US4833049A Expired / Lapsed US ⏱️ 0.0 years remaining

Terminal assembly having two sealing layers

Assignee: Emerson Electric Co
•
Filing: 1988-04-18
•
Granted: 1989-05-23
•
Expires: 2008-04-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A terminal pin seal for an hermetic terminal assembly including at least two laminations one of which has the inner surface adjacent the assembly structure with electrochemical properties resistant to attack from chemical ingredients within the assembly and another of which laminations has the outer surface adjacent to ambient with electrochemical properties different from that lamination facing the assembly housing to produce a greater resistance to chemical attack from ambient.

Inventors

  • 👤 Richard L. Teaford
  • 👤 Glenn A. Honkomp
  • 👤 Donald H. Hall

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 15:36
CPC Classifications
H; H01; H01B; H01B17/00; H01B17/26; H01B17/30; H01B17/303; H01B17/305; H01M; H01M50/00; H01M50/10; H01M50/183; H01M50/186; H01M50/188; H01M50/19; H01M50/191; H10; H10W; H10W95/00; Y; Y02; Y02E; Y02E60/00; Y02E60/10

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 240 words
In an hermetic terminal assembly having a terminal pin extending from within the assembly through an apertured assembly wall to ambient, said assembly housing having a corrosive environment, an improved aperture seal structure between said pin and assembly wall comprising: a first substantially flat aperture sealing lamination having spaced inner and outer planar surfaces extending continuously between the outer peripheral surface of said terminal pin and the periphery of said assembly wall aperture with said inner surface of said first lamination being adjacent and exposed to said corrosive environment of said assembly structure, said first sealing lamination having corrosive resistant properties to produce a preselected resistance to attack from ingredients producing said corrosive environment within the assembly; and, a second flat aperture sealing lamination having spaced inner and outer planar surface extending continuously between the outer peripheral surface of said terminal pin and the periphery of said assembly wall aperture with said outer surface adjacent ambient, said second aperture sealing lamination having corrosion resistant properties different from those of said first aperture sealing lamination to produce a preselected resistance to attack from ambient conditions; said first and said second sealing laminations being of different corrosive resistant properties but with similar viscosities having setting points within approximately 10° C. of each other and coefficients of expansion within approximately 1% of each other which coefficients of expansion are compatible with that of the material to which the sealing laminations are sealingly bonded.
Claim 2
Dependent Claim 240 words
In an hermetic terminal assembly having a terminal pin extending from within the assembly through an apertured assembly wall to ambient, said assembly housing having a corrosive environment, an improved aperture seal structure between said pin and assembly wall comprising: a first substantially flat aperture sealing lamination having spaced inner and outer planar surfaces extending continuously between the outer peripheral surface of said terminal pin and the periphery of said assembly wall aperture with said inner surface of said first lamination being adjacent and exposed to said corrosive environment of said assembly structure, said first sealing lamination having corrosive resistant properties to produce a preselected resistance to attack from ingredients producing said corrosive environment within the assembly; and, a second flat aperture sealing lamination having spaced inner and outer planar surface extending continuously between the outer peripheral surface of said terminal pin and the periphery of said assembly wall aperture with said outer surface adjacent ambient, said second aperture sealing lamination having corrosion resistant properties different from those of said first aperture sealing lamination to produce a preselected resistance to attack from ambient conditions; said first and said second sealing laminations being of different corrosive resistant properties but with similar viscosities having setting points within approximately 10° C. of each other and coefficients of expansion within approximately 1% of each other which coefficients of expansion are compatible with that of the material to which the sealing laminations are sealingly bonded.
Claim 3
Dependent Claim 15 words
The seal structure of claim 1, said first and second sealing lamination having adjoining surfaces.
Claim 4
Dependent Claim 67 words
The seal structure of claim 1, said assembly wall through which said terminal pin extends comprising an end closure having an aperture therein and an extended peripheral wall portion integral therewith to surround said aperture and extend at a preselected angle to said main body portion for a preselected distance, said first and second sealing laminations extending between said terminal pin and said extended peripheral wall portion.
Claim 5
Dependent Claim 26 words
The seal structure of claim 1, said terminal assembly including an end closure and an apertured eyelet through which said terminal pin passes and is sealed.
Claim 6
Dependent Claim 20 words
The seal structure of claim 1, said first and said second sealing laminations being glass of different corrosion resistant properties.
Claim 7
Dependent Claim 59 words
The structure of claim 1, said terminal assembly comprising a lithium battery assembly, said first and said second sealing laminations being glass of different corrosion resistant properties with the SiO 2 content in said first lamination being substantially less by weight than the SiO 2 content in said second lamination to increase the corrosion resistance to lithium battery electrolytes.
Claim 8
Dependent Claim 29 words
The structure of claim 1 and an intermediate lamination between said first and second sealing laminations having properties to inhibit corrosion migration between said first and second sealing laminations.
Claim 9
Dependent Claim 146 words
The structure of claim 1, said terminal assembly comprising a lithium battery assembly, said first lamination being comprised approximately by weight of 10 to 45% SiO 2 , 10 to 25% B 2 O 3 , 3 to 10% Al 2 O 3 , 2 to 10% La 2 O 3 , 10 to 30% light metal oxides of the second group in the periodic chemical table and 5 to 25% light metal oxides of the first group in the periodic chemical table; and, said second lamination being comprised approximately by weight of 50 to 65% SiO 2 , 4 to 12% B 2 O 3 , 1 to 5% Al 2 O 3 , 5 to 15% light metal oxides of the second group in the periodic chemical table and 5 to 25% light metal oxides of the first group of the periodic chemical table.
Claim 10
Dependent Claim 69 words
The structure of claim 8, said first lamination light metal oxides of the second group comprising MgO, CaO, SrO and BaO and of the first group comprising LiO 2 , Na 2 O and K 2 O; and, said second lamination light metal oxides of the second group comprising CaO, SrO, and BaO and of the first group comprising LiO 2 , Na 2 O and K 2 O.
Claim 11
Dependent Claim 361 words
An improved lithium battery assembly comprising: a battery housing having lithium electrolytes disposed therein; an end closure cover for said battery housing, said end closure having an aperture disposed therein; an annular metallic eyelet fuse welded in said end closure aperture; a metallic terminal pin extending through said eyelet; and, a seal structure extending continuously between the outer peripheral surface of said pin and the inner wall of said annular metallic eyelet including a first flat glass sealing lamination having spaced inner and outer planar surfaces extending continuously between the outer peripheral surface of said pin and said wall of said annular eyelet with said inner surface adjacent said lithium electrolytes in said battery house, said first glass lamination being comprised approximately by weight of 10 to 45% SiO 2 , 10 to 25% B 2 O 3 , 3 to 20% Al 2 O 3 , 2 to 10% LaO 3 , 10 to 30% light metal oxides including MgO, CaO, SrO and BaO and 5 to 25% light metal oxides including LiO 2 , Na 2 O and K 2 O; and, a second flat glass sealing lamination having spaced inner and outer planar surfaces extending continuously between the outer peripheral surface of said pin and said inner wall of said annular eyelet with said inner surface abutting said outer surface of said first lamination and said outer surface exposed to ambient, said second glass lamination being comprised approximately by weight of 50 to 65% SiO 2 , 4 to 12% B 2 O 3 , 1 to 5% Al 2 O 3 , 5 to 15% light metal oxides including CaO, SrO and BaO and 5 to 25% light metal oxides of LiO 2 , Na 2 O and K 2 O; said first and said second glass sealing laminations abuttingly facing each other to be coextensive along the entirety of the abutting faces and having similar viscosities having setting points within approximately 10° C. of each other and coefficients of expansion within approximately 1% of each other, which coefficients of expansion are compatible with that of the metallic material to which the glass laminations are sealingly bonded.
Claim 12
Dependent Claim 361 words
An improved lithium battery assembly comprising: a battery housing having lithium electrolytes disposed therein; an end closure cover for said battery housing, said end closure having an aperture disposed therein; an annular metallic eyelet fuse welded in said end closure aperture; a metallic terminal pin extending through said eyelet; and, a seal structure extending continuously between the outer peripheral surface of said pin and the inner wall of said annular metallic eyelet including a first flat glass sealing lamination having spaced inner and outer planar surfaces extending continuously between the outer peripheral surface of said pin and said wall of said annular eyelet with said inner surface adjacent said lithium electrolytes in said battery house, said first glass lamination being comprised approximately by weight of 10 to 45% SiO 2 , 10 to 25% B 2 O 3 , 3 to 20% Al 2 O 3 , 2 to 10% LaO 3 , 10 to 30% light metal oxides including MgO, CaO, SrO and BaO and 5 to 25% light metal oxides including LiO 2 , Na 2 O and K 2 O; and, a second flat glass sealing lamination having spaced inner and outer planar surfaces extending continuously between the outer peripheral surface of said pin and said inner wall of said annular eyelet with said inner surface abutting said outer surface of said first lamination and said outer surface exposed to ambient, said second glass lamination being comprised approximately by weight of 50 to 65% SiO 2 , 4 to 12% B 2 O 3 , 1 to 5% Al 2 O 3 , 5 to 15% light metal oxides including CaO, SrO and BaO and 5 to 25% light metal oxides of LiO 2 , Na 2 O and K 2 O; said first and said second glass sealing laminations abuttingly facing each other to be coextensive along the entirety of the abutting faces and having similar viscosities having setting points within approximately 10° C. of each other and coefficients of expansion within approximately 1% of each other, which coefficients of expansion are compatible with that of the metallic material to which the glass laminations are sealingly bonded.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-05-22 1992-11-21 1993-05-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-05-22 1996-11-21 1997-05-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-05-22 2000-11-21 2001-05-23 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag