Bond strength measurement of composite panel products

Assignee: Weyerhaeuser Co
•
Filing: 1987-05-26
•
Granted: 1988-06-14
•
Expires: 2007-05-26
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The invention is a method for the on-line nondestructive determination of the internal bond strength of composite panel products. The method involves impinging an ultrasound pulse against the panel by a first transducer and receiving a transmitted pulse at a second transducer. The received signal strength, temperature and panel thickness are entered into an algorithm from which the internal bond may be calculated. Preferably the receiving transducer is located on the opposite side of the panel and displaced somewhat from the first transducer. The inclusion of temperature and panel thickness as independent variables greatly improves the accuracy over that available from uncorrected ultrasound testing.

Inventors

  • 👤 Dwayne M. Shearer
  • 👤 Richard C. Beetham
  • 👤 Frank C. Beall

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 18:20
CPC Classifications
G; G01; G01N; G01N29/00; G01N29/22; G01N29/32; G01N29/326; G01N29/24; G01N29/2493; G01N2291/00; G01N2291/01; G01N2291/015; G01N2291/02; G01N2291/023; G01N2291/0231; G01N2291/0237; G01N2291/04; G01N2291/048; G01N2291/10; G01N2291/102

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 113 words
A method for the on-line, nondestructive determination of the internal bond strength of composite panel products which comprises: designating a thickness class for the panels being measured; determining the temperature of the panel; impinging an ultrasound pulse against the panel through a first transducer in contact with the panel; receiving the transmitted pulse at a second transducer in contact with the panel and spaced apart from the first transducer; expressing the received signal as an output voltage; entering the temperature and output signal voltage into a linear equation of the form; IB=a+b(output voltage)+c(temperature) where the coefficients are determined for the given thickness class; and solving the equation to determine the internal bond strength.
Claim 2
Independent Claim 113 words
A method for the on-line, nondestructive determination of the internal bond strength of composite panel products which comprises: designating a thickness class for the panels being measured; determining the temperature of the panel; impinging an ultrasound pulse against the panel through a first transducer in contact with the panel; receiving the transmitted pulse at a second transducer in contact with the panel and spaced apart from the first transducer; expressing the received signal as an output voltage; entering the temperature and output signal voltage into a linear equation of the form; IB=a+b(output voltage)+c(temperature) where the coefficients are determined for the given thickness class; and solving the equation to determine the internal bond strength.
Claim 3
Dependent Claim 14 words
The method of claim 1 wherein the panel product is a composite wood panel.
Claim 4
Dependent Claim 24 words
The method of claim 1 where the output of the second transducer is the average RMS voltage produced in response to the transmitted pulse.
Claim 5
Dependent Claim 30 words
The method of claim 1 where the output of the second transducer is a voltage analog of the ringdown count of the oscillations produced in response to the transmitted pulse.
Claim 6
Dependent Claim 23 words
The method of claim 4 in which the ringdown count is measured above a bias level set greater than the ambient noise level.
Claim 7
Dependent Claim 23 words
The method of claim 1 in which the second transducer is located on the opposite side of the panel from the first transducer.
Claim 8
Dependent Claim 25 words
The method of claim 6 in which the second transducer is linearly displaced either transversely or longitudinally from the contact point of the first transducer.
Claim 9
Independent Claim 102 words
A method for the on-line, nondestructive determination of the internal bond strength of composite panel products which comprises: measuring the thickness of the panel; determining the temperature of the panel; impinging an ultrasound pulse against the panel through a first transducer in contact with the panel; receiving the transmitted pulse at a second transducer in contact with the panel and spaced apart from the first transducer; expressing the received signal as an output voltage; entering the thickness, the temperature, and output signal voltage into an equation of the form IB=a+b(output voltage)+c(temperature)+d(thickness)+e(thickness).sup.2 ; and solving the equation to determine the internal bond strength.
Claim 10
Independent Claim 102 words
A method for the on-line, nondestructive determination of the internal bond strength of composite panel products which comprises: measuring the thickness of the panel; determining the temperature of the panel; impinging an ultrasound pulse against the panel through a first transducer in contact with the panel; receiving the transmitted pulse at a second transducer in contact with the panel and spaced apart from the first transducer; expressing the received signal as an output voltage; entering the thickness, the temperature, and output signal voltage into an equation of the form IB=a+b(output voltage)+c(temperature)+d(thickness)+e(thickness).sup.2 ; and solving the equation to determine the internal bond strength.
Claim 11
Dependent Claim 14 words
The method of claim 8 wherein the panel product is a composite wood panel.
Claim 12
Dependent Claim 24 words
The method of claim 8 where the output of the second transducer is the average RMS voltage produced in response to the transmitted pulse.
Claim 13
Dependent Claim 30 words
The method of claim 8 where the output of the second transducer is a voltage analog of the ringdown count of the oscillations produced in response to the transmitted pulse.
Claim 14
Dependent Claim 23 words
The method of claim 11 in which the ringdown count is measured above a bias level set greater than the ambient noise level.
Claim 15
Dependent Claim 23 words
The method of claim 8 in which the second transducer is located on the opposite side of the panel from the first transducer.
Claim 16
Dependent Claim 25 words
The method of claim 13 in which the second transducer is linearly displaced either transversely or longitudinally from the contact point of the first transducer.

References Cited (Backward Citations)

US3384767A Cited
US3423991A Cited
US3780570A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-06-14 1991-12-14 1992-06-14 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-06-14 1995-12-14 1996-06-14 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-06-14 1999-12-14 2000-06-14 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag