← Back to Patent Explorer
US4820775A Expired / Lapsed US ⏱️ 0.0 years remaining

Alpha-olefin block copolymer particles and process for the production thereof

Assignee: Sumitomo Chemical Co Ltd
•
Filing: 1986-05-23
•
Granted: 1989-04-11
•
Expires: 2006-05-23
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process for the production of alpha -olefin block copolymer particles having excellent impact resistance at low temperature and excellent molding and processing characteristics, is disclosed. The process includes a two step gas phase polymerization procedure under specific conditions in the presence of a specific catalyst system.

Inventors

  • 👤 Akinobu Shiga
  • 👤 Masahiro Kakugo
  • 👤 Hajime Sadatoshi
  • 👤 Hiroyuki Kora
  • 👤 Toshio Sasaki
  • 👤 Junpei Kojima
  • 👤 Kazuki Wakamatsu
  • 👤 Syozo Kawamata

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 21:31
CPC Classifications
C; C08; C08F; C08F297/00; C08F297/06; C08F297/08; C08F297/083

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 236 words
A process for the production of α-olefin block copolymer particles which comprises the steps of (1) homopolymerizing propylene or copolymerizing propylene with a comonomer of ethylene or an α-olefin having 4 to 6 carbon atoms so that the comonomer content of the copolymerization product produced is not more than 6% by mole, said polymerization being carried out utilizing propylene in a liquid or gaseous phase, (2) in the presence of the product produced by step (1), homopolymerizing ethylene or copolymerizing ethylene with propylene, with an α-olefin having 4 to 6 carbon atoms or with a mixture thereof so that the ethylene content in the copolymerization product produced is not less than 10% by mole, said copolymerizing being carried out utilizing propylene in a liquid or a gaseous phase when present, the polymerization being carried out in the degree of 10 to 70% by weight based on the total polymerization amount, said polymerizaton in said first and second steps being carried out in the presence of a catalyst system comprising (A) a solid catalyst component containing at least titanium, chlorine and an electron-donating compound and having a pore volume of not less than 0.08 cc/g in the range of a pore radius of 200 to 15,000 Å, a mean particle size of 5 to 100 μm, and a geometric standard deviation (σg) of the particle distribution of not more than 2, and (B) an organic aluminum compound.
Claim 2
Dependent Claim 236 words
A process for the production of α-olefin block copolymer particles which comprises the steps of (1) homopolymerizing propylene or copolymerizing propylene with a comonomer of ethylene or an α-olefin having 4 to 6 carbon atoms so that the comonomer content of the copolymerization product produced is not more than 6% by mole, said polymerization being carried out utilizing propylene in a liquid or gaseous phase, (2) in the presence of the product produced by step (1), homopolymerizing ethylene or copolymerizing ethylene with propylene, with an α-olefin having 4 to 6 carbon atoms or with a mixture thereof so that the ethylene content in the copolymerization product produced is not less than 10% by mole, said copolymerizing being carried out utilizing propylene in a liquid or a gaseous phase when present, the polymerization being carried out in the degree of 10 to 70% by weight based on the total polymerization amount, said polymerizaton in said first and second steps being carried out in the presence of a catalyst system comprising (A) a solid catalyst component containing at least titanium, chlorine and an electron-donating compound and having a pore volume of not less than 0.08 cc/g in the range of a pore radius of 200 to 15,000 Å, a mean particle size of 5 to 100 μm, and a geometric standard deviation (σg) of the particle distribution of not more than 2, and (B) an organic aluminum compound.
Claim 3
Dependent Claim 87 words
The process for the production of α-olefin block copolymer particles according to claim 1, wherein the catalyst system is a system that when said propylene is polymerized by use of said liquified propylene in the presence of said catalyst system at 65° C. for 4 hours, polypropylene is produced in an amount of not less than 6,000 g per 1 g of the solid catalyst component, and said polypropylene contains not more than 5% by weight of a component which is soluble in xylene at 20° C.
Claim 4
Dependent Claim 86 words
The process for the production of α-olefin block copolymer particles according to claim 1, wherein the catalyst system is a system that when said propylene is polymerized by using said liquefied propylene in the presence of said catalyst system at 65° C. for 4 hours, polypropylene is produced in an amount of not less than 6,000 g per 1 g of the solid catalyst component, and said polypropylene contains not more than 4% by weight of a component which is soluble in xylene at 20° C.
Claim 5
Dependent Claim 195 words
The process for the production of α-olefin block copolymer particles according to claim 1, wherein the catalyst system comprises (A) a solid catalyst component consisting essentially of a titanium compound carried on a magnesium compound and 1 to 20% by weight of an electron donating compound selected from ether compounds and ester compounds, which has a pore volume of not less than 0.1 cc/g in the range of a pore radius of 200 to 15,000 Å, a mean particle size of 10 to 75 μm, and a geometric standard deviation (σg) of the particle distribution of not more than 1.8. (B) an organic aluminum compound of the formula: R e AlX 3-e wherein R is a hydrocarbon group having 1 to 18 carbon atoms, X is a halogen atom, and e is a number in the formula 2.5≦e≦3 in an amount of 40 to 1,500 mole per 1 mole of titanium in the solid catalyst component (A), and (C) an electron donor selected from the group consisting of esters, amines, and organic silicon compounds having Si--O--C bond in an amount of not more than 1 mole per 1 mole of the organic aluminum compound (B).
Claim 6
Dependent Claim 165 words
The process for the production of α-olefin block copolymer particles according to claim 1, wherein the catalyst system comprises (A) a solid catalyst component comprising a titanium compound of the formula: Ti(OR 1 ) b Cl 3-b wherein R 1 is a hydrocarbon group having 1 to 20 carbon atoms and b is a number in the formula 0.001<b<0.15, and 1 to 15% by weight of an ether compound, which has a pore volume of not less than 0.1 cc/g in the range of a pore radius of 200 to 15,000 Å, a mean particle size of 10 to 75 μm, and a geometric standard deviation (σg) of the particle distribution of not more than 1.8, and (B) an organic aluminum compound of the formula: R 2 AlX wherein R is a hydrocarbon group having 1 to 18 carbon atoms and X is a halogen atom in an amount of 1 to 30 mole per 1 mole of titanium in the solid catalyst component (A).
Claim 7
Dependent Claim 138 words
The process for the production of α-olefin block copolymer particles according to claim 1, wherein the catalyst system comprises (A) a solid catalyst component comprising a titanium trichloride having a layer structure and 1 to 15% by weight of an ether compound, which has a pore volume of not less than 0.1 cc/g in the range of a pore radius of 200 to 15,000 Å, a mean particle size of 10 to 75 μm, and a geometric standard deviation (σg) of the particle distribution of not more than 1.8, and (B) an organic aluminum compound of the formula: R 2 AlX wherein R is a hydrocarbon group having 1 to 18 carbon atoms and X is a halogen atom in an amount of 1 to 30 mole per 1 mole of titanium in the solid catalyst component (A).
Claim 8
Dependent Claim 40 words
The process for the production of α-olefin block copolymer particles according to claim 2, wherein said polymer produced in the first step contains not more than 15% by weight of a component which is soluble in xylene at 20° C.
Claim 9
Dependent Claim 40 words
The process for the production of α-olefin block copolymer particles according to claim 3, wherein said polymer produced in the first step contains not more than 5% by weight of a component which is soluble in xylene at 20° C.

References Cited (Backward Citations)

US4210738A Cited
US4259461A Cited
US4298713A Cited
US4485035A Cited
US4339557A Cited
US4412049A Cited
US4483966A Cited
US4455405A Cited
US4550144A Cited
US4533706A Cited
US4554264A Cited
US4711940A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-04-10 1992-10-10 1993-04-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-04-10 1996-10-10 1997-04-11 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-04-10 2000-10-10 2001-04-11 $7700.00 Window Closed / Lapsed