Ski wax composition and process of application

Assignee: Edge Line Products Inc
•
Filing: 1987-12-23
•
Granted: 1989-05-09
•
Expires: 2007-12-23
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A wax composition for waxing skis comprising a wax matrix having incorporated therein a silicone polymer of relatively low volatility.

Inventors

  • 👤 Ira E. Rosenberg

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 13:08
CPC Classifications
C; C09; C09G; C09G3/00

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 160 words
A process for waxing a ski to improve its glide characteristics comprising the steps of: applying to a bottom surface of said ski a composition formed by the following steps: (a) melting a wax component until the wax component is in liquid form; (b) removing heat from the melted wax component; (c) adding to the melted wax component a solvent and a polymer of a siloxane selected from the group consisting of dimethyl siloxane and cyclo siloxane, said polymer having a molecular weight between about 100 and about 2,000 and a vapor pressure at 20 C between about 1.5 and about 100 mm of Hg; (d) stirring the mixture of the wax component, the solvent and the siloxane until the mixture is uniform to form said composition; (e) pouring said composition into a stick mold; (f) applying said molded stick to the bottom surface of said ski; and allowing said composition to set on the bottom surface of said ski.
Claim 2
Dependent Claim 160 words
A process for waxing a ski to improve its glide characteristics comprising the steps of: applying to a bottom surface of said ski a composition formed by the following steps: (a) melting a wax component until the wax component is in liquid form; (b) removing heat from the melted wax component; (c) adding to the melted wax component a solvent and a polymer of a siloxane selected from the group consisting of dimethyl siloxane and cyclo siloxane, said polymer having a molecular weight between about 100 and about 2,000 and a vapor pressure at 20 C between about 1.5 and about 100 mm of Hg; (d) stirring the mixture of the wax component, the solvent and the siloxane until the mixture is uniform to form said composition; (e) pouring said composition into a stick mold; (f) applying said molded stick to the bottom surface of said ski; and allowing said composition to set on the bottom surface of said ski.
Claim 3
Dependent Claim 196 words
A process for waxing a ski to improve its glide characteristics comprising the steps of: applying to a bottom surface of said ski a composition formed by the following steps: (a) melting a wax component in an amount between about 40% and about 80% by weight of the total composition until the wax component is in liquid form; (b) removing heat from the melted wax component; (c) adding to the melted wax component a solvent in an amount between about 5% and about 30% by weight of the total composition and a polymer of a siloxane selected from the group consisting of dimethyl siloxane and cyclo siloxane, said polymer having a molecular weight between about 100 and about 2,000 and a vapor pressure at 20 C between about 1.5 and about 100 mm of Hg, said polymer comprising an amount between about 5% and about 30% by weight of the total composition; (d) stirring the mixture of the wax component, the solvent and the siloxane until the mixture is uniform to form said composition; and (e) pouring said composition into a stick mold; and allowing said composition to set on the bottom surface of said ski.
Claim 4
Dependent Claim 196 words
A process for waxing a ski to improve its glide characteristics comprising the steps of: applying to a bottom surface of said ski a composition formed by the following steps: (a) melting a wax component in an amount between about 40% and about 80% by weight of the total composition until the wax component is in liquid form; (b) removing heat from the melted wax component; (c) adding to the melted wax component a solvent in an amount between about 5% and about 30% by weight of the total composition and a polymer of a siloxane selected from the group consisting of dimethyl siloxane and cyclo siloxane, said polymer having a molecular weight between about 100 and about 2,000 and a vapor pressure at 20 C between about 1.5 and about 100 mm of Hg, said polymer comprising an amount between about 5% and about 30% by weight of the total composition; (d) stirring the mixture of the wax component, the solvent and the siloxane until the mixture is uniform to form said composition; and (e) pouring said composition into a stick mold; and allowing said composition to set on the bottom surface of said ski.
Claim 5
Dependent Claim 17 words
The process of claim 2, wherein said composition is a wax composition which is in stick form.

References Cited (Backward Citations)

US4126481A Cited
US4144325A Cited
US4202879A Cited
US4379136A Cited
US4321295A Cited
US4343863A Cited
US4404035A Cited
US4729794A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-05-08 1992-11-07 1993-05-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-05-08 1996-11-07 1997-05-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-05-08 2000-11-07 2001-05-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag