Abstract

Abstract An acid gold electroplating bath contains gold in an electrodepositable form, (e.g. potassium gold cyanide), together with 3-(3-pyridyl) acrylic acid or 3-(3-quinolyl) acrylic acid, and optionally a metallic additive. The metallic additive is preferably a cobalt, nickel or iron salt.

Inventors

  • 👤 Peter Wilkinson

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 18:50
CPC Classifications
C; C25; C25D; C25D3/00; C25D3/02; C25D3/48

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 26 words
An acid gold electroplating bath comprising gold in electrodepositable form and one or more additives selected from 3-(3-pyridyl) acrylic acid, 3-(3-quinolyl) acrylic acid, and salts thereof.
Claim 2
Dependent Claim 26 words
An acid gold electroplating bath comprising gold in electrodepositable form and one or more additives selected from 3-(3-pyridyl) acrylic acid, 3-(3-quinolyl) acrylic acid, and salts thereof.
Claim 3
Dependent Claim 15 words
An acid gold electroplating bath according to claim 1, which also contains a metallic additive.
Claim 4
Dependent Claim 20 words
An acid gold electroplating bath according to claim 1, wherein the metallic additive is a cobalt, nickel or iron salt.
Claim 5
Dependent Claim 25 words
An acid gold electroplating bath according to claim 1, wherein 3-(3-pyridyl) acrylic acid is present at a concentration of from 0.01 g/l to 5 g/l.
Claim 6
Dependent Claim 25 words
An acid gold electroplating bath according to claim 1, wherein 3-(3-pyridyl) acrylic acid is present at a concentration of from 0.5 g/l to 1.0 g/l.
Claim 7
Dependent Claim 28 words
An acid gold electroplating bath according to claim 1, wherein the gold is present as a water soluble complex at a concentration of from 1 to 20 g/l.
Claim 8
Dependent Claim 23 words
A process for forming a gold deposit on a metallic article, comprising electroplating said article in a bath as claimed in claim 1.

References Cited (Backward Citations)

CH455434A Cited
DE2237807A1 Cited
US3901773A Cited
US3929595A Cited
US4038161A Cited
EP0150439A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-08-30 1992-02-29 1992-08-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-08-30 1996-02-29 1996-08-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-08-30 2000-02-29 2000-08-30 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag