Abstract

Abstract A soft thermoplastic, elastomeric alloy containing a thermoplastic, elastomeric block copolymer material, a polyethylene, and a polyphenylene ether material, prepared by blending in an extruder with an L/D ratio equal to or greater than 30 to 1. The alloy comprises a blend of from about 80 to 98% thermoplastic, elastomeric block copolymer material; from about 1 to 10% by weight of low melt index, highly crystalline polyethylene; and from about 1 to 10% by weight of polyphenylene ether. The material demonstrates excellent creep resistance at elevated temperatures as well as a variety of other excellent physical properties.

Inventors

  • 👤 John A. Hudson, Jr.

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 16:40
CPC Classifications
C; C08; C08L; C08L53/00; C08L53/02; C08L53/025; Y; Y10; Y10S; Y10S525/00; Y10S525/905

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 54 words
A thermoplastic, elastomeric alloy, comprising: (a) from about 80 to 98% by weight of styrene-ethylene-butylene-styrene block copolymer; (b) from about 1 to 10% by weight of low melt index, cystalline polyethylene; and, (c) from about 1 to 10% polyphenylene ether; said elastomeric alloy having a Shore A hardness of approximately 32 to approximately 45A.
Claim 2
Dependent Claim 54 words
A thermoplastic, elastomeric alloy, comprising: (a) from about 80 to 98% by weight of styrene-ethylene-butylene-styrene block copolymer; (b) from about 1 to 10% by weight of low melt index, cystalline polyethylene; and, (c) from about 1 to 10% polyphenylene ether; said elastomeric alloy having a Shore A hardness of approximately 32 to approximately 45A.
Claim 3
Dependent Claim 48 words
A thermoplastic, elastomeric alloy comprising: (a) approximately 94% by weight of styrene-ethylene-butylene-styrene block copolymer; (b) approximately 3% by weight of low melt index, crystalline polyethylene; and, (c) approximately 3% by weight of polyphenylene ether; said elastomeric alloy having a Shore A hardness of approximately 32 to approximately 45A.
Claim 4
Dependent Claim 48 words
A thermoplastic, elastomeric alloy comprising: (a) approximately 94% by weight of styrene-ethylene-butylene-styrene block copolymer; (b) approximately 3% by weight of low melt index, crystalline polyethylene; and, (c) approximately 3% by weight of polyphenylene ether; said elastomeric alloy having a Shore A hardness of approximately 32 to approximately 45A.
Claim 5
Dependent Claim 48 words
A thermoplastic, elastomeric alloy comprising: (a) approximately 96% by weight of styrene-ethylene-butylene-styrene block copolymer; (b) approximately 2% by weight of low melt index crystalline polyethylene; and, (c) approximately 2% by weight of polyphenylene ether; said elastomeric alloy having a Shore A hardness of approximately 32 to approximately 45A.
Claim 6
Dependent Claim 48 words
A thermoplastic, elastomeric alloy comprising: (a) approximately 96% by weight of styrene-ethylene-butylene-styrene block copolymer; (b) approximately 2% by weight of low melt index crystalline polyethylene; and, (c) approximately 2% by weight of polyphenylene ether; said elastomeric alloy having a Shore A hardness of approximately 32 to approximately 45A.
Claim 7
Dependent Claim 48 words
A thermoplastic, elastomeric alloy comprising: (a) approximately 92% by weight of styrene-ethylene-butylene-styrene block copolymer; (b) approximately 2% by weight of low melt index crystalline polyethylene; and, (c) approximately 6% by weight of polyphenylene ether; said elastomeric alloy having a Shore A hardness of approximately 32 to approximately 45A.
Claim 8
Dependent Claim 48 words
A thermoplastic, elastomeric alloy comprising: (a) approximately 92% by weight of styrene-ethylene-butylene-styrene block copolymer; (b) approximately 2% by weight of low melt index crystalline polyethylene; and, (c) approximately 6% by weight of polyphenylene ether; said elastomeric alloy having a Shore A hardness of approximately 32 to approximately 45A.
Claim 9
Dependent Claim 48 words
A thermoplastic, elastomeric alloy comprising: (a) approximately 87% by weight of styrene-ethylene-butylene-styrene block copolymer; (b) approximately 5% by weight of low melt index crystalline polyethylene; and, (c) approximately 8% by weight of polyphenylene ether; said elastomeric alloy having a Shore A hardness of approximately 32 to approximately 45A.
Claim 10
Dependent Claim 48 words
A thermoplastic, elastomeric alloy comprising: (a) approximately 87% by weight of styrene-ethylene-butylene-styrene block copolymer; (b) approximately 5% by weight of low melt index crystalline polyethylene; and, (c) approximately 8% by weight of polyphenylene ether; said elastomeric alloy having a Shore A hardness of approximately 32 to approximately 45A.

References Cited (Backward Citations)

US3485787A Cited
US3830767A Cited
US4039629A Cited
US4006116A Cited
US4041103A Cited
US4166055A Cited
US4616067A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-06-28 1991-12-28 1992-06-28 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-06-28 1995-12-28 1996-06-28 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-06-28 1999-12-28 2000-06-28 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag