Method for induction melting reactive metals and alloys

Assignee: BW/IP Inc
•
Filing: 1986-12-04
•
Granted: 1988-04-19
•
Expires: 2006-12-04
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for melting a charge of reactive metals or metal alloys is disclosed in which the charge is induction melted in a segmented crucible in the absence of insulating slag, under a non-reactive environment utilizing an induced alternating current.

Inventors

  • 👤 Donald R. Stickle
  • 👤 Shelby W. Scott
  • 👤 Donald J. Chronister

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 20:04
CPC Classifications
C; C22; C22B; C22B34/00; C22B34/30; C22B34/32; C22B34/10; C22B34/12; C22B34/1295; C22B34/14; C22B34/20; C22B34/24; C22B34/34; C22B59/00; C22B60/00; C22B60/02; C22B60/0204; C22B60/0286; C22B60/0291; C22B9/00; C22B9/003; C22B9/04; F; F27; F27B; F27B14/00; F27B14/06; F27B14/061; F27B14/063; H; H05; H05B; H05B6/00; H05B6/02; H05B6/22; H05B6/24; Y; Y02; Y02P; Y02P10/00; Y02P10/25

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 219 words
A method for induction melting a reactive metal charge in order to provide a molten metal pool for producing castings, ingots, and other products, comprising the steps of: (a) providing a crucible chamber comprised of a hollow, elongate metal structure, the elongate metal side walls of which are comprised of and made up by at least two elongate metal side wall segments, each such segment being spaced apart from any adjacent segment but all such segments nevertheless being in electrical interconnection, said crucible chamber being provided with means for cooling its outside surfaces, and at least a portion of said crucible chamber being surrounded by a primary induction coil; (b) arranging said crucible chamber in a closed environment evacuated to remove air to a pressure less than about 500 microns; (c) introducing into said crucible chamber a charge comprised of reactive metal in the absence of any intentionally added insulating slag materials such that during the melting of such charge in said crucible chamber no insulating slag layer is formed; (d) subjecting said metal charge to an alternating current flux induced by an alternating current supplied to said primary induction coil; and (e) maintaining said alternating current flux, while cooling the outer surfaces of said crucible chamber, to melt the charge and heat the molten pool in said chamber.
Claim 2
Independent Claim 219 words
A method for induction melting a reactive metal charge in order to provide a molten metal pool for producing castings, ingots, and other products, comprising the steps of: (a) providing a crucible chamber comprised of a hollow, elongate metal structure, the elongate metal side walls of which are comprised of and made up by at least two elongate metal side wall segments, each such segment being spaced apart from any adjacent segment but all such segments nevertheless being in electrical interconnection, said crucible chamber being provided with means for cooling its outside surfaces, and at least a portion of said crucible chamber being surrounded by a primary induction coil; (b) arranging said crucible chamber in a closed environment evacuated to remove air to a pressure less than about 500 microns; (c) introducing into said crucible chamber a charge comprised of reactive metal in the absence of any intentionally added insulating slag materials such that during the melting of such charge in said crucible chamber no insulating slag layer is formed; (d) subjecting said metal charge to an alternating current flux induced by an alternating current supplied to said primary induction coil; and (e) maintaining said alternating current flux, while cooling the outer surfaces of said crucible chamber, to melt the charge and heat the molten pool in said chamber.
Claim 3
Dependent Claim 16 words
The method according to claim 1 wherein said reactive metal charge consists of a titanium alloy.
Claim 4
Dependent Claim 33 words
The method according to claim 1 wherein said reactive metal charge comprises a metal selected from the group consisting of zirconium, hafnium, chromium, niobium, tantalum, molybdenum, uranium, rare-earth metals, thorium, and alloys thereof.
Claim 5
Independent Claim 279 words
A method for induction melting of a reactive metal charge in order to provide a molten metal pool for production of parts therefrom, comprising the steps of: (a) providing a crucible chamber comprised of a hollow, elongate metal structure, the elongate metal side walls of which are comprised of and made up by at least two elongate metal side wall segments, each such segment being spaced apart from any adjacent segment but all such segments nevertheless being in electrical interconnection, said crucible chamber being provided with means for cooling its outside surfaces, and at least a portion of the length of said crucible being surrounded by a primary induction coil; (b) arranging said crucible chamber in a closed environment evacuated to remove air to a pressure less than about 500 microns; (c) introducing into said crucible chamber a charge comprised of reactive metal, with the charge being essentially free of insulating slag materials, the composition of such charge of reactive metal remaining essentially slag-free and being such that there is present in said crucible, after induction melting, a pool of molten metal comprised of materials selected from the group consisting of titanium alloy, zirconium, hafnium, chromium, niobium, tantalum, molybdenum, uranium, rare-earth metals, thorium, alloys of zirconium, hafnium, chromium, niobium, tantalum, molybdenum, uranium, rare-earth metals and thorium with each other or with other metals, and mixtures thereof; (d) subjecting said metal charge to an alternating current flux induced by an alternating current supplied to said primary induction coil; and (e) maintaining said alternating current flux, while cooling the outer surfaces of said crucible chamber, to melt the reactive metal charge and to heat the molten pool in said crucible chamber.
Claim 6
Independent Claim 279 words
A method for induction melting of a reactive metal charge in order to provide a molten metal pool for production of parts therefrom, comprising the steps of: (a) providing a crucible chamber comprised of a hollow, elongate metal structure, the elongate metal side walls of which are comprised of and made up by at least two elongate metal side wall segments, each such segment being spaced apart from any adjacent segment but all such segments nevertheless being in electrical interconnection, said crucible chamber being provided with means for cooling its outside surfaces, and at least a portion of the length of said crucible being surrounded by a primary induction coil; (b) arranging said crucible chamber in a closed environment evacuated to remove air to a pressure less than about 500 microns; (c) introducing into said crucible chamber a charge comprised of reactive metal, with the charge being essentially free of insulating slag materials, the composition of such charge of reactive metal remaining essentially slag-free and being such that there is present in said crucible, after induction melting, a pool of molten metal comprised of materials selected from the group consisting of titanium alloy, zirconium, hafnium, chromium, niobium, tantalum, molybdenum, uranium, rare-earth metals, thorium, alloys of zirconium, hafnium, chromium, niobium, tantalum, molybdenum, uranium, rare-earth metals and thorium with each other or with other metals, and mixtures thereof; (d) subjecting said metal charge to an alternating current flux induced by an alternating current supplied to said primary induction coil; and (e) maintaining said alternating current flux, while cooling the outer surfaces of said crucible chamber, to melt the reactive metal charge and to heat the molten pool in said crucible chamber.
Claim 7
Dependent Claim 44 words
The method according to claim 1 or 4 wherein, prior to the subjecting of said metal charge to said alternating current flux, said vacuum is replaced with an inert gas atmosphere selected from the group of gases consisting of argon, helium, neon, and krypton.
Claim 8
Independent Claim 33 words
The method according to claims 1 or 4 wherein said products made from said molten pool are selected from the group consisting of ingots, castings, powders, foils, flakes, fibers, crystals, and granular materials.
Claim 9
Dependent Claim 14 words
The method according to claim 4 wherein said charge consists of a titanium alloy.

References Cited (Backward Citations)

US2091087A Cited
US3223519A Cited
US3014255A Cited
US3598168A Cited
US3775091A Cited
US4058668A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-04-19 1991-10-19 1992-04-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-04-19 1995-10-19 1996-04-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-04-19 1999-10-19 2000-04-19 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag