Abstract

Abstract A silver halide color photographic light-sensitive material has a support and at least one silver halide emulsion layer. At least one of the silver halide emulsion layers has a group of substantially monodisperse core/shell type silver halide grains having a value of not greater than 0.15. This value is obtained by dividing a standard deviation value by the average grain size value. The substantially monodisperse core/shell-type silver halide grains have shells from 0.01 to 0.1 in thickness. The silver halide grains include a silver iodide in the core in an amount of less than 8 mole % and a silver iodide in the shell of from 0.1 mole % to 6 mole %. A development inhibitor releasing compound having a relative development inhibitability of not less than 1 is also present in the emulsion layer.

Inventors

  • 👤 Katsumasa Yamazaki
  • 👤 Toshihiko Yagi
  • 👤 Kenji Michiue
  • 👤 Sohei Goto
  • 👤 Yoshiharu Mochizuki

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 04:24
CPC Classifications
G; G03; G03C; G03C7/00; G03C7/30; G03C7/3003; G03C7/305; G03C1/00; G03C1/005; G03C1/035; G03C2001/03535; G03C7/30541; Y; Y10; Y10S; Y10S430/00; Y10S430/156; Y10S430/158

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 237 words
A silver halide color photographic light-sensitive material comprising a support having thereon at least one silver halide emulsion layer, wherein at least one of said silver halide emulsion layers includes a group of substantially monodisperse core/shell-type silver halide grains having a value of not greater than 0.15, said value being obtained by dividing a standard deviation value by the average grain size value, wherein said substantially monodisperse core/shell-type silver halide grains have a shell of a thickness of 0.01μ to 0.1μ and wherein the silver halide grains contain a silver iodide in the core thereof in an amount of not less than 8 mole % and a silver iodide in the shell thereof in an amount from 0.1 mole % to 6 mole %; and (b) a development inhibitor releasing compound which releases a development inhibitor by the reaction thereof with the oxidized product of a color developing agent and wherein said development inhibiting releasing compound has a relative development inhibitability ρs of not less than 1, as defined below: ##EQU4## wherein, ρ represents a development inhibitability of the DIR compound to be used; γi represents a gamma value of a color developed silver halide color photographic light-sensitive material containing the aforementioned DIR compound; γ0 represents a gamma value of a color developed silver halide color photographic light-sensitive material not containing the DIR compound; ρB represents a development inhibitability of the following DIR compound D B ##STR24##
Claim 2
Dependent Claim 237 words
A silver halide color photographic light-sensitive material comprising a support having thereon at least one silver halide emulsion layer, wherein at least one of said silver halide emulsion layers includes a group of substantially monodisperse core/shell-type silver halide grains having a value of not greater than 0.15, said value being obtained by dividing a standard deviation value by the average grain size value, wherein said substantially monodisperse core/shell-type silver halide grains have a shell of a thickness of 0.01μ to 0.1μ and wherein the silver halide grains contain a silver iodide in the core thereof in an amount of not less than 8 mole % and a silver iodide in the shell thereof in an amount from 0.1 mole % to 6 mole %; and (b) a development inhibitor releasing compound which releases a development inhibitor by the reaction thereof with the oxidized product of a color developing agent and wherein said development inhibiting releasing compound has a relative development inhibitability ρs of not less than 1, as defined below: ##EQU4## wherein, ρ represents a development inhibitability of the DIR compound to be used; γi represents a gamma value of a color developed silver halide color photographic light-sensitive material containing the aforementioned DIR compound; γ0 represents a gamma value of a color developed silver halide color photographic light-sensitive material not containing the DIR compound; ρB represents a development inhibitability of the following DIR compound D B ##STR24##
Claim 3
Dependent Claim 40 words
A silver halide photographic light-sensitive material as claimed in claim 1, wherein said silver halide emulsion layer comprises said development inhibitor releasing compound in an amount of from 0.0001 mole to 0.01 mole per mole of the silver halide thereof.
Claim 4
Dependent Claim 26 words
A silver halide photographic light-sensitive material as claimed in claim 1, wherein said relative development inhibitability ρs is in the range of from 1 to 2.

References Cited (Backward Citations)

US3206313A Cited
US3317322A Cited
US4444877A Cited
US4461826A Cited
US4477564A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-08-09 1992-02-08 1992-08-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-08-09 1996-02-08 1996-08-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-08-09 2000-02-08 2000-08-09 $7700.00 Window Closed / Lapsed