Abstract
Abstract A terminal pin seal for an hermetic terminal assembly including at least two laminations one of which has the inner surface adjacent the assembly structure with electrochemical properties resistant to attack from chemical ingredients within the assembly and another of which laminations has the outer surface adjacent to ambient with electrochemical properties different from that lamination facing the assembly housing to produce a greater resistance to chemical attack from ambient.
Inventors
- 👤 Richard L. Teaford
- 👤 Glenn A. Honkomp
- 👤 Donald H. Hall
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-30 20:26
CPC Classifications
H; H01; H01B; H01B17/00; H01B17/26; H01B17/30; H01B17/303; H01B17/305; H01M; H01M50/00; H01M50/10; H01M50/183; H01M50/186; H01M50/188; H01M50/19; H01M50/191; H10; H10W; H10W95/00; Y; Y02; Y02E; Y02E60/00; Y02E60/10
Claims Analysis
Total Claims: 12
Claim 1
Independent Claim
240 words
In an hermetic terminal assembly having a terminal pin extending from within the assembly through an apertured assembly wall to ambient, said assembly housing having a corrosive environment, an improved aperture seal structure between said pin and assembly wall comprising: a first substantially flat aperture sealing lamination having spaced inner and outer planar surfaces extending continuously between the outer peripheral surface of said terminal pin and the periphery of said assembly wall aperture with said inner surface of said first lamination being adjacent and exposed to said corrosive environment of said assembly structure, said first sealing lamination having corrosive resistant properties to produce a preselected resistance to attack from ingredients producing said corrosive environment within the assembly; and, a second flat aperture sealing lamination having spaced inner and outer planar surface extending continuously between the outer peripheral surface of said terminal pin and the periphery of said assembly wall aperture with said outer surface adjacent ambient, said second aperture sealing lamination having corrosion resistant properties different from those of said first aperture sealing lamination to produce a preselected resistance to attack from ambient conditions; said first and said second sealing laminations being of different corrosive resistant properties but with similar viscosities having setting points within approximately 10° C. of each other and coefficients of expansion within approximately 1% of each other which coefficients of expansion are compatible with that of the material to which the sealing laminations are sealingly bonded.
Claim 2
Dependent Claim
240 words
In an hermetic terminal assembly having a terminal pin extending from within the assembly through an apertured assembly wall to ambient, said assembly housing having a corrosive environment, an improved aperture seal structure between said pin and assembly wall comprising: a first substantially flat aperture sealing lamination having spaced inner and outer planar surfaces extending continuously between the outer peripheral surface of said terminal pin and the periphery of said assembly wall aperture with said inner surface of said first lamination being adjacent and exposed to said corrosive environment of said assembly structure, said first sealing lamination having corrosive resistant properties to produce a preselected resistance to attack from ingredients producing said corrosive environment within the assembly; and, a second flat aperture sealing lamination having spaced inner and outer planar surface extending continuously between the outer peripheral surface of said terminal pin and the periphery of said assembly wall aperture with said outer surface adjacent ambient, said second aperture sealing lamination having corrosion resistant properties different from those of said first aperture sealing lamination to produce a preselected resistance to attack from ambient conditions; said first and said second sealing laminations being of different corrosive resistant properties but with similar viscosities having setting points within approximately 10° C. of each other and coefficients of expansion within approximately 1% of each other which coefficients of expansion are compatible with that of the material to which the sealing laminations are sealingly bonded.
Claim 3
Dependent Claim
15 words
The seal structure of claim 1, said first and second sealing lamination having adjoining surfaces.
Claim 4
Dependent Claim
67 words
The seal structure of claim 1, said assembly wall through which said terminal pin extends comprising an end closure having an aperture therein and an extended peripheral wall portion integral therewith to surround said aperture and extend at a preselected angle to said main body portion for a preselected distance, said first and second sealing laminations extending between said terminal pin and said extended peripheral wall portion.
Claim 5
Dependent Claim
26 words
The seal structure of claim 1, said terminal assembly including an end closure and an apertured eyelet through which said terminal pin passes and is sealed.
Claim 6
Dependent Claim
20 words
The seal structure of claim 1, said first and said second sealing laminations being glass of different corrosion resistant properties.
Claim 7
Dependent Claim
59 words
The structure of claim 1, said terminal assembly comprising a lithium battery assembly, said first and said second sealing laminations being glass of different corrosion resistant properties with the SiO 2 content in said first lamination being substantially less by weight than the SiO 2 content in said second lamination to increase the corrosion resistance to lithium battery electrolytes.
Claim 8
Dependent Claim
29 words
The structure of claim 1 and an intermediate lamination between said first and second sealing laminations having properties to inhibit corrosion migration between said first and second sealing laminations.
Claim 9
Dependent Claim
146 words
The structure of claim 1, said terminal assembly comprising a lithium battery assembly, said first lamination being comprised approximately by weight of 10 to 45% SiO 2 , 10 to 25% B 2 O 3 , 3 to 10% Al 2 O 3 , 2 to 10% La 2 O 3 , 10 to 30% light metal oxides of the second group in the periodic chemical table and 5 to 25% light metal oxides of the first group in the periodic chemical table; and, said second lamination being comprised approximately by weight of 50 to 65% SiO 2 , 4 to 12% B 2 O 3 , 1 to 5% Al 2 O 3 , 5 to 15% light metal oxides of the second group in the periodic chemical table and 5 to 25% light metal oxides of the first group of the periodic chemical table.
Claim 10
Dependent Claim
69 words
The structure of claim 8, said first lamination light metal oxides of the second group comprising MgO, CaO, SrO and BaO and of the first group comprising LiO 2 , Na 2 O and K 2 O; and, said second lamination light metal oxides of the second group comprising CaO, SrO, and BaO and of the first group comprising LiO 2 , Na 2 O and K 2 O.
Claim 11
Dependent Claim
361 words
An improved lithium battery assembly comprising: a battery housing having lithium electrolytes disposed therein; an end closure cover for said battery housing, said end closure having an aperture disposed therein; an annular metallic eyelet fuse welded in said end closure aperture; a metallic terminal pin extending through said eyelet; and, a seal structure extending continuously between the outer peripheral surface of said pin and the inner wall of said annular metallic eyelet including a first flat glass sealing lamination having spaced inner and outer planar surfaces extending continuously between the outer peripheral surface of said pin and said wall of said annular eyelet with said inner surface adjacent said lithium electrolytes in said battery house, said first glass lamination being comprised approximately by weight of 10 to 45% SiO 2 , 10 to 25% B 2 O 3 , 3 to 20% Al 2 O 3 , 2 to 10% LaO 3 , 10 to 30% light metal oxides including MgO, CaO, SrO and BaO and 5 to 25% light metal oxides including LiO 2 , Na 2 O and K 2 O; and, a second flat glass sealing lamination having spaced inner and outer planar surfaces extending continuously between the outer peripheral surface of said pin and said inner wall of said annular eyelet with said inner surface abutting said outer surface of said first lamination and said outer surface exposed to ambient, said second glass lamination being comprised approximately by weight of 50 to 65% SiO 2 , 4 to 12% B 2 O 3 , 1 to 5% Al 2 O 3 , 5 to 15% light metal oxides including CaO, SrO and BaO and 5 to 25% light metal oxides of LiO 2 , Na 2 O and K 2 O; said first and said second glass sealing laminations abuttingly facing each other to be coextensive along the entirety of the abutting faces and having similar viscosities having setting points within approximately 10° C. of each other and coefficients of expansion within approximately 1% of each other, which coefficients of expansion are compatible with that of the metallic material to which the glass laminations are sealingly bonded.
Claim 12
Dependent Claim
361 words
An improved lithium battery assembly comprising: a battery housing having lithium electrolytes disposed therein; an end closure cover for said battery housing, said end closure having an aperture disposed therein; an annular metallic eyelet fuse welded in said end closure aperture; a metallic terminal pin extending through said eyelet; and, a seal structure extending continuously between the outer peripheral surface of said pin and the inner wall of said annular metallic eyelet including a first flat glass sealing lamination having spaced inner and outer planar surfaces extending continuously between the outer peripheral surface of said pin and said wall of said annular eyelet with said inner surface adjacent said lithium electrolytes in said battery house, said first glass lamination being comprised approximately by weight of 10 to 45% SiO 2 , 10 to 25% B 2 O 3 , 3 to 20% Al 2 O 3 , 2 to 10% LaO 3 , 10 to 30% light metal oxides including MgO, CaO, SrO and BaO and 5 to 25% light metal oxides including LiO 2 , Na 2 O and K 2 O; and, a second flat glass sealing lamination having spaced inner and outer planar surfaces extending continuously between the outer peripheral surface of said pin and said inner wall of said annular eyelet with said inner surface abutting said outer surface of said first lamination and said outer surface exposed to ambient, said second glass lamination being comprised approximately by weight of 50 to 65% SiO 2 , 4 to 12% B 2 O 3 , 1 to 5% Al 2 O 3 , 5 to 15% light metal oxides including CaO, SrO and BaO and 5 to 25% light metal oxides of LiO 2 , Na 2 O and K 2 O; said first and said second glass sealing laminations abuttingly facing each other to be coextensive along the entirety of the abutting faces and having similar viscosities having setting points within approximately 10° C. of each other and coefficients of expansion within approximately 1% of each other, which coefficients of expansion are compatible with that of the metallic material to which the glass laminations are sealingly bonded.
References Cited (Backward Citations)
US3416964A
Cited
GB1264697A
Cited
US3876437A
Cited
FR2334640A1
Cited
GB2014354A
Cited
US4315974A
Cited
US4202700A
Cited
US4233372A
Cited
US4556613A
Cited
US4279975A
Cited
US4308323A
Cited
US4362792A
Cited
EP0067278A1
Cited
US4514590A
Cited
JPS59207577A
Cited
JPH0686755A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1992-05-22 | 1992-11-21 | 1993-05-23 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1996-05-22 | 1996-11-21 | 1997-05-23 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2000-05-22 | 2000-11-21 | 2001-05-23 | $7700.00 | Window Closed / Lapsed |