least a portion of the porosity of the ceramic body in the reaction zone with a polymerizable fluid which forms a polymer under polymerizing conditions; and (d) subjecting the infiltrated ceramic body in the reaction zone to polymerizing conditions to form a ceramic body containing a polymer component.
Claim 8
Independent Claim
117 words
A method of producing a self-supporting ceramic body containing a polymer component comprising the steps of: (a) providing a self-supporting ceramic body comprising (i) a polycrystalline oxidation reaction product formed upon oxidation of a molten parent metal with an oxidant, and (ii) interconnected porosity at least partially accessible from at least one surface of said ceramic body; (b) positioning the ceramic body in a reaction zone; (c) infiltrating at least a portion of the porosity of the ceramic body in the reaction zone with a polymerizable fluid which forms a polymer under polymerizing conditions; and (d) subjecting the infiltrated ceramic body in the reaction zone to polymerizing conditions to form a ceramic body containing a polymer component.
Claim 9
Independent Claim
35 words
The method of any of claims 1 or 2 or 3 or 4, wherein the parent metal comprises at least one material selected from the group consisting of aluminum, silicon, titanium, tin, zirconium, and hafnium.
Claim 10
Independent Claim
27 words
The method of any of claims 1 or 2 or 3 or 4, wherein the parent metal comprises aluminum and the polycrystalline oxidation reaction product comprises alumina.
Claim 11
Independent Claim
39 words
The method of any of claims 1 or 2 or 3 or 4, wherein the interconnected porosity is between about 5 to 45 percent by volume of the ceramic body before the ceramic body is impregnated with the polymer.
Claim 12
Independent Claim
29 words
The method of any of claims 1 or 2 or 3 or 4, wherein the self-supporting ceramic body further comprises a filler infiltrated by said polycrystalline oxidation reaction product.
Claim 13
Dependent Claim
17 words
The method of claim 8, further comprising the additional step of shaping said filler into a preform.
Claim 14
Dependent Claim
51 words
A self-supporting ceramic body which comprises: a polycrystalline oxidation reaction product formed upon oxidation of a molten parent metal with an oxidant, and possessing interconnected porosity at least partially accessible from at least one surface of said ceramic body; and a polymer disposed in at least a portion of said porosity.
Claim 15
Dependent Claim
51 words
A self-supporting ceramic body which comprises: a polycrystalline oxidation reaction product formed upon oxidation of a molten parent metal with an oxidant, and possessing interconnected porosity at least partially accessible from at least one surface of said ceramic body; and a polymer disposed in at least a portion of said porosity.
Claim 16
Independent Claim
64 words
The method of any of claims 1 or 2 or 3 or 4, wherein said ceramic body further comprises an interconnected metallic component at least partially accessible from at least one surface of said ceramic body, and wherein said ceramic body is placed in a heating zone prior to step (b) to at least partially vaporize said interconnected metallic component from said ceramic body.
Claim 17
Independent Claim
64 words
The method of any of claims 1 or 2 or 3 or 4, wherein said ceramic body further comprises an interconnected metallic component at least partially accessible from at least one surface of said ceramic body, and wherein said ceramic body is additionally immersed into a leachant prior to step (b) to at least partially dissolve said interconnected metallic component from said ceramic body.
Claim 18
Independent Claim
313 words
A method of producing a self-supporting ceramic composite body comprising a polycrystalline material comprising an oxidation reaction product of a parent metal and an oxidant, said ceramic composite body containing a polymer component, said method comprising the steps of: (a) positioning a parent metal adjacent to a permeable mass of filler material and orienting said parent metal and said filler relative to each other so that formation of an oxidation reaction product of said parent metal will occur in a direction towards and into said mass of filler; (b) heating said parent metal to a temperature above its melting point but below the melting point of its oxidation reaction product to form a body of parent metal and reacting the molten parent metal with an oxidant at said temperature to form said oxidation reaction product, and at said temperature maintaining at least a portion of said oxidation reaction product in contact with and extending between said body of molten metal and said oxidant, to draw molten metal through the oxidation reaction product towards the oxidant and towards and into the adjacent mass of filler material so that fresh oxidation reaction product continues to form within the mass of filler at an interface between the oxidant and previously formed oxidation reaction product; (c) continuing said reacting for a time sufficient to embed at least a portion of the filler with said oxidation reaction product, thereby forming a ceramic composite body; (d) forming at least some porosity in said ceramic composite body by utilizing at least one treatment step selected from the group consisting of taking the oxidation reaction process to completion, vaporizing residual parent metal from the ceramic composite body and leaching residual parent metal from the ceramic composite body; and (e) disposing a polymer into at least a portion of said formed porosity, thereby forming a ceramic composite body containing a polymer component.
Claim 19
Independent Claim
313 words
A method of producing a self-supporting ceramic composite body comprising a polycrystalline material comprising an oxidation reaction product of a parent metal and an oxidant, said ceramic composite body containing a polymer component, said method comprising the steps of: (a) positioning a parent metal adjacent to a permeable mass of filler material and orienting said parent metal and said filler relative to each other so that formation of an oxidation reaction product of said parent metal will occur in a direction towards and into said mass of filler; (b) heating said parent metal to a temperature above its melting point but below the melting point of its oxidation reaction product to form a body of parent metal and reacting the molten parent metal with an oxidant at said temperature to form said oxidation reaction product, and at said temperature maintaining at least a portion of said oxidation reaction product in contact with and extending between said body of molten metal and said oxidant, to draw molten metal through the oxidation reaction product towards the oxidant and towards and into the adjacent mass of filler material so that fresh oxidation reaction product continues to form within the mass of filler at an interface between the oxidant and previously formed oxidation reaction product; (c) continuing said reacting for a time sufficient to embed at least a portion of the filler with said oxidation reaction product, thereby forming a ceramic composite body; (d) forming at least some porosity in said ceramic composite body by utilizing at least one treatment step selected from the group consisting of taking the oxidation reaction process to completion, vaporizing residual parent metal from the ceramic composite body and leaching residual parent metal from the ceramic composite body; and (e) disposing a polymer into at least a portion of said formed porosity, thereby forming a ceramic composite body containing a polymer component.
Claim 20
Dependent Claim
76 words
The method of claim 13, wherein said disposing of a polymer comprises at least one step selected from the group consisting of infiltrating a polymer into at least a portion of said ceramic composite body, forming a polymer in situ in at least a portion of said ceramic composite body and infiltrating at least a portion of the ceramic composite body in a reaction zone with a polymerizable fluid which forms a polymer under polymerizing conditions.
Claim 21
Independent Claim
30 words
The method of any claims 13 or 14, wherein the parent metal comprises at least one material selected from the group consisting of aluminum, silicon, titanium, tin, zirconium, and hafnium.
Claim 22
Independent Claim
23 words
The method of any of claims 13 or 14, wherein the parent metal comprises aluminum and the polycrystalline oxidation reaction product comprises alumina.
Claim 23
Independent Claim
36 words
The method of any of claims 13 or 14, wherein the interconnected porosity is between about 5 to 45% by volume of the ceramic composite body before the ceramic composite body has a polymer disposed therein.
Claim 24
Independent Claim
236 words
A method of producing a self-supporting ceramic body by oxidation of a parent metal to form a polycrystalline material comprising (i) an oxidation reaction product of said parent metal with a vapor-phase oxidant and (ii) at least some residual parent metal which comprises: (a) heating said parent metal to a temperature above its melting point, but below the melting point of its oxidation reaction product to form a body of molten parent metal; (b) reacting said body of molten parent metal with said vapor-phase oxidant at said temperature to form oxidation reaction product; (c) maintaining at least a portion of said oxidation reaction product in contact with and between said body of molten parent metal and said oxidant, to draw molten parent metal through the oxidation reaction product towards the oxidant so that fresh oxidation reaction product continues to form at an interface between the oxidant and previously formed oxidation reaction product; (d) continuing said reaction for a time sufficient to produce said ceramic body; (e) forming at least some porosity in said ceramic body by utilizing at least one treatment step selected from the group consisting of taking the oxidation reaction process to completion, vaporizing residual parent metal from the ceramic body and leaching residual parent metal from the ceramic body; and (f) disposing a polymer into at least a portion of said formed porosity, thereby forming a ceramic composite body containing a polymer component.
Claim 25
Independent Claim
236 words
A method of producing a self-supporting ceramic body by oxidation of a parent metal to form a polycrystalline material comprising (i) an oxidation reaction product of said parent metal with a vapor-phase oxidant and (ii) at least some residual parent metal which comprises: (a) heating said parent metal to a temperature above its melting point, but below the melting point of its oxidation reaction product to form a body of molten parent metal; (b) reacting said body of molten parent metal with said vapor-phase oxidant at said temperature to form oxidation reaction product; (c) maintaining at least a portion of said oxidation reaction product in contact with and between said body of molten parent metal and said oxidant, to draw molten parent metal through the oxidation reaction product towards the oxidant so that fresh oxidation reaction product continues to form at an interface between the oxidant and previously formed oxidation reaction product; (d) continuing said reaction for a time sufficient to produce said ceramic body; (e) forming at least some porosity in said ceramic body by utilizing at least one treatment step selected from the group consisting of taking the oxidation reaction process to completion, vaporizing residual parent metal from the ceramic body and leaching residual parent metal from the ceramic body; and (f) disposing a polymer into at least a portion of said formed porosity, thereby forming a ceramic composite body containing a polymer component.
References Cited (Backward Citations)
US3172775A
Cited
US2657153A
Cited
US2741822A
Cited
US3255027A
Cited
US3298842A
Cited
US3296002A
Cited
US3419404A
Cited
US3473987A
Cited
US3421863A
Cited
US3437468A
Cited
US3789096A
Cited
US3473938A
Cited
US3713867A
Cited
US3607681A
Cited
US3712830A
Cited
US3926702A
Cited
US3864154A
Cited
US3973977A
Cited
US4119763A
Cited
US4000982A
Cited
US4215161A
Cited
US4267211A
Cited
US4204021A
Cited
US4299865A
Cited
US4551358A
Cited
US4536358A
Cited
EP0116809A1
Cited
US4525429A
Cited
US4591480A
Cited
EP0155831A2
Cited
EP0169067A2
Cited
EP0193292A2
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1993-01-08 | 1993-07-10 | 1994-01-09 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1997-01-08 | 1997-07-10 | 1998-01-09 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2001-01-08 | 2001-07-10 | 2002-01-09 | $7700.00 | Window Closed / Lapsed |