Abstract

Abstract A heat resistant copolymer composition is provided by blending two kinds of copolymers one of which is obtainable by polymerizing a maleimide monomer (A), an aromatic vinyl monomer (B), an unsaturated nitrile monomer (C) and optionally at least one other comonomer copolymerizable therewith (D) in a specific monomer ratio in the presence or absence of an elastomeric polymer and which has an intrinsic viscosity of 0.3 to 1.2 dl/g, and another of which is obtainable by copolymerizing the aromatic vinyl monomer (B), the unsaturated nitrile (C) and optionally at least one other comonomer copolymerizable therewith (D) in a specific monomer ratio in the presence or absence of the elastomeric polymer and which has an intrinsic viscosity of 0.3 to 1.5 dl/g.

Inventors

  • 👤 Masatsune Kondo
  • 👤 Kiyoshi Ogura
  • 👤 Koiti Kuramoto

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 21:23
CPC Classifications
C; C08; C08L; C08L25/00; C08L25/02; C08L25/04; C08L25/08; C08L25/12; C08L25/16; C08L33/00; C08L33/18; C08L35/00; C08L35/06

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 415 words
A heat resistant copolymer composition comprising: 5 to 95% by weight of a copolymer (I) which is obtainable by copolymerizing (A) a maleimide monomer (B) an aromatic vinyl monomer, (C) an unsaturated nitrile monomer, and 0% to 50% by weight of the total weight of (A), (B), (C), and (D) of (D) at least one other comonomer copolymerizable with (A), (B) and (C) in the presence of 0% to 80% by weight of the total weight of (A), (B), (C), (D) and (E) of (E) an elastomeric polymer and has an intrinsic viscosity of 0.3 to 1.2 dl/g, and 95 to 5% by weight of a copolymer (II) which is obtainable by copolymerizing (B) the aromatic vinyl monomer, (C) the unsaturated nitrile and 0 to 50% by weight of the total weight of (B), (C) and (D) of (D) at least one other comonomer copolymerizable with (B) and (C) in the presence of 0% to 80% by weight of the total weight of (B), (C), (D) and (E) of (E) an elastic polymer and has an intrinsic viscosity of 0.3 to 1.5 dl/g, wherein the total weight percentage of the monomers (A) and (C) in the copolymer (I) per total weight of the monomers (A), (B), (C) and (D) in the copolymer (I) and the weight percentage of the monomer (C) in the copolymer (II) per total weight of the monomers (B), (C) and (D) in the copolymer (II) satisfy the following equation: (Said total weight percentage of the monomers (A) and (C) in copolymer (I))-(Said weight percentage of the monomer (C) in copolymer (II))=+40 to -15% by weight, and wherein the intrinsic viscosities of the copolymers (I) and (II) satisfy the following equation: (The intrinsic viscosity of the copolymer(I))-(The intrinsic viscosity of the copolymer (II))=+0.5 to -1.2 dl/g, wherein all intrinsic viscosities refer to the intrinsic viscosity of the non-grafted polymers, when grafted polymers are present, said copolymer (I) having a composition of the monomers (A), (B), (C) and (D) satisfying the following equations (1), (2), and (3) wherein (A), (B), (C) and (D) stand for the respective weights thereof: ##EQU10## where (F) ranges from 1 to 60% by weight, (G) ranges from 99 to 40% by weight and (H) ranges from 5 to 45% by weight, said copolymer (II) having a composition of the monomers (B) and (C) satisfying the following equation (4) wherein (B) and (C) stand for the respective weights thereof: ##EQU11## where (J) ranges from 20 to 45% by weight.
Claim 2
Dependent Claim 415 words
A heat resistant copolymer composition comprising: 5 to 95% by weight of a copolymer (I) which is obtainable by copolymerizing (A) a maleimide monomer (B) an aromatic vinyl monomer, (C) an unsaturated nitrile monomer, and 0% to 50% by weight of the total weight of (A), (B), (C), and (D) of (D) at least one other comonomer copolymerizable with (A), (B) and (C) in the presence of 0% to 80% by weight of the total weight of (A), (B), (C), (D) and (E) of (E) an elastomeric polymer and has an intrinsic viscosity of 0.3 to 1.2 dl/g, and 95 to 5% by weight of a copolymer (II) which is obtainable by copolymerizing (B) the aromatic vinyl monomer, (C) the unsaturated nitrile and 0 to 50% by weight of the total weight of (B), (C) and (D) of (D) at least one other comonomer copolymerizable with (B) and (C) in the presence of 0% to 80% by weight of the total weight of (B), (C), (D) and (E) of (E) an elastic polymer and has an intrinsic viscosity of 0.3 to 1.5 dl/g, wherein the total weight percentage of the monomers (A) and (C) in the copolymer (I) per total weight of the monomers (A), (B), (C) and (D) in the copolymer (I) and the weight percentage of the monomer (C) in the copolymer (II) per total weight of the monomers (B), (C) and (D) in the copolymer (II) satisfy the following equation: (Said total weight percentage of the monomers (A) and (C) in copolymer (I))-(Said weight percentage of the monomer (C) in copolymer (II))=+40 to -15% by weight, and wherein the intrinsic viscosities of the copolymers (I) and (II) satisfy the following equation: (The intrinsic viscosity of the copolymer(I))-(The intrinsic viscosity of the copolymer (II))=+0.5 to -1.2 dl/g, wherein all intrinsic viscosities refer to the intrinsic viscosity of the non-grafted polymers, when grafted polymers are present, said copolymer (I) having a composition of the monomers (A), (B), (C) and (D) satisfying the following equations (1), (2), and (3) wherein (A), (B), (C) and (D) stand for the respective weights thereof: ##EQU10## where (F) ranges from 1 to 60% by weight, (G) ranges from 99 to 40% by weight and (H) ranges from 5 to 45% by weight, said copolymer (II) having a composition of the monomers (B) and (C) satisfying the following equation (4) wherein (B) and (C) stand for the respective weights thereof: ##EQU11## where (J) ranges from 20 to 45% by weight.
Claim 3
Dependent Claim 58 words
The heat resistant copolymer composition according to claim 1 which comprises 5 to 90% by weight of the copolymer (I), 5 to 90% by weight of the copolymer (II) and further 0.5 to 90% by weight of at least one polymeric component other than copolymers (I) and (II) selected from the group consisting of thermoplastic resins and elastomers.
Claim 4
Dependent Claim 63 words
The heat resistant copolymer composition according to claim 1, wherein the amount of comonomer (C) for copolymer (I) ranges from 0 to 40% by weight of the total weight of (A), (B), (C) and (D) for copolymer (I), (F) ranges from 5 to 50% by weight, (G) ranges from 95 to 50% by weight and (H) ranges from 10 to 40% by weight.
Claim 5
Dependent Claim 63 words
The heat resistant copolymer composition according to claim 2 wherein the amount of comonomer (D) for copolymer (I) ranges from 0 to 40% by weight of the total weight of (A), (B), (C) and (D) for copolymer (I), (F) rages from 5 to 50% by weight, (G) ranges from 95 to 50% by weight, and (H) ranges from 10 to 40% by weight.
Claim 6
Dependent Claim 46 words
The heat resistant copolymer composition according to claim 1, wherein the amount of comonomer (D) for copolymer (II) ranges for 0 to 30% by weight of the total weight of (B), (C) and (D) for copolymer (II) and (J) ranges from 20 to 40% by weight.
Claim 7
Dependent Claim 46 words
The heat resistant copolymer composition according to claim 2, wherein the amount of comonomer (D) for copolymer (II) ranges from 0 to 30% by weight of the total weight of (B), (C) and (D) for copolymer (II) and (J) ranges from 20 to 40% by weight.
Claim 8
Dependent Claim 83 words
The heat resistant copolymer composition according to claim 1, wherein the total weight percentage of the maleimide monomer (A) and the unsaturated nitrile monomer (C) per total weight of the monomers (A), (B), (C) and (D) in the copolymer (I) and the weight percentage of the unsaturated nitrile monomer (C) per total weight of the monomers (B), (C) and (D) in the copolymer (II) satisfy the following equation: ##EQU12## the intrinsic viscosities of the copolymers (I) and (II) satisfy the following equation: ##EQU13##
Claim 9
Dependent Claim 83 words
The heat resistant copolymer composition according to claim 2, wherein the total weight percentage of the maleimide monomer (A) and the unsaturated nitrile monomer (C) per total weight of the monomers (A), (B), (C) and (D) in the copolymer (I) and the weight percentage of the unsaturated nitrile monomer (C) per total weight of the monomers (B), (C) and (D) in the copolymer (II) satisfy the following equation: ##EQU14## the intrinsic viscosities of the copolymers (I) and (II) satisfy the following equation: ##EQU15##
Claim 10
Dependent Claim 29 words
The heat resistant copolymer composition according to claim 2 wherein said polymeric component is selected from the group consisting of polyester, polycarbonate, polyamide, ethylene/glycidyl methacrylate copolymer and acrylonitrile-butadiene copolymer.

References Cited (Backward Citations)

US4567233A Cited
US4699947A Cited
US4608414A Cited
US4663390A Cited
US4559386A Cited
US4701493A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-10-30 1993-05-01 1993-10-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-10-30 1997-05-01 1997-10-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-10-30 2001-05-01 2001-10-31 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag