← Back to Patent Explorer
US4769682A Expired / Lapsed US ⏱️ 0.0 years remaining

Boron doped semiconductor materials and method for producing same

Assignee: United Solar Systems Corp
•
Filing: 1987-04-20
•
Granted: 1988-09-06
•
Expires: 2007-04-20
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An improved p-type semiconductor alloy film, an improved substantially intrinsic amorphous semiconductor alloy film, improved photovoltaic and photoresponsive devices incorporating such films and r.f. and microwave glow discharge methods for fabricating same. The improved semiconductor alloy films preferably include at least silicon deposited by the glow discharge of a compound containing at least silicon and a boron species that remains substantially monoatomic as it is incorporated into the silicon matrix. The p-type film is particularly stable, is characterized by a non-narrowed band gap, reduced bulk stress, improved morphology, growth and adhesion and reduced peeling and cracking. The substantially intrinsic film is characterized by substantially reduced Staebler-Wronski degradation. The method includes the novel step of introducing a boron species that does not form higher order boron hydrides or other boron polymers or oligomers in the glow discharge plasma.

Inventors

  • 👤 Chi C. Yang
  • 👤 Ralph Mohr
  • 👤 Stephen Hudgens
  • 👤 Annette Johncock
  • 👤 Prem Nath

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 19:13
CPC Classifications
H; H10; H10F; H10F71/00; H10F71/10; H10F71/107; G; G03; G03G; G03G5/00; G03G5/02; G03G5/04; G03G5/08; G03G5/082; G03G5/08214; G03G5/08264; G03G5/08278; H10F71/103; H10P; H10P14/00; H10P14/20; H10P14/24; H10P14/29; H10P14/2901; H10P14/2923; H10P14/32; H10P14/3202; H10P14/3204; H10P14/3211; H10P14/3242; H10P14/3244; H10P14/3251; H10P14/34; H10P14/3402; H10P14/3404; H10P14/3411; H10P14/3438; H10P14/3441; H10P14/3444; Y; Y02; Y02E; Y02E10/00; Y02E10/50; Y02P; Y02P70/00; Y02P70/50

Claims Analysis

Total Claims: 26
Claim 1
Independent Claim 95 words
In an electronic device which includes at least one pair of adjacent p-doped and n-doped thin film semiconductor alloy layers; a tunnel junction formed between said doped layers, said tunnel junction indicated by a kink in the first quadrant of the IV curve thereof; said kink representing the impediment encountered by charge carriers tunnelling through the p-n interface; the improvement comprising, in combination; means adapted to improve the tunneling of charge carriers through the p-n interface to such an extent that the kink in the first quadrant of the IV curve thereof is substantially eliminated.
Claim 2
Dependent Claim 95 words
In an electronic device which includes at least one pair of adjacent p-doped and n-doped thin film semiconductor alloy layers; a tunnel junction formed between said doped layers, said tunnel junction indicated by a kink in the first quadrant of the IV curve thereof; said kink representing the impediment encountered by charge carriers tunnelling through the p-n interface; the improvement comprising, in combination; means adapted to improve the tunneling of charge carriers through the p-n interface to such an extent that the kink in the first quadrant of the IV curve thereof is substantially eliminated.
Claim 3
Dependent Claim 23 words
A device as in claim 1, wherein at least one p-doped semiconductor alloy layer includes at least boron and a halogen or pseudo-halogen.
Claim 4
Dependent Claim 13 words
A device as in claim 2, wherein the halogen or pseudo-halogen is fluorine.
Claim 5
Dependent Claim 15 words
A device as in claim 3, wherein the semiconductor is silicon or a silicon alloy.
Claim 6
Dependent Claim 15 words
A device as in claim 3, wherein the semiconductor is germanium or a germanium alloy.
Claim 7
Dependent Claim 13 words
A device as in claim 3, wherein the semiconductor is a silicon-germanium alloy.
Claim 8
Dependent Claim 18 words
A device as in claim 3, wherein the boron is substantially tetrahedrally incorporated into the semiconductor host matrix.
Claim 9
Dependent Claim 22 words
A device as in claim 2, wherein the device is a tandem p-i-n type photovoltaic device which includes at least two cells.
Claim 10
Dependent Claim 126 words
In a photovoltaic device which includes a p-doped and an n-doped thin film semiconductor alloy layer the p-doped and the n-doped layer sandwich a layer of substantially intrinsic thin film semiconductor alloy material; the p-doped layer incorporating at least boron and a halogen or a pseudo-halogen therein; the improvement comprising, in combination: said p-doped layer (1) monoatomically incorporating boron species in the semiconductor alloy matrix, (2) exhibiting reduced bulk stress, and (3) having a band gap substantially equal to the band gap of an undoped semiconductor alloy; and said intrinsic layer monoatomically incorporating at least trace amounts of boron, whereby the device is characterized by reduced Staebler-Wronski degradation, the field of the n-doped/intrinsic layer interface is enhanced, and minimum light absorbtion occurs in the p-doped layer.
Claim 11
Dependent Claim 126 words
In a photovoltaic device which includes a p-doped and an n-doped thin film semiconductor alloy layer the p-doped and the n-doped layer sandwich a layer of substantially intrinsic thin film semiconductor alloy material; the p-doped layer incorporating at least boron and a halogen or a pseudo-halogen therein; the improvement comprising, in combination: said p-doped layer (1) monoatomically incorporating boron species in the semiconductor alloy matrix, (2) exhibiting reduced bulk stress, and (3) having a band gap substantially equal to the band gap of an undoped semiconductor alloy; and said intrinsic layer monoatomically incorporating at least trace amounts of boron, whereby the device is characterized by reduced Staebler-Wronski degradation, the field of the n-doped/intrinsic layer interface is enhanced, and minimum light absorbtion occurs in the p-doped layer.
Claim 12
Dependent Claim 13 words
A device as in claim 9, wherein the halogen or pseudo-halogen is fluorine.
Claim 13
Dependent Claim 21 words
A device as in claim 10, wherein the semiconductor alloy in each of the layers is silicon or a silicon alloy.
Claim 14
Dependent Claim 21 words
A device as in claim 10, wherein the semiconductor in each of the alloy layers is germanium or a germanium alloy.
Claim 15
Dependent Claim 20 words
A device as in claim 10, wherein the semiconductor in each of the alloy layers is a silicon-germanium alloy. PG,76
Claim 16
Dependent Claim 35 words
A device as in claim 10, wherein the trace levels of boron are graded through at least a portion of the bulk of the intrinsic layer for profiling the field induced across said intrinsic layer.
Claim 17
Dependent Claim 35 words
A device as in claim 10, wherein the intrinsic layer further includes fluorine for reducing the density of defect states in the band gap thereof and stabilizing the boron atoms by filling vacant orbitals thereof.
Claim 18
Dependent Claim 98 words
In a semiconductor structure which includes at least one thin film p-doped semiconductor alloy layer upon which at least one other thin film semiconductor alloy layer is subsequently deposited, said p-doped semiconductor alloy layer including at least boron incorporated into the semiconductor host matrix; the improvement comprising, in combination; the boron being incorporated, in monoatomic species, into the semiconductor alloy host matrix so as to provide a morphologically improved surface for the growth of said subsequently deposited semiconductor alloy layers, whereby a non-cloudy, non-hazy series of semiconductor alloy layers are formed for the adsorption of incident solar radiation.
Claim 19
Dependent Claim 98 words
In a semiconductor structure which includes at least one thin film p-doped semiconductor alloy layer upon which at least one other thin film semiconductor alloy layer is subsequently deposited, said p-doped semiconductor alloy layer including at least boron incorporated into the semiconductor host matrix; the improvement comprising, in combination; the boron being incorporated, in monoatomic species, into the semiconductor alloy host matrix so as to provide a morphologically improved surface for the growth of said subsequently deposited semiconductor alloy layers, whereby a non-cloudy, non-hazy series of semiconductor alloy layers are formed for the adsorption of incident solar radiation.
Claim 20
Dependent Claim 19 words
A structure as in claim 16, wherein the p-doped semiconductor alloy layer further includes a halogen or a pseudo-halogen.
Claim 21
Dependent Claim 14 words
A structure as in claim 17, wherein the halogen or the pseudo-halogen is fluorine.
Claim 22
Dependent Claim 15 words
A structure as in claim 17, wherein the semiconductor is silicon or a silicon alloy.
Claim 23
Dependent Claim 15 words
A structure as in claim 17, wherein the semiconductor is germanium or a germanium alloy.
Claim 24
Dependent Claim 13 words
A structure as in claim 17, wherein the semiconductor is a silicon-germanium alloy.
Claim 25
Dependent Claim 18 words
A structure as in claim 17, wherein the boron is substantially tetrahedrally incorporated into the semiconductor host matrix.
Claim 26
Dependent Claim 15 words
A structure as in claim 17, wherein the structure is a tandem p-i-n photovoltaic cell.

References Cited (Backward Citations)

US4605941A Cited
US4703336A Cited
US4703336B1 Cited
US4703336B2 Cited
US4698658A Cited
US4600801A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-09-06 1992-03-07 1992-09-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-09-06 1996-03-07 1996-09-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-09-06 2000-03-07 2000-09-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag