Low oxygen barrier type plastic closure with an adhered gasketing compound and method of forming same
Abstract
Abstract A container closure formed from a thermoplastic polyolefin, e.g. polypropylene, which has been molded and adheres simultaneously to a coated foil, e.g. an aluminum insert, to which a conventional plastisol gasketing compound may be adhered to provide a hermetic container seal under hot fill and retort conditions. In order to facilitate adhesion to both the polypropylene closure panel and the PVC plastisol gasketing compound, a dead soft aluminum foil web was first coated on one side with an organosol utilizing a gravure coater, after which the coated web was passed through an oven. The partially coated web was then coated with a primer dispersion again utilizing a gravure coater, after which the coated web was passed through a second oven. A layer of polypropylene homopolymer was applied to the primer and inserts were die cut from the resultant web. The inserts were incorporated in a closure injection molding apparatus and a plastic closure injection molded thereabout. Thereafter a plastisol gasket compound was applied to the exposed surface of the insert and fused by convection and/or induction or dielectric heat.
Inventors
- 👤 Alfred W. Kehe
- 👤 John N. Banich, Sr.
Bibliographic Details
Claims Analysis
Total Claims: 14References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1991-09-27 | 1992-03-28 | 1992-09-27 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1995-09-27 | 1996-03-28 | 1996-09-27 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1999-09-27 | 2000-03-28 | 2000-09-27 | $7700.00 | Window Closed / Lapsed |