Abstract A method of making a magneto-optical recording medium comprises the steps of moving a rotating substrate along a first dielectric target, at least one rare earth metal target, and a second dielectric target which are disposed in this order from an upstream side toward the downstream side in an in-line sputtering apparatus, and carrying out simultaneous sputtering on the substrate in the course of the movement of the substrate by use of the first dielectric target and the rare earth metal target. Thereafter, sputtering is carried out on the substrate by use of the rare earth metal target. Then, simultaneous sputtering is carried out on the substrate by use of the rare earth metal target and the second dielectric target.

Inventors

  • 👤 Masaaki Nomura
  • 👤 Takashi Yamada
  • 👤 Ryoichi Yamamoto
  • 👤 Akira Nahara

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 06:17
CPC Classifications
G; G11; G11B; G11B5/00; G11B5/84; G11B5/851; C; C23; C23C; C23C14/00; C23C14/22; C23C14/56; C23C14/568; G11B11/00; G11B11/10; G11B11/105; G11B11/10582; G11B11/10586

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 163 words
A method of making a magneto-optical recording medium wherein a rotating transparent substrate is moved from an upstream side to a downstream side in an in-line sputtering apparatus, and a thin film is overlaid by sputtering on said substrate in the course of movement of said substrate, the method of making a magneto-optical recording medium comprising the steps of: (i) moving said substrate along a first dielectric target, at least one rare earth metal target, and a second dielectric target which are disposed in this order from said upstream side toward said downstream side, (ii) carrying out simultaneous sputtering on said substrate in the course of the movement of said substrate by use of said first dielectric target and said rare earth metal target, (iii) thereafter carrying out sputtering on said substrate by use of said rare earth metal target, and (iv) then carrying out simultaneous sputtering on said substrate by use of said rare earth metal target and said second dielectric target.
Claim 2
Independent Claim 163 words
A method of making a magneto-optical recording medium wherein a rotating transparent substrate is moved from an upstream side to a downstream side in an in-line sputtering apparatus, and a thin film is overlaid by sputtering on said substrate in the course of movement of said substrate, the method of making a magneto-optical recording medium comprising the steps of: (i) moving said substrate along a first dielectric target, at least one rare earth metal target, and a second dielectric target which are disposed in this order from said upstream side toward said downstream side, (ii) carrying out simultaneous sputtering on said substrate in the course of the movement of said substrate by use of said first dielectric target and said rare earth metal target, (iii) thereafter carrying out sputtering on said substrate by use of said rare earth metal target, and (iv) then carrying out simultaneous sputtering on said substrate by use of said rare earth metal target and said second dielectric target.
Claim 3
Dependent Claim 74 words
A method as defined in claim 1 wherein sputtering is carried out on said substrate by use of only said first dielectric target prior to simultaneous sputtering carried out by use of said first dielectric target and said rare earth metal target, and sputtering is carried out by use of only said second dielectric target after simultaneous sputtering is carried out by use of said rare earth metal target and said second dielectric target.
Claim 4
Dependent Claim 51 words
A method as defined in claim 1 wherein conditions of simultaneous sputtering carried out by use of said first dielectric target and said rare earth metal target are adjusted so that the thickness of a thin film formed by said simultaneous sputtering on said substrate is not larger than 200 Å.

References Cited (Backward Citations)

CA868514A Cited
US3843420A Cited
US4013830A Cited
US4022939A Cited
US4500407A Cited
US4664977A Cited
US4680742A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-04-05 1991-10-05 1992-04-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-04-05 1995-10-05 1996-04-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-04-05 1999-10-05 2000-04-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag