Abstract

Abstract A method for bonding a restorative composite resin to dentin which comprises: treating the surface of dentin with a dentin-treating liquid for, 1 to 90 seconds obtained by adding glutaraldehyde and ferric chloride to an aqueous solution of ethylenediaminetetraacetic acid regulated to a hydrogen ion concentration (pH) of 7.4; removing the treating liquid by water-rinsing to dry the thus treated surface of dentin; applying a primer comprising an ethylene related unsaturated monomer, a (meth)acrylic ester polymer and tri-n-butyl borane on the dried surface of dentin; and filling the restorative composite resin onto the applied surface of dentin.

Inventors

  • 👤 Reiichi Okuda
  • 👤 Masashi Komatsu
  • 👤 Shin Asanuma
  • 👤 Noriko Hiratsuka

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 21:13
CPC Classifications
A; A61; A61C; A61C5/00; A61K; A61K6/00; A61K6/40

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 94 words
A method for bonding a composite resin to dentin, which comprises: treating the surface of dentin with a dentin-treating liquid obtained by adding glutaraldehyde and ferric chloride to an aqueous solution of ethylenediaminetetraacetic acid (abbreviated to EDTA) regulated to a hydrogen ion concentration (pH) of 7.4, removing said treating liquid by water-rinsing to dry the thus treated surface of dentin, applying a primer comprising an ethylene related unsaturated monomer, a (meth)acrylic ester polymer and tri-n-butyl borane on the dried surface of dentin, and filling a restorative composite resin onto the applied surface of dentin.
Claim 2
Independent Claim 94 words
A method for bonding a composite resin to dentin, which comprises: treating the surface of dentin with a dentin-treating liquid obtained by adding glutaraldehyde and ferric chloride to an aqueous solution of ethylenediaminetetraacetic acid (abbreviated to EDTA) regulated to a hydrogen ion concentration (pH) of 7.4, removing said treating liquid by water-rinsing to dry the thus treated surface of dentin, applying a primer comprising an ethylene related unsaturated monomer, a (meth)acrylic ester polymer and tri-n-butyl borane on the dried surface of dentin, and filling a restorative composite resin onto the applied surface of dentin.
Claim 3
Dependent Claim 33 words
A bonding method as defined in claim 1, wherein the concentration of glutaraldehyde in said treating liquid is 0.01 to 20 parts by weight with respect to 100 parts by weight of water.
Claim 4
Dependent Claim 36 words
A bonding method as defined in claim 1 ro 2, wherein the concentration of ferric chloride in said treating liquid is 0.01 to 5.00 parts by weight with respect to 100 parts by weight of water.
Claim 5
Dependent Claim 33 words
A bonding method as defined in claim 1 or 2, wherein the concentration of EDTA in said treating liquid is 0.1 to 1.0 mol/l with respect to 100 parts by weight of water.
Claim 6
Dependent Claim 26 words
A bonding method as defined in claim 1 or 2, wherein said ethylene related unsaturated monomer of said primer is one or more (meth)acrylic ester monomers.
Claim 7
Dependent Claim 23 words
A bonding method as defined in claim 1 or 2, wherein said (meth)acrylic ester polymer of said primer is a methyl methacrylate polymer.
Claim 8
Dependent Claim 27 words
A bonding method as defined in claim 1 or 2, wherein said (meth)acrylic ester polymer of said primer is a copolymer of methyl methacrylate and ethyl methacrylate.
Claim 9
Dependent Claim 31 words
A bonding method as defined in claim 1 or 2, wherein said (meth)acrylic ester polymer of said primer is a methyl methacrylate polymer and copolymer of methyl methacrylate and ethyl methacrylate.

References Cited (Backward Citations)

US4259075A Cited
US4612384A Cited
US4654007A Cited
US4655712A Cited
US4748198A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-05-15 1992-11-14 1993-05-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-05-15 1996-11-14 1997-05-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-05-15 2000-11-14 2001-05-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag