Claims Analysis
Total Claims: 11
Claim 1
Independent Claim
325 words
A method of fabricating a bipolar transistor on a semiconductor substrate, comprising steps of: forming a first polycrystalline silicon layer over a main surface of a silicon substrate having a first conductivity type land region; forming an antioxidizing film in selected areas over the surface of the first polycrystalline silicon layer; selectively oxidizing portions of the first polycrystalline silicon layer using the antioxidizing film as a mask; introducing a second conductivity type impurity through the antioxidizing film into at least some unoxidized portions of the first polycrystalline silicon layer; forming an opening by selectively removing the oxidized first polycrystalline silicon layer to expose a part of the land region; forming a thin oxide film over the surface of the exposed land region and a side surface of the opening; forming a first region of the second conductivity type in the unexposed land region; forming a second region of the second conductivity type disposed on a side of the first region by introducing a second conductivity type impurity through the thin oxide film into the land region; forming a first oxide film through a CVD process over an entire surface of the structure obtained by said steps; forming a second polycrystalline silicon layer over an entire surface of the oxide film; selectively removing the second polycrystalline silicon layer through an anisotropic etching process so as to be remained the second polycrystalline silicon layer only on the side surface of the opening; etching the exposed first oxide film and thin oxide film to expose the second region; selectively forming a third polycrystalline silicon layer dopsed the first conductivity type impurity at least on the exposed second region; diffusing the first conductivity type impurity from the third polycrystalline silicon layer into the second region to form a third region of the first conductivity type in the second region; and forming a metal silicide film at least over the surface of a portion of the first polycrystalline silicon layer.
Claim 2
Independent Claim
325 words
A method of fabricating a bipolar transistor on a semiconductor substrate, comprising steps of: forming a first polycrystalline silicon layer over a main surface of a silicon substrate having a first conductivity type land region; forming an antioxidizing film in selected areas over the surface of the first polycrystalline silicon layer; selectively oxidizing portions of the first polycrystalline silicon layer using the antioxidizing film as a mask; introducing a second conductivity type impurity through the antioxidizing film into at least some unoxidized portions of the first polycrystalline silicon layer; forming an opening by selectively removing the oxidized first polycrystalline silicon layer to expose a part of the land region; forming a thin oxide film over the surface of the exposed land region and a side surface of the opening; forming a first region of the second conductivity type in the unexposed land region; forming a second region of the second conductivity type disposed on a side of the first region by introducing a second conductivity type impurity through the thin oxide film into the land region; forming a first oxide film through a CVD process over an entire surface of the structure obtained by said steps; forming a second polycrystalline silicon layer over an entire surface of the oxide film; selectively removing the second polycrystalline silicon layer through an anisotropic etching process so as to be remained the second polycrystalline silicon layer only on the side surface of the opening; etching the exposed first oxide film and thin oxide film to expose the second region; selectively forming a third polycrystalline silicon layer dopsed the first conductivity type impurity at least on the exposed second region; diffusing the first conductivity type impurity from the third polycrystalline silicon layer into the second region to form a third region of the first conductivity type in the second region; and forming a metal silicide film at least over the surface of a portion of the first polycrystalline silicon layer.
Claim 3
Dependent Claim
47 words
A method of of fabricating a bipolar transistor according to claim 1, wherein said first conductivity type is an n-type, said second conductivity type is a p-type, said first conductivity type impurity is arsenic, and said second conductivity type impurity is boron or a compound containing boron.
Claim 4
Dependent Claim
18 words
A method of fabricating a bipolar transistor according to claim 1, wherein said metal silicide is platinum silicide.
Claim 5
Independent Claim
371 words
A method of fabricating a bipolar transistor on a semiconductor substrate, comprising steps of: forming a first polycrystalline silicon layer over a main surface of a semiconductor substrate of a first conductivity type having a first and a second land regions of a second conductivity type on the main surface thereof, the first and the second land regions connected to each other; selectively oxidizing the first polycrystalline silicon layer excepting a first, a second and a third areas thereof, a portion of the first and the second areas located on the first land region; the third area located on the second land region; introducing a first conductivity type impurity into the first and second areas of the first polycrystalline silicon layer and a second conductivity type impurity into a collector area of the first polycrystalline silicon layer; selectively removing the oxidized first polycrystalline silicon layer located between the first and the second areas to form an opening; oxidizing the structure obtained by said steps to form a thin oxide film over the surface of the opening and to diffuse a first conductivity type impurity from the first and second areas to the substrate whereby a first and a second inactive base regions of the first conductivity type is defined in the first region; introducing the first conductivity type impurity through the thin oxide film to the first region to form an active base region connected between the first and second inactive bases in the first region; alternately forming an oxide film and a second polycrystalline silicon layer on an entire surface of the structure obtained by said steps; removing the second polycrystalline silicon layer, the oxide film and, the thin oxide film by an reactive ion etching process to expose said active base region whereby the second polycrystalline silicon layer located on a side surface of the opening only remains and the third area of the first polycrystalline silicon layer is exposed as a collector electrode; forming a third polycrystalline silicon layer of the second conductivity type on the entire surface of the structure obtained by said steps; and diffusing the first conductivity type impurity from the third polycrystalline silicon layer to the inactive base region to form an emitter region.
Claim 6
Independent Claim
371 words
A method of fabricating a bipolar transistor on a semiconductor substrate, comprising steps of: forming a first polycrystalline silicon layer over a main surface of a semiconductor substrate of a first conductivity type having a first and a second land regions of a second conductivity type on the main surface thereof, the first and the second land regions connected to each other; selectively oxidizing the first polycrystalline silicon layer excepting a first, a second and a third areas thereof, a portion of the first and the second areas located on the first land region; the third area located on the second land region; introducing a first conductivity type impurity into the first and second areas of the first polycrystalline silicon layer and a second conductivity type impurity into a collector area of the first polycrystalline silicon layer; selectively removing the oxidized first polycrystalline silicon layer located between the first and the second areas to form an opening; oxidizing the structure obtained by said steps to form a thin oxide film over the surface of the opening and to diffuse a first conductivity type impurity from the first and second areas to the substrate whereby a first and a second inactive base regions of the first conductivity type is defined in the first region; introducing the first conductivity type impurity through the thin oxide film to the first region to form an active base region connected between the first and second inactive bases in the first region; alternately forming an oxide film and a second polycrystalline silicon layer on an entire surface of the structure obtained by said steps; removing the second polycrystalline silicon layer, the oxide film and, the thin oxide film by an reactive ion etching process to expose said active base region whereby the second polycrystalline silicon layer located on a side surface of the opening only remains and the third area of the first polycrystalline silicon layer is exposed as a collector electrode; forming a third polycrystalline silicon layer of the second conductivity type on the entire surface of the structure obtained by said steps; and diffusing the first conductivity type impurity from the third polycrystalline silicon layer to the inactive base region to form an emitter region.
Claim 7
Dependent Claim
63 words
A method of fabricating a bipolar transistor according to claim 4, wherein said selectively oxidizing step of first polycrystalline silicon layer comprises steps of: selectively forming an antioxidizing film over the first, the second and the third areas of the first polycrystalline silicon layer; selectively oxidezing the first polycrystalline silicon layer using the antioxidizing film as a mask; and removing the antioxidizing film.
Claim 8
Dependent Claim
54 words
A method of fabricating a bipolar transistor according to claim 5, wherein said antioxidizing film located over the first and second areas are removed after forming an emitter region, and said antioxidizing film located over the third area is removed before introducing the impurity into said third area of the first polycrystalline silicon layer.
Claim 9
Dependent Claim
37 words
A method of fabricating a bipolar transistor according to claim 4, wherein said method further comprises steps of: annealing the structure obtained by introducing the impurity into the first and second areas to uniformly distribute said impurity.
Claim 10
Dependent Claim
25 words
A method of fabricating a bipolar transistor according to claim 4, wherein said second polycrystalline silicon layer is formed by a chemical vapor deposition process.
Claim 11
Dependent Claim
51 words
A method of fabricating a bipolar transistor according to claim 4, wherein said third polycrystalline silicon layer forming step comprises steps of: forming a third polycrystalline silicon layer; oxidizing a surface of the third layer to form thin oxide film; and introducing the first conductivity type impurity into the third layer.