← Back to Patent Explorer
US4880583A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for reduction of mold cycle time

Assignee: Shell USA Inc
•
Filing: 1988-05-23
•
Granted: 1989-11-14
•
Expires: 2008-05-23
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for the reductin of mold cycle time. A heat recoverable member in a compressed state is placed within a channel defined relative to the surface of a mold. A hardenable liquid used to form the article then flows in an accelerated manner through the channel. Thermal energy supplied to the heat recoverable material causes the heat recoverable material to expand within the channel, thereby displacing the hardenable liquid from the channel. The temperature of gelation of the hardenable liquid and the recovery temperature of the heat recoverable material may be selected such that the channels are substantially filled by the heat recoverable material prior to the hardening of the hardenable liquid. In this manner, the heat recoverable material becomes flush with the surface of the mold prior to hardening of the liquid so as to yield an article of manufacture having a relatively planar surface.

Inventors

  • 👤 Paul I. Douglas

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 01:14
CPC Classifications
B; B29; B29C; B29C45/00; B29C45/17; B29C45/76; B29C33/00; B29C33/0061; B29C33/42; B29C70/00; B29C70/04; B29C70/28; B29C70/40; B29C70/42; B29C70/46; B29C70/48; B29C70/54; B29C70/546; B29C70/548; Y; Y02; Y02P; Y02P70/00; Y02P70/10

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 203 words
A method for reducing the fabrication time of a molded article of manufacture wherein a portion of said molded article is formed by a hardenable liquid, said method including the steps of: providing a mold having two mold section surfaces with at least one of said surfaces having one hardenable liquid injection port defined therethrough, at least one of said mold section surfaces having at least one channel with an associated channel surface and channel opening defined relative to said mold surface, providing a heat-recoverable member, said member previously having been deformed under heat and/or pressure from an expanded first configuration to a compressed second configuration, said member when subjected to a suitable temperature of recovery capable of recovering to or towards its expanded first configuration, locating said heat recoverable member within a portion of said channel, flowing said hardenable liquid into said mold, heating said heat recoverable member at least to said suitable temperature of recovery, thereby expanding said heat recoverable member to said first configuration within said channel, retaining said hardenable liquid in said mold for a sufficient period for said liquid to harden sufficiently to dimensionally stabilize said article of manufacture, and removing said article of manufacture from said mold.
Claim 2
Independent Claim 203 words
A method for reducing the fabrication time of a molded article of manufacture wherein a portion of said molded article is formed by a hardenable liquid, said method including the steps of: providing a mold having two mold section surfaces with at least one of said surfaces having one hardenable liquid injection port defined therethrough, at least one of said mold section surfaces having at least one channel with an associated channel surface and channel opening defined relative to said mold surface, providing a heat-recoverable member, said member previously having been deformed under heat and/or pressure from an expanded first configuration to a compressed second configuration, said member when subjected to a suitable temperature of recovery capable of recovering to or towards its expanded first configuration, locating said heat recoverable member within a portion of said channel, flowing said hardenable liquid into said mold, heating said heat recoverable member at least to said suitable temperature of recovery, thereby expanding said heat recoverable member to said first configuration within said channel, retaining said hardenable liquid in said mold for a sufficient period for said liquid to harden sufficiently to dimensionally stabilize said article of manufacture, and removing said article of manufacture from said mold.
Claim 3
Dependent Claim 70 words
The method of claim 1 wherein the step of providing a heat recoverable member previously having been deformed under heat and/or pressure from an expanded first configuration to a compressed second configuration, further includes the step of: defining the shape of said expanded first configuration in the shape of said channel opening, so as to define a surface planar to said mold surface when said heat recoverable member is expanded.
Claim 4
Dependent Claim 31 words
The method of claim 1 wherein the step of heating said heat recoverable member at least to said temperature of recovery is done by thermal energy supplied to heat said mold.
Claim 5
Dependent Claim 31 words
The method of claim 1 wherein the step of heating said heat recoverable member at least to said temperature of recovery is done by thermal energy supplied to said hardenable liquid.
Claim 6
Dependent Claim 32 words
The method of claim 1 further including, subsequent to the step of locating said heat recoverable member within a portion of said channel, the step of positioning filament matrix in said mold.
Claim 7
Dependent Claim 43 words
The method of claim 1 further including, subsequent to the step of locating said heat recoverable member within said opening, the step of coating with a parting agent at least the portion of the surface of the member located adjacent said mold surface.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-11-13 1993-05-15 1993-11-14 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-11-13 1997-05-15 1997-11-14 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-11-13 2001-05-15 2001-11-14 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag