← Back to Patent Explorer
US4776223A Expired / Lapsed US ⏱️ 0.0 years remaining

Double bevel construction of a diamond anvil

Assignee: United States Department of Energy
•
Filing: 1987-02-06
•
Granted: 1988-10-11
•
Expires: 2007-02-06
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A double or multiple bevel culet geometry is used on a diamond anvil in a high pressure cell apparatus to provide increased sample pressure and stability for a given force applied to the diamond tables. Double or multiple bevel culet geometries can also be used for sapphire or other hard crystal anvils. Pressures up to and above 5 Megabars can be reached.

Inventors

  • 👤 William C. Moss

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 13:05
CPC Classifications
G; G01; G01N; G01N21/00; G01N21/01; G01N21/03; G01N21/0317

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 288 words
Improved diamond anvil apparatus, the apparatus comprising: a first diamond crystal, including a centrally positioned flat surface of radius substantially 15-45 μm, a first bevel region, of substantially annular shape, of facets with an associated first bevel angle, contiguous to and surrounding the perimeter of the flat surface, with outer annulus radius substantially 60-90 μm, and a second bevel region, of substantially annular shape, of facets with an associated second bevel angle, contiguous to and surrounding the outer perimeter of the first bevel region, with outer annulus radius substantially 120 μm or greater; a second diamond crystal, including a centrally positioned flat surface of radius substantially equal to the radius of the central flat surface of the first diamond crystal, a first bevel region, of substantially annular shape, of facets with an associated first bevel angle, contiguous to and surrounding the perimeter of the flat surface, with outer annulus radius substantially 60-90 μm, and a second bevel region, of substantially annular shape, of facets with an associated second bevel angle, contiguous to and surrounding the outer perimeter of the first bevel region, with outer annulus radius substantially 120 μm or greater; a planar sheet of high yield strength material, with an aperture in the sheet of radius substantially equal to the radius of the central flat surface in the first diamond crystal and with a sheet thickness of substantially 10-40 μm adjacent to the aperture; and with the planes of the flat surfaces of the two diamond crystals being oriented parallel to one another, being spaced apart by a distance substantially equal to the planar sheet thickness, and being positioned so that these flat surfaces and the perimeter of the planar sheet aperture form a substantially closed chamber.
Claim 2
Dependent Claim 288 words
Improved diamond anvil apparatus, the apparatus comprising: a first diamond crystal, including a centrally positioned flat surface of radius substantially 15-45 μm, a first bevel region, of substantially annular shape, of facets with an associated first bevel angle, contiguous to and surrounding the perimeter of the flat surface, with outer annulus radius substantially 60-90 μm, and a second bevel region, of substantially annular shape, of facets with an associated second bevel angle, contiguous to and surrounding the outer perimeter of the first bevel region, with outer annulus radius substantially 120 μm or greater; a second diamond crystal, including a centrally positioned flat surface of radius substantially equal to the radius of the central flat surface of the first diamond crystal, a first bevel region, of substantially annular shape, of facets with an associated first bevel angle, contiguous to and surrounding the perimeter of the flat surface, with outer annulus radius substantially 60-90 μm, and a second bevel region, of substantially annular shape, of facets with an associated second bevel angle, contiguous to and surrounding the outer perimeter of the first bevel region, with outer annulus radius substantially 120 μm or greater; a planar sheet of high yield strength material, with an aperture in the sheet of radius substantially equal to the radius of the central flat surface in the first diamond crystal and with a sheet thickness of substantially 10-40 μm adjacent to the aperture; and with the planes of the flat surfaces of the two diamond crystals being oriented parallel to one another, being spaced apart by a distance substantially equal to the planar sheet thickness, and being positioned so that these flat surfaces and the perimeter of the planar sheet aperture form a substantially closed chamber.
Claim 3
Dependent Claim 30 words
Apparatus according to claim 1, wherein said first bevel angle of said first diamond crystal and said first bevel angle of said second diamond crystal are each substantially 3-8 degrees.
Claim 4
Dependent Claim 30 words
Apparatus according to claim 2, wherein said second bevel angle of said first diamond crystal and said second bevel angle of said second diamond crystal are each substantially 1-6 degrees.
Claim 5
Dependent Claim 288 words
Improved sapphire anvil apparatus, the apparatus comprising: a first sapphire crystal, including a centrally positioned flat surface of radius substantially 15-500 μm, a first bevel region, of substantially annular shape, of facets with an associated first bevel angle, contiguous to and surrounding the perimeter of the flat surface, with outer annulus radius substantially 60-2500 μm, and a second bevel region, of substantially annular shape, of facets with an associated second bevel angle, contiguous to and surrounding the outer perimeter of the first bevel region, with outer annulus radius substantially 120 μm or greater; a second sapphire crystal, including a centrally positioned flat surface of radius substantially equal to the radius of the central flat surface of the first sapphire crystal, a first bevel region, of substantially annular shape, of facets with an associated first bevel angle, contiguous to and surrounding the perimeter of the flat surface, with outer annulus radius substantially 60-2500 μm, and a second bevel region, of substantially annular shape, of facets with an associated second bevel angle, contiguous to and surrounding the outer perimeter of the first bevel region, with outer annulus radius substantially 120 μm or greater; a planar sheet of high yield strength material, with an aperture in the sheet of radius substantially equal to the radius of the central flat surface in the first diamond crystal and with a sheet thickness of substantially 10-40 μm adjacent to the aperture; and with the planes of the flat surfaces of the two sapphire crystals being oriented parallel to one another, being spaced apart by a distance substantially equal to the planar sheet thickness, and being positioned so that these flat surfaces and the perimeter of the planar sheet aperture form a substantially closed chamber.
Claim 6
Dependent Claim 288 words
Improved sapphire anvil apparatus, the apparatus comprising: a first sapphire crystal, including a centrally positioned flat surface of radius substantially 15-500 μm, a first bevel region, of substantially annular shape, of facets with an associated first bevel angle, contiguous to and surrounding the perimeter of the flat surface, with outer annulus radius substantially 60-2500 μm, and a second bevel region, of substantially annular shape, of facets with an associated second bevel angle, contiguous to and surrounding the outer perimeter of the first bevel region, with outer annulus radius substantially 120 μm or greater; a second sapphire crystal, including a centrally positioned flat surface of radius substantially equal to the radius of the central flat surface of the first sapphire crystal, a first bevel region, of substantially annular shape, of facets with an associated first bevel angle, contiguous to and surrounding the perimeter of the flat surface, with outer annulus radius substantially 60-2500 μm, and a second bevel region, of substantially annular shape, of facets with an associated second bevel angle, contiguous to and surrounding the outer perimeter of the first bevel region, with outer annulus radius substantially 120 μm or greater; a planar sheet of high yield strength material, with an aperture in the sheet of radius substantially equal to the radius of the central flat surface in the first diamond crystal and with a sheet thickness of substantially 10-40 μm adjacent to the aperture; and with the planes of the flat surfaces of the two sapphire crystals being oriented parallel to one another, being spaced apart by a distance substantially equal to the planar sheet thickness, and being positioned so that these flat surfaces and the perimeter of the planar sheet aperture form a substantially closed chamber.

References Cited (Backward Citations)

US3079505A Cited
US3509597A Cited
US3610757A Cited
US4151253A Cited
US4339252A Cited
US4602377A Cited
US4715711A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-10-11 1992-04-11 1992-10-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-10-11 1996-04-11 1996-10-11 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-10-11 2000-04-11 2000-10-11 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag