Abstract

Abstract This invention relates to an improved heated nozzle for injection molding and an improved method of manufacturing it. The nozzle has an elongated body with a melt bore extending generally centrally through it. The cylindrical outer surface of the body has a variable pitched spiral channel extending around it along its length. A helical electric heating element is embedded in the channel to form an integral structure by which the temperature of the hot melt can be maintained within a narrow range as it flows through the bore. The nozzle is manufactured by forming the body with the channel and bore either by investment casting or machining. The heating element is wound in the channel and a bead of nickel brazing paste is run along the top of it. The nozzle is then heated in a vacuum furnace to braze the heating element in the channel. The highly conductive nickel completely covers the heating element and is fused to both the heating element and the walls of the channel. Thus, a low cost integral nozzle is provided which during use efficiently dissipates heat from the element to prolong its effective life, and applies the heat uniformly along the melt bore.

Inventors

  • 👤 Jobst U. Gellert

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 17:30
CPC Classifications
B; B29; B29C; B29C45/00; B29C45/17; B29C45/26; B29C45/27; B29C45/2737; B29C2045/274; B29C2045/2743; B29C2045/2748; B29C2045/2751; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49082; Y10T29/49083; Y10T29/49087; Y10T29/49096

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 186 words
A method of manufacturing an integral injection molding heated nozzle, comprising the steps of: (a) forming an elongated steel body with an inlet end, an outlet end, and a generally cylindrical outer surface, the body having a melt bore extending longitudinally therethrough from a central melt inlet at the inlet end to a melt outlet adjacent the outlet end, the generally cylindrical outer surface having a generally spiral channel extending therein from a first end adjacent the inlet end of the body to a second end adjacent the outlet end of the body; (b) locating an electrically insulated heating element in the channel to extend helically around the body of the nozzle, the heating element having a cold terminal extending from the first end of the channel; (c) applying a bead of highly conductive material along the heating element adjacent the channel; and (d) heating the body in a vacuum furnace for a period of time and at a temperature sufficient to melt the highly conductive material and bond it to the heating element in the channel to integrally embed the heating element in the channel.
Claim 2
Independent Claim 186 words
A method of manufacturing an integral injection molding heated nozzle, comprising the steps of: (a) forming an elongated steel body with an inlet end, an outlet end, and a generally cylindrical outer surface, the body having a melt bore extending longitudinally therethrough from a central melt inlet at the inlet end to a melt outlet adjacent the outlet end, the generally cylindrical outer surface having a generally spiral channel extending therein from a first end adjacent the inlet end of the body to a second end adjacent the outlet end of the body; (b) locating an electrically insulated heating element in the channel to extend helically around the body of the nozzle, the heating element having a cold terminal extending from the first end of the channel; (c) applying a bead of highly conductive material along the heating element adjacent the channel; and (d) heating the body in a vacuum furnace for a period of time and at a temperature sufficient to melt the highly conductive material and bond it to the heating element in the channel to integrally embed the heating element in the channel.
Claim 3
Dependent Claim 18 words
A method as claimed in claim 1 wherein step (a) comprises forming the steel body by investment casting.
Claim 4
Dependent Claim 29 words
A method as claimed in claim 2 comprising the further step of coating the bead of highly conductive material with acrylic lacquer prior to heating in the vacuum furnace.
Claim 5
Dependent Claim 29 words
A method as claimed in claim 2 comprising the further step of machining at least a portion of the outer surface of the body to provide a smooth finish.
Claim 6
Dependent Claim 63 words
A method as claimed in claim 2 comprising the further steps of mounting an insulation bushing and connector sleeve on the nozzle, apply brazing paste having a melting temperature lower than the melting temperature of the said highly conductive material to the necessary joints, and brazing in a vacuum furnace at a temperature lower than the melting temperature of said highly conductive material.
Claim 7
Dependent Claim 26 words
A method as claimed in claim 1 wherein step (a) includes cutting the channel into the outer surface of the body with an automatic machine tool.
Claim 8
Dependent Claim 29 words
A method as claimed in claim 6 comprising the further step of coating the bead of highly conductive material with acrylic lacquer prior to heating in the vacuum furnace.
Claim 9
Dependent Claim 29 words
A method as claimed in claim 6 comprising the further step of machining at least a portion of the outer surface of the body to provide a smooth finish.
Claim 10
Dependent Claim 63 words
A method as claimed in claim 6 comprising the further steps of mounting an insulation bushing and connector sleeve on the nozzle, apply brazing paste having a melting temperature lower than the melting temperature of the said highly conductive material to the necessary joints, and brazing in a vacuum furnace at a temperature lower than the melting temperature of said highly conductive material.

References Cited (Backward Citations)

US2647976A Cited
US2858401A Cited
US4349145A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-04-21 1989-10-21 1990-04-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-04-21 1993-10-21 1994-04-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-04-21 1997-10-21 1998-04-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag