Storage stable polyurethane coating

Assignee: Huntsman Corp
•
Filing: 1987-05-18
•
Granted: 1988-08-30
•
Expires: 2007-05-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A storage stable polyurethane coating composition which may be heat cured under relatively mild conditions comprising an isocyanate which has been chemically blocked and a curing agent comprising a partially alkoxylated polyoxyalkylene amine is described.

Inventors

  • 👤 Michael Cuscurida

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 07:36
CPC Classifications
C; C08; C08G; C08G18/00; C08G18/06; C08G18/28; C08G18/30; C08G18/32; C08G18/3271; C08G18/3275; C08G18/40; C08G18/48; C08G18/50; C08G18/5021; C08G18/70; C08G18/72; C08G18/80; C08G18/8061

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 26 words
A storage stable, heat curable polyurethane coating comprising a blocked isocyanate and a curing agent comprising a partially alkoxylated polyoxyalkylene amine of the general formula: ##STR4##
Claim 2
Dependent Claim 26 words
A storage stable, heat curable polyurethane coating comprising a blocked isocyanate and a curing agent comprising a partially alkoxylated polyoxyalkylene amine of the general formula: ##STR4##
Claim 3
Dependent Claim 44 words
A heat curable polyurethane coating as in claim 1 wherein the curing agent comprises a partially alkoxylated polyoxyalkylene amine of about 200 to 5000 molecular weight with a functionality of about 2 to 3 which has been alkoxylated from about 25 to 75 percent.
Claim 4
Dependent Claim 39 words
A storage stable, heat curable polyurethane coating comprising a blocked isocyanate and a curing agent comprising a partially alkoxylated polyoxyalkylene amine wherein the isocyanate is a prepolymer and the partially alkoxylated polyoxyalkylene amine is of the general formula: ##STR5##
Claim 5
Dependent Claim 39 words
A storage stable, heat curable polyurethane coating comprising a blocked isocyanate and a curing agent comprising a partially alkoxylated polyoxyalkylene amine wherein the isocyanate is a prepolymer and the partially alkoxylated polyoxyalkylene amine is of the general formula: ##STR5##

References Cited (Backward Citations)

US4590009A Cited
JPS58270A Cited
US4490520A Cited
US4491663A Cited
US4495229A Cited
US4465858A Cited
GB2151643A Cited
US4624996A Cited
US4590254A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-08-30 1992-02-29 1992-08-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-08-30 1996-02-29 1996-08-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-08-30 2000-02-29 2000-08-30 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag