Claims Analysis
Total Claims: 16
Claim 1
Independent Claim
135 words
A multilayer shrink film comprising: (a) a core layer comprising a linear low density polyethylene or ethylene propylene copolymer; (b) two outer layers comprising a polymeric material selected from the group consisting of linear low density polyethylene and ethylene propylene copolymer; and (c) two intermediate layers comprising a polymeric material or blend of materials having a melting point of less than about 100° C.; wherein said film has an average machine direction shrink tension at 205° F. of no more than about 250 pounds per square inch, and an average transverse direction shrink tension at 205° F. of no more than about 300 pounds per square inch, said shrink tension values as measured by ASTM D 2838; and wherein the intermediate layers comprise about 60% to 90% of the total thickness of the multilayer film.
Claim 2
Dependent Claim
135 words
A multilayer shrink film comprising: (a) a core layer comprising a linear low density polyethylene or ethylene propylene copolymer; (b) two outer layers comprising a polymeric material selected from the group consisting of linear low density polyethylene and ethylene propylene copolymer; and (c) two intermediate layers comprising a polymeric material or blend of materials having a melting point of less than about 100° C.; wherein said film has an average machine direction shrink tension at 205° F. of no more than about 250 pounds per square inch, and an average transverse direction shrink tension at 205° F. of no more than about 300 pounds per square inch, said shrink tension values as measured by ASTM D 2838; and wherein the intermediate layers comprise about 60% to 90% of the total thickness of the multilayer film.
Claim 3
Dependent Claim
26 words
A multilayer shrink film according to claim 1 wherein the two outer layers are each derived from a blend of two linear low density polyethylene resins.
Claim 4
Dependent Claim
60 words
A multilayer shrink film according to claim 1 wherein the two intermediate layers comprise a polymeric material selected from the group consisting of: (a) ethylene vinyl acetate copolymer; (b) a blend of ethylene vinyl acetate copolymer and very low density polyethylene; (c) ethylene butyl acrylate copolymer; and (d) a blend of ethylene vinyl acetate copolymer and ethylene butyl acrylate copolymer.
Claim 5
Dependent Claim
31 words
A multilayer shrink film according to claim 3 wherein the two intermediate layers comprise an ethylene vinyl acetate copolymer having between about 8% and about 30% by weight of vinyl acetate.
Claim 6
Dependent Claim
14 words
A multilayer shrink film according to claim 1 wherein the film layers are cross-linked.
Claim 7
Dependent Claim
22 words
A multilayer shrink film according to claim 1 wherein the shrink tension of the film is substantially controlled by the intermediate layers.
Claim 8
Dependent Claim
124 words
A multilayer shrink film comprising: (a) a core layer comprising a linear low density polyethylene or ethylene propylene copolymer; (b) two outer layers comprising a polymeric material selected from the group consisting of linear low density polyethylene and ethylene propylene copolymer; (c) two intermediate layers comprising a polymeric material or blend of materials having a melting point of less than about 100° C.; wherein said film has an average machine direction free shrink at 205° F. of at least about 30% and an average transverse direction free shrink at 205° F. of at least about 30%, said free shrink values as measured by ASTM D 2732; and wherein the intermediate layers comprise about 60% to 90% of the total thickness of the multilayer film.
Claim 9
Dependent Claim
124 words
A multilayer shrink film comprising: (a) a core layer comprising a linear low density polyethylene or ethylene propylene copolymer; (b) two outer layers comprising a polymeric material selected from the group consisting of linear low density polyethylene and ethylene propylene copolymer; (c) two intermediate layers comprising a polymeric material or blend of materials having a melting point of less than about 100° C.; wherein said film has an average machine direction free shrink at 205° F. of at least about 30% and an average transverse direction free shrink at 205° F. of at least about 30%, said free shrink values as measured by ASTM D 2732; and wherein the intermediate layers comprise about 60% to 90% of the total thickness of the multilayer film.
Claim 10
Dependent Claim
24 words
A multilayer shrink film according to claim 7 wherein the two outer layers each comprise a blend of two linear low density poly-ethylene resins.
Claim 11
Dependent Claim
60 words
A multilayer shrink film according to claim 7 wherein the two intermediate layers comprise a polymeric material selected from the group consisting of: (a) ethylene vinyl acetate copolymer; (b) a blend of ethylene vinyl acetate copolymer and very low density polyethylene; (c) ethylene butyl acrylate copolymer; and (d) a blend of ethylene vinyl acetate copolymer and ethylene butyl acrylate copolymer.
Claim 12
Dependent Claim
31 words
A multilayer shrink film according to claim 9 wherein the two intermediate layers comprise an ethylene vinyl acetate copolymer having between about 8% and about 30% by weight of vinyl acetate.
Claim 13
Dependent Claim
14 words
A multilayer shrink film according to claim 7 wherein the film layers are cross-linked.
Claim 14
Dependent Claim
22 words
A multilayer shrink film according to claim 7 wherein the free shrink of the film is substantially controlled by the intermediate layers.
Claim 15
Dependent Claim
26 words
A multilayer shrink film according to claim 1 wherein the intermediate layers include between about 1% and 2% mineral oil by weight of the intermediate layer.
Claim 16
Dependent Claim
26 words
A multilayer shrink film according to claim 7 wherein the intermediate layers include between about 1% and 2% mineral oil by weight of the intermediate layer.