Abstract

Abstract A multi-layered back reflecting mirror having a dielectric multi-layered coating on oen side of a glass or plastic transparent substrate which is further overlaid with a light-absorbing layer. The dielectric multi-layered coating is composed of four to eight dielectric layers laminated one on top of another having alternately differing refractive indices. At least one of these dielectric layers has an optical thickness of λ 0 /2 (λ 0 is the wavelength of light used as the reference measurement for design purposes) and each of the remaining dielectric layers has an optical thickness of λ 0 /4. The mirror has a relative reflection minimum for visible light in the range of 480 to 550 nonometers.

Inventors

  • 👤 Yuji Nakajima

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 15:18
CPC Classifications
G; G02; G02B; G02B5/00; G02B5/08; G02B5/0816; G02B5/0825; G02B5/0833; B; B60; B60R; B60R1/00; B60R1/02; B60R1/08; B60R1/083; C; C03; C03C; C03C17/00; C03C17/34; C03C17/3411; C03C17/3417

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 115 words
A multi-layered back reflecting mirror having a dielectric multi-layered coating on one side of a glass or plastic transparent substrate which is further overlaid with a light-absorbing layer, said dielectric multi-layered coating being composed of four to eight dielectric layers laminated one on top of another having alternately differing refractive indices, at least one of said dielectric layers having an optical thickness of λ 0 /2, wherein λ 0 is the wavelength of light used as the reference measurement for design purposes, each of the remaining dielectric layers has an optical thickness of λ 0 /4, and said mirror has a relative reflection minimum for visible light in a range of 480 to 550 nanometers.
Claim 2
Dependent Claim 115 words
A multi-layered back reflecting mirror having a dielectric multi-layered coating on one side of a glass or plastic transparent substrate which is further overlaid with a light-absorbing layer, said dielectric multi-layered coating being composed of four to eight dielectric layers laminated one on top of another having alternately differing refractive indices, at least one of said dielectric layers having an optical thickness of λ 0 /2, wherein λ 0 is the wavelength of light used as the reference measurement for design purposes, each of the remaining dielectric layers has an optical thickness of λ 0 /4, and said mirror has a relative reflection minimum for visible light in a range of 480 to 550 nanometers.
Claim 3
Dependent Claim 22 words
A multi-layered back reflecting mirror according to claim (1) wherein the dielectric multi-layered coating is composed of five or six dielectric layers.
Claim 4
Dependent Claim 201 words
A multi-layered back reflecting mirror according to claim (2) wherein the dielectric multi-layered coating is composed of dielectric layers which are formed on one side of the transparent substrate in the order, as seen from the substrate side, of an H layer, a 2L layer, an H layer, an L layer and an H layer, or in the order of an H layer, an L layer, an H layer, a 2L layer and an H layer, the H layer being a high-refractive index layer that is made of a material having a high refractive index of 1.9-2.4 and which has an optical thickness of λ 0 /4, the 2H layer being a high-refractive index layer that is made of a material having a high refractive index of 1.9-2.4 and which has an optical thickness of λ 0 /2, the L layer being a low-refractive index layer that is made of a material having a low refractive index of 1.3-1.8 and which has an optical thickness of λ 0 /4, and the 2L layer being a low-refractive index layer that is made of a material having a low refractive index of 1.3-1.8 and which has an optical thickness of λ 0 /2.
Claim 5
Dependent Claim 61 words
A multi-layered back reflecting mirror according to claim (3) where the 2L layer is a combination layer in which a low-refractive index layer (L 1 layer) that is made of a low-refractive index material and which has an optical thickness of λ 0 /4 is combined with another low-refractive index material and which has an optical thickness of λ 0 /4.
Claim 6
Dependent Claim 45 words
A multi-layered back reflecting mirror according to claim (2) wherein the dielectric multi-layered coating is composed of dielectric layers that are formed on one side of the transparent substrate in the order of the 2H layer, L layer, H layer, L layer and 2H layer.
Claim 7
Dependent Claim 77 words
A multi-layered back reflecting mirror according to claim (5) wherein one or both of the two 2H layers is a combination layer in which a high-refractive index layer (H 1 layer) that is made of a high-refractive index material and which has an optical thickness of λ 0 /4 is combined with another high-refractive index layer (H 2 layer) that is made of another high-refractive index material and which has an optical thickness of λ 0 /4.
Claim 8
Dependent Claim 62 words
A multi-layered back reflecting mirror according to claim (2) wherein the dielectric multi-layered coating is composed of dielectric layers that are formed on one side of the transparent substrate in the order of the 2H layer, L layer, H layer, L layer and H layer or in the order of the H layer, L layer, H layer, L layer and 2H layer.
Claim 9
Dependent Claim 72 words
A multi-layered back reflecting mirror according to claim (7) wherein the 2H layer is a combination layer in which a high-refractive index layer (H 1 layer) that is made of a high-refractive index material and which has an optical thickness of λ 0 /4 is combined with another high-refractive index layer (H 2 layer) that is made of another high-refractive index material and which has an optical thickness of λ 0 /4.

References Cited (Backward Citations)

US4352006A Cited
JPS57144504A Cited
US4673248A Cited
JPS59195205A Cited
US4634242A Cited
JPS6098405A Cited
JPS60212705A Cited
JPS60212704A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-02-21 1992-08-22 1993-02-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-02-21 1996-08-22 1997-02-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-02-21 2000-08-22 2001-02-21 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag