Claims Analysis
Total Claims: 22
Claim 1
Independent Claim
261 words
A method for producing a self-supporting ceramic structure comprising a polycrystalline material comprised of a first region and a terminal region integral with said first region but differing therefrom in at least one property selected from the group consisting of composition and microstructure, the method comprising the steps of: (a) heating a parent metal to a temperature range above its melting point but below the melting point of the oxidation reaction product to form a body of molten parent metal; and (b) within said temperature range, (i) reacting said body of molten parent metal with an oxidant to form said oxidation reaction product, (ii) initially maintaining at least a portion of said oxidation reaction product in contact with and between said body of molten parent metal and said oxidant to progressively transport molten parent metal from said body of molten parent metal through the oxidation reaction product and towards the oxidant, so that oxidation reaction product continues to form at the interface between the oxidant and previously formed oxidation reaction product, thereby forming a progressively thicker first region of oxidation reaction product initially containing interconnected parent metal; (c) attenuating said transport of molten parent metal from said body of molten parent metal, and (d) after step (c) resuming a reaction between at least a portion of said interconnected parent metal from said first region of oxidation reaction product toward a surface of said first region to form oxidation reaction product on said surface and continuing said resumed reaction for a time sufficient to form a terminal region of oxidation reaction product.
Claim 2
Independent Claim
261 words
A method for producing a self-supporting ceramic structure comprising a polycrystalline material comprised of a first region and a terminal region integral with said first region but differing therefrom in at least one property selected from the group consisting of composition and microstructure, the method comprising the steps of: (a) heating a parent metal to a temperature range above its melting point but below the melting point of the oxidation reaction product to form a body of molten parent metal; and (b) within said temperature range, (i) reacting said body of molten parent metal with an oxidant to form said oxidation reaction product, (ii) initially maintaining at least a portion of said oxidation reaction product in contact with and between said body of molten parent metal and said oxidant to progressively transport molten parent metal from said body of molten parent metal through the oxidation reaction product and towards the oxidant, so that oxidation reaction product continues to form at the interface between the oxidant and previously formed oxidation reaction product, thereby forming a progressively thicker first region of oxidation reaction product initially containing interconnected parent metal; (c) attenuating said transport of molten parent metal from said body of molten parent metal, and (d) after step (c) resuming a reaction between at least a portion of said interconnected parent metal from said first region of oxidation reaction product toward a surface of said first region to form oxidation reaction product on said surface and continuing said resumed reaction for a time sufficient to form a terminal region of oxidation reaction product.
Claim 3
Dependent Claim
24 words
The method of claim 1, including continuing said resumed reaction at least to a point of exhaustion of said body of molten parent metal.
Claim 4
Dependent Claim
86 words
The method of claim 1, including orienting a mass of filler material and at least one growth material selected from the group consisting of said parent metal and said first region of oxidation reaction product relative to each other so that said at least one growth material grows towards and into said mass of filler material, whereby at least a portion of said mass of filler material is embedded by said at least one growth material to provide said ceramic structure as a ceramic composite body.
Claim 5
Independent Claim
52 words
The method of any one of claims 1, 2 or 3, including forming of at least a portion of said first region in a first reacting stage, followed by interrupting said first reacting stage in an interim stage and, after said interim stage, forming said terminal region in a second reaction stage.
Claim 6
Dependent Claim
23 words
The method of claim 4, wherein said interim stage includes allowing said first region of oxidation reaction product to cool to ambient temperature.
Claim 7
Dependent Claim
71 words
The method of claim 4, including terminating said first reacting stage prior to exhaustion of said body of parent metal and, in said interim stage, separating at least a portion of said first region of oxidation reaction prodcut from said body of parent metal, and therafter carrying out said second reacting stage on said at least a portion of said first region out of contact with said body of parent metal.
Claim 8
Dependent Claim
19 words
The method of claim 6, including shaping the separated first region prior to carrying out said second reacting stage.
Claim 9
Dependent Claim
78 words
The method of claim 1, including forming at least a portion of said first region of oxidation reaction product in a first reacting stage and thereafter orienting a mass of filler material and said first region relative to each other so that upon forming said terminal region grows towards and into said filler material, whereby at least a portion of said filler material is embedded by said terminal region and said ceramic structure comprises a ceramic composite structure.
Claim 10
Dependent Claim
115 words
The method of claim 1, including providing said ceramic structure as a ceramic composite structure by (1) orienting said parent metal and a mass of first filler material relative to each other and, in a first reacting stage, forming said first region of oxidation reaction product towards and into said first filler material to embed at least a portion of said first filler material therein, and (2) thereafter orienting the first region of oxidation reaction product and a mass of second filler material relative to each other and, during formation of said terminal region, growing said terminal region into said second filler material to embed at least a portion of said second filler material therein.
Claim 11
Dependent Claim
21 words
The method of claim 9, wherein said first filler material comprises a material which is different from said second filler material.
Claim 12
Independent Claim
23 words
The method of any one of claims 1, 2, 3, 6, 7, 8, 9 or 10, wherein said oxidant is a vapor-phase oxidant.
Claim 13
Dependent Claim
43 words
The method of claim 11, wherein said vapor-phase oxidant comprises an oxygen containing gas, said parent metal comprises an aluminum parent, metal, said polycrystalline material is comprised of alpha-alumina, and including using at least one suitable dopant in conjunction with said parent metal.
Claim 14
Dependent Claim
23 words
The method of claim 12, wherein said oxidant comprises air and said temperature range is from about 850° C. to about 1450° C.
Claim 15
Independent Claim
30 words
The method of any one of claims 1, 2, 3, 6, 7, 8, 9 or 10, including using at least one suitable dopant material in conjunction with said parent metal.
Claim 16
Dependent Claim
14 words
The method of claim 14, wherein said parent metal comprises an aluminum parent metal.
Claim 17
Independent Claim
28 words
The method of any one of claims 1, 2, 3, 6, 7, 8, 9 or 10, wherein said terminal region has a finer microstructure than said first region.
Claim 18
Dependent Claim
52 words
The method of anyone of claim 1, 2, 3, 6, 7, 8, 9 or 10, including interposing a barrier means in at least a portion of the path of formation of at least one of said first region and said terminal region to thereby limit and define the extent of such formation.
Claim 19
Dependent Claim
59 words
The method of claim 17, including orienting said barrier means and said parent metal relative to each other so that growth of said terminal region is prevented in the vicinity of said barrier means but occurs in at least one other direction in which the path of formation of said first region is not blocked by said barrier means.
Claim 20
Independent Claim
38 words
The method of any one of claims 1, 2, 3, 6, 7, 8, 9 or 10, including forming said first region of polycrystalline material to a preselected geometry and thereafter forming said terminal region on said first region.
Claim 21
Dependent Claim
19 words
The method of claim 4, including using at least one suitable dopant material in conjunction with said parent metal.
Claim 22
Dependent Claim
14 words
The method of claim 20, wherein said parent metal comprises an aluminum parent metal.