Patent US4745139A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4745139A Expired / Lapsed US ⏱️ 0.0 years remaining

Elastomeric coatings containing glass bubbles

Assignee: PDI Inc
•
Filing: 1987-02-09
•
Granted: 1988-05-17
•
Expires: 2007-02-09
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A formulation for surface coating applications, particularly surfaces which are in frequent contact with water and remain water-wet, and/or surfaces of elastomeric and plastic foams, especially foams fabricated from polyethylene and polyurethane resins. The formulation includes a vehicle consisting primarily of a block polymer of styrene/ethylene/butylene/styrene and methylmethacrylate copolymer or related block polymer with lesser degrees of ethylenic unsaturation together with a rubber tackifier, with fillers being provided including particulate colloidal or powdered silicon dioxide, and glass microspheres having an average size of less than about 70 microns. The formulation is such that it is adaptable to be applied by either air pressure spray systems or aerosol packaging techniques.

Inventors

  • 👤 Robert J. Haasl
  • 👤 Thomas M. Miller
  • 👤 Scott R. Haasl

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 12:14
CPC Classifications
C; C09; C09D; C09D153/00

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 178 words
Surface coating formulation for application to surfaces in contact with water for providing surface roughness and for increasing frictional and anti-slip characteristics of such surfaces while wet, said formulation comprising: (a) a styrene/ethylene/butylene/styrene block copolymer and contained in said formulation in an amount ranging from between about 30 and 60 parts by weight; (b) finely divided silicon dioxide filler selected from the group consisting of particulate colloidal and powdered silicon dioxide and contained in said formulation in an amount ranging from between about 3 and 10 parts by weight; (c) solvent solution of methylmethacrylate copolymer solids and contained in said formulation in an amount ranging from between about 15 parts and 25 parts by weight; (d) rubber tackifier solids and contained in said formulation in an amount ranging from between about 5 parts and 15 parts by weight; and (e) glass microspheres substantially uniformly distributed in said formulation and having an average size of up to about 70 microns, and contained in said formulation in an amount ranging from between about 5 parts and 15 parts by weight.
Claim 2
Dependent Claim 178 words
Surface coating formulation for application to surfaces in contact with water for providing surface roughness and for increasing frictional and anti-slip characteristics of such surfaces while wet, said formulation comprising: (a) a styrene/ethylene/butylene/styrene block copolymer and contained in said formulation in an amount ranging from between about 30 and 60 parts by weight; (b) finely divided silicon dioxide filler selected from the group consisting of particulate colloidal and powdered silicon dioxide and contained in said formulation in an amount ranging from between about 3 and 10 parts by weight; (c) solvent solution of methylmethacrylate copolymer solids and contained in said formulation in an amount ranging from between about 15 parts and 25 parts by weight; (d) rubber tackifier solids and contained in said formulation in an amount ranging from between about 5 parts and 15 parts by weight; and (e) glass microspheres substantially uniformly distributed in said formulation and having an average size of up to about 70 microns, and contained in said formulation in an amount ranging from between about 5 parts and 15 parts by weight.
Claim 3
Dependent Claim 36 words
The formulation as set forth in claim 1 wherein said particulate solid filler is selected from the group consisting of particulate solid silicon dioxide and glass microspheres having an average size of less than 70 microns.
Claim 4
Dependent Claim 168 words
Surface coating formulation for application to surfaces of plastic foam structures for increasing frictional and anti-slip characteristics of such surfaces, said formulation comprising: (a) as styrene/ethylene/butylene/styrene block copolymer and contained in said formulation in an amount ranging from between about 30 and 60 parts by weight; (b) finely divided silicon dioxide filler selected from the group consisting of particulate colloidal and powdered silicon dioxide and contained in said formulation in an amount ranging from between about 3 and 10 parts by weight; (c) solvent solution of methylmethacrylate copolymer solids and contained in said formulation in an amount ranging from between about 15 and 25 parts by weight; (d) rubber tackifier solids and contained in said formulation in an amount ranging from between about 5 and 15 parts by weight; and (e) glass microspheres substantially uniformly distributed in said formulation and having an average size of up to about 70 microns, and contained in said formulation in an amount ranging from between about 5 and 15 parts by weight.
Claim 5
Dependent Claim 168 words
Surface coating formulation for application to surfaces of plastic foam structures for increasing frictional and anti-slip characteristics of such surfaces, said formulation comprising: (a) as styrene/ethylene/butylene/styrene block copolymer and contained in said formulation in an amount ranging from between about 30 and 60 parts by weight; (b) finely divided silicon dioxide filler selected from the group consisting of particulate colloidal and powdered silicon dioxide and contained in said formulation in an amount ranging from between about 3 and 10 parts by weight; (c) solvent solution of methylmethacrylate copolymer solids and contained in said formulation in an amount ranging from between about 15 and 25 parts by weight; (d) rubber tackifier solids and contained in said formulation in an amount ranging from between about 5 and 15 parts by weight; and (e) glass microspheres substantially uniformly distributed in said formulation and having an average size of up to about 70 microns, and contained in said formulation in an amount ranging from between about 5 and 15 parts by weight.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-05-17 1991-11-16 1992-05-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-05-17 1995-11-16 1996-05-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-05-17 1999-11-16 2000-05-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag