Abstract An optical recording medium comprising practically a naphthalocyanine dye represented by the following general formula (I): ##STR1## wherein M means a metal, metal oxide or metal halide, and --OR 1 , --OR 2 , --OR 3 and --OR 4 are the same or different and denote ether groups respectively having R 1 , R 2 , R 3 and R 4 each of which is a saturated or unsaturated hydrocarbon group having 4-12 carbon atoms.

Inventors

  • 👤 Sumio Hirose
  • 👤 Hiroshi Ozawa
  • 👤 Kenji Abe
  • 👤 Yoichi Hosono
  • 👤 Shigeru Takahara
  • 👤 Tadashi Koike

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 23:13
CPC Classifications
G; G11; G11B; G11B7/00; G11B7/24; G11B7/241; G11B7/242; G11B7/244; G11B7/246; G11B7/248; Y; Y10; Y10S; Y10S430/00; Y10S430/146

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 110 words
An optical recording medium permitting recording and reading-out of signals, comprising a transparent substrate and an optically reflective recording layer provided directly on said substrate, said recording layer having an amount of resinous binder therein of substantially 0 wt. % and containing a napthalocyanine dye having the formula (I): ##STR4## wherein M is a metal, metal oxide or metal halide, and --OR 1 , --OR 2 , --OR 3 and --OR 4 are the same or different and denote ether groups, respectively, having R 1 , R 2 , R 3 and R 4 each of which is a saturated or unsaturated hydrocarbon group having 4 to 12 carbon atoms.
Claim 2
Dependent Claim 110 words
An optical recording medium permitting recording and reading-out of signals, comprising a transparent substrate and an optically reflective recording layer provided directly on said substrate, said recording layer having an amount of resinous binder therein of substantially 0 wt. % and containing a napthalocyanine dye having the formula (I): ##STR4## wherein M is a metal, metal oxide or metal halide, and --OR 1 , --OR 2 , --OR 3 and --OR 4 are the same or different and denote ether groups, respectively, having R 1 , R 2 , R 3 and R 4 each of which is a saturated or unsaturated hydrocarbon group having 4 to 12 carbon atoms.
Claim 3
Dependent Claim 29 words
The optical recording medium as claimed in claim 1, wherein said transparent substrate has a transmittance of light of 85% or higher, and is substantially free of optical anisotrophy.
Claim 4
Dependent Claim 19 words
The optical recording medium as claimed in claim 2, wherein said transparent substrate is a glass or plastic material.
Claim 5
Dependent Claim 70 words
The optical recording medium as claimed in claim 1, wherein said ether groups --OR 1 , --OR 2 , --OR 3 and --OR 4 are selected from the group consisting of n-butoxy, sec-butoxy, tert-butoxy, n-pentoxy, iso-pentoxy, sec-pentoxy, tert-pentoxy, n-hexoxy, iso-hexoxy, 1-methyl-1-ethylpropioxy, 1,1-dimethylbutoxy, n-heptoxy, iso-heptoxy, sec-heptoxy, tert-heptoxy, octoxy, 2-ethylhexoxy, nonyloxy, decyloxy, dodecyloxy, cyclohexyloxy, methylcyclohexyloxy, allyloxy, butenoxy, hexenoxy, octenoxy, dodecenoxy, cyclohexenoxy, methylcyclohexenoxy, phenoxy, methylphenoxy, ethylphenoxy, dimethylphenoxy, butylphenoxy, hexylphenoxy, benzyloxy, phenylethoxy and phenylhexoxy.
Claim 6
Dependent Claim 64 words
The optical recording medium as claimed in claim 1, wherein said metal, metal oxide or metal halide M is selected from the group consisting of a Group Ib metal, a Group II metal, a Group III metal, a Group IV metal, a Group V metal, a Group VI metal, a Group VIII metal, and a Group VIII metal and the oxides and halides thereof.
Claim 7
Dependent Claim 48 words
The optical recording medium as claimed in claim 5, wherein said metal, metal oxide or metal halide M is selected from the group consisting of Cu, Ni, Mg, Pd, Co, Nb, Sn, In, Ge, Ga, VO, TiO and the chloride, bromide or oxide of Al, Ga and In.
Claim 8
Dependent Claim 38 words
The optical recording medium as claimed in claim 6, wherein said metal, metal oxide or metal halide M is selected from the group consisting of VO, TiO, In, In--Cl, In--Br, Al--Cl, Al--Br, Ga--Cl, Ga--Br, Al--O--AI, Ga--O--Ga and In--O--In.

References Cited (Backward Citations)

US4458004A Cited
US4492750A Cited
US4725525A Cited
US4719613A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-08-21 1993-02-20 1993-08-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-08-21 1997-02-20 1997-08-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-08-21 2001-02-20 2001-08-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag