US4824871A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Electrically conductive polymer composite and method of making same
Assignee: Inoac Corp
•
Filing: 1988-02-29
•
Granted: 1989-04-25
•
Expires: 2008-02-29
Abstract
Abstract An electrically conductive polymer composite comprising a porous body of polymer A containing interconnected cavities, and polymer B containing an electrically conductive filler and filling the cavities of the porous body. This polymer composite can be made by filling the cavities of the porous body with a liquid monomer, monomer mixture or prepolymer and then polymerizing or cross-linking it to yield polymer B in solid form. The polymer composite has excellent mechanical properties and high electrical conductivity and, therefore, is suitable for use as an electrically conductive material, electromagnetic wave shielding material, heating element and antistatic material.
Inventors
- 👤 Toshihiko Shinomura
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-28 15:33
CPC Classifications
C; C08; C08J; C08J9/00; C08J9/36; C08J9/40; C08J9/405; H; H01; H01B; H01B1/00; H01B1/20; H01B1/22; H01B1/24; Y; Y10; Y10S; Y10S521/00; Y10S521/918
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
98 words
A method of making an electrically conductive polymer composite which comprises the steps of (a) providing a porous body of polymer A containing interconnected cavities ranging in diameter from 0.05 μm to 10 mm and having a porosity of 5 to 95% by volume, (b) filing the cavities of said porous body with a liquid monomer, monomer mixture or prepolymer suitable for the formation of polymer B and containing 10 to 95% by weight of an electrically conductive filler, and (c) polymerizing or cross-linking said liquid monomer, monomer mixture or prepolymer to yield polymer B in solid form.
Claim 2
Independent Claim
98 words
A method of making an electrically conductive polymer composite which comprises the steps of (a) providing a porous body of polymer A containing interconnected cavities ranging in diameter from 0.05 μm to 10 mm and having a porosity of 5 to 95% by volume, (b) filing the cavities of said porous body with a liquid monomer, monomer mixture or prepolymer suitable for the formation of polymer B and containing 10 to 95% by weight of an electrically conductive filler, and (c) polymerizing or cross-linking said liquid monomer, monomer mixture or prepolymer to yield polymer B in solid form.
References Cited (Backward Citations)
US4171410A
Cited
US4719039A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1992-04-24 | 1992-10-24 | 1993-04-25 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1996-04-24 | 1996-10-24 | 1997-04-25 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2000-04-24 | 2000-10-24 | 2001-04-25 | $7700.00 | Window Closed / Lapsed |