Abstract

Abstract This invention relates to an improved injection molding nozzle and method of making it. The components are assembled and dipped in lacquer and powdered nickel prior to brazing in a vacuum furnace. This integrally brazes the components together, embeds an electrical heating element in a spiral channel, and provides the surfaces with a protective nickel coating. In one embodiment, the forward end has an integral high speed steel insert and the remote end of the heating element extends into the forward end of the nozzle. In addition to providing the protective coating, carrying out the method with a single vacuum brazing step considerably reduces manufacturing costs.

Inventors

  • 👤 Jobst U. Gellert

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 14:23
CPC Classifications
B; B29; B29C; B29C45/00; B29C45/17; B29C45/26; B29C45/27; B29C45/2735; B29C45/2737; B29C2045/274; B29C2045/2774; B29C45/278; B29C2045/2782; B29C2045/2783; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49082; Y10T29/49083; Y10T29/49826; Y10T29/49888

Claims Analysis

Total Claims: 22
Claim 1
Independent Claim 339 words
A method of making an integral injection molding heated nozzle comprising the steps of: (a) forming an elongated steel body having a forward end, a rear end and a melt bore extending therethrough, the melt bore extending centrally from the rear end to adjacent the front end, the body having a neck portion adjacent the rear end and a generally cylindrical outer surface extending from the neck portion to adjacent the front end, the cylindrical outer surface having a spiral channel extending therearound, (b) winding an electrically insulated heating element in the channel with a remote end fixed adjacent the forward end of the body and a cold terminal at the opposite end extending radially from the channel adjacent the rear end of the body, (c) forming a steel collar portion having a central opening therethrough to snugly receive the neck portion of the body therein, the collar portion also having an opening extending radially therethrough from the central opening to receive therethrough the end of the heating element having the cold terminal, (d) locating the collar portion in position on the rear end of the body with the neck portion of the body extending through the central opening in the collar portion, and the cold terminal projecting through the radial opening in the collar portion, (e) locating a hollow steel sleeve portion in position over the projecting cold terminal to partially enclose the cold terminal, with one end of the sleeve portion abutting against the collar portion in alignment with the radial opening therethrough, (f) applying a coating of sticky liquid and metallic powder to the surfaces of the assembled body, collar portion and sleeve portion, and (g) heating the assembly in a vacuum furnace for a period of time and to a temperature sufficient to melt the metallic powder and remove the liquid, thereby integrally brazing the body, collar portion and sleeve portion together and the heating element in the channel, and providing a protective metallic coating of substantially uniform thickness over the surfaces of the assembly.
Claim 2
Independent Claim 339 words
A method of making an integral injection molding heated nozzle comprising the steps of: (a) forming an elongated steel body having a forward end, a rear end and a melt bore extending therethrough, the melt bore extending centrally from the rear end to adjacent the front end, the body having a neck portion adjacent the rear end and a generally cylindrical outer surface extending from the neck portion to adjacent the front end, the cylindrical outer surface having a spiral channel extending therearound, (b) winding an electrically insulated heating element in the channel with a remote end fixed adjacent the forward end of the body and a cold terminal at the opposite end extending radially from the channel adjacent the rear end of the body, (c) forming a steel collar portion having a central opening therethrough to snugly receive the neck portion of the body therein, the collar portion also having an opening extending radially therethrough from the central opening to receive therethrough the end of the heating element having the cold terminal, (d) locating the collar portion in position on the rear end of the body with the neck portion of the body extending through the central opening in the collar portion, and the cold terminal projecting through the radial opening in the collar portion, (e) locating a hollow steel sleeve portion in position over the projecting cold terminal to partially enclose the cold terminal, with one end of the sleeve portion abutting against the collar portion in alignment with the radial opening therethrough, (f) applying a coating of sticky liquid and metallic powder to the surfaces of the assembled body, collar portion and sleeve portion, and (g) heating the assembly in a vacuum furnace for a period of time and to a temperature sufficient to melt the metallic powder and remove the liquid, thereby integrally brazing the body, collar portion and sleeve portion together and the heating element in the channel, and providing a protective metallic coating of substantially uniform thickness over the surfaces of the assembly.
Claim 3
Dependent Claim 25 words
A method as claimed in claim 1 wherein step (f) comprises applying a coating of sticky liquid and then applying a coating of metallic powder.
Claim 4
Dependent Claim 25 words
A method as claimed in claim 2 wherein the coating of sticky liquid is applied by dipping the assembly in a bath of sticky liquid.
Claim 5
Dependent Claim 17 words
A method as claimed in claim 2 wherein the coating of sticky liquid is applied by spraying.
Claim 6
Dependent Claim 23 words
A method as claimed in claim 2 wherein the coating of metallic powder is applied by dipping the assembly in agitated metallic powder.
Claim 7
Dependent Claim 17 words
A method as claimed in claim 2 wherein the coating of metallic powder is applied by spraying.
Claim 8
Dependent Claim 25 words
A method as claimed in claim 2 wherein the sticky liquid is an acrylic lacquer and the metallic powder is nickel or an alloy thereof.
Claim 9
Dependent Claim 53 words
A method as claimed in claim 1 further including shaping the forward end of the body to receive a high speed steel portion, integrally brazing the high speed steel portion to the body in step (g), and machining to provide the body with a high speed steel forward end of a selected configuration.
Claim 10
Dependent Claim 25 words
A method as claimed in claim 8 including machining to provide the forward end with a conical surface having an integral high speed steel tip.
Claim 11
Dependent Claim 32 words
A method as claimed in claim 9 including drilling melt bores to extend diagonally from the conical surface to join the melt bore extending centrally from the rear end of the body.
Claim 12
Dependent Claim 29 words
A method as claimed in claim 8 including forming the steel body with an outwardly projecting circumferential sealing flange located between the cylindrical outer surface and the forward end.
Claim 13
Dependent Claim 59 words
A method as claimed in claim 11 including drilling a hole in the body to extend diagonally beneath the sealing flange from the spiral channel into the forward end, and inserting the remote end of the heating element into the hole prior to winding the heating element in the spiral channel in the cylindrical outer surface of the body.
Claim 14
Dependent Claim 64 words
A method as claimed in claim 8 including forming the body with a nose portion, drilling a hole centrally in the nose portion, brazing a high speed steel insert portion into the hole in step (g), and machining the nose portion and the insert portion to provide the forward end of the body with a conical surface having an integral high speed steel tip.
Claim 15
Dependent Claim 53 words
A method as claimed in claim 13 including orienting the assembly with the forward end upright, placing the insert portion into the hole in the nose portion, pouring a predetermined quantity of nickel powder into the hole on top of the insert portion, and then brazing with this same orientation in step (g).
Claim 16
Dependent Claim 33 words
A method as claimed in claim 14 including forming the steel body with an outwardly projecting circumferential sealing flange located between the cylindrical outer surface and the conical surface of the forward end.
Claim 17
Dependent Claim 61 words
A method as claimed in claim 15 including drilling a hole in the body to extend diagonally beneath the sealing flange from the spiral channel into the conical shaped forward end, and inserting the remote end of the heating element into the hole prior to winding the heating element in the spiral channel in the cylindrical outer surface of the body.
Claim 18
Dependent Claim 35 words
A method as claimed in claim 16 wherein the diagonal hole extending into the conical shaped forward end meets the central hole drilled in the nose portion to receive the high speed steel insert portion.
Claim 19
Dependent Claim 56 words
A method as claimed in claim 1 including making the collar portion with a circumferential insulation flange which is larger in diameter than the outer surface of the body, whereby when assembled the insulation flange extends towards the forward end of the nozzle around the outer surface of the body with an insulative air space therebetween.
Claim 20
Dependent Claim 43 words
A method as claimed in claim 1 including providing the outer surface of the heating element and the abutting surfaces of the body, collar portion and sleeve portion with a rough finish to promote capilliary action of the nickel in the brazing step.
Claim 21
Dependent Claim 19 words
A method as claimed in claim 1 wherein the coating is applied to the surface of the melt bore.
Claim 22
Dependent Claim 38 words
A method as claimed in claim 1 including machining a hole diagonally into the body to adjacent the forward end to removably receive a thermocouple therein to measure the operating temperature of the body adjacent the forward end.

References Cited (Backward Citations)

CA532677A Cited
US4238671A Cited
US4643664A Cited
US4386262A Cited
US4355460A Cited
US4344750A Cited
US4403405A Cited
US4446360A Cited
US4557685A Cited
US4583284A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-09-06 1992-03-07 1992-09-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-09-06 1996-03-07 1996-09-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-09-06 2000-03-07 2000-09-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag