Patent US4731558A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4731558A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of reducing the reflectance of a transparent viewing screen and viewing screen with reduced reflectance

Assignee: US Philips Corp
•
Filing: 1986-11-03
•
Granted: 1988-03-15
•
Expires: 2006-11-03
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A viewing screen is described, in particular the screen of a display tube, which has excellent anti-reflective properties and a method of making this screen anti-reflective. In this method the outer surface of the screen is mechanically roughened in conformity with specific requirements and subsequently an anti-reflective coating of constant thickness is applied to the roughened surface.

Inventors

  • 👤 Jan Haisma
  • 👤 Johannes M. M. Pasmans
  • 👤 Pieter van der Werf
  • 👤 Albertus J. M. Rombouts

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 03:31
CPC Classifications
H; H04; H04N; H04N5/00; H04N5/64; H04N5/65; G; G02; G02B; G02B1/00; G02B1/10; G02B1/11; G02B1/113; H01; H01J; H01J29/00; H01J29/02; H01J29/10; H01J29/18; H01J29/24; H01J29/86; H01J29/89; H01J29/896; H01J2229/00; H01J2229/89; H01J2229/8913; H01J2229/8915; H01J2229/8918

Claims Analysis

Total Claims: 19
Claim 1
Independent Claim 168 words
A method of reducing the reflectance of a transparent viewing screen comprising first mechanically roughening the outer surface of the screen until the roughness parameters of the resultant roughened outer surface satisfies the following requirements 25 nm<R a <200 nm 50 nm<R q <250 nm 25 nm<R tm <1500 nm 25 μm<S m <100 μm wherein R a is the arithmetic average of the absolute difference between the surface profile and the average surface level measured along a line, R q is the square root of the average difference squared between the surface profile and the average surface level measured along a line, R tm is the peak-to-valley height difference of the surface profile averaged over a number of line intervals, and S m is the average distance between positive crossings of the surface profile and the average surface level measured along a line and then providing an anti-reflective coating on the roughened outer surface in such a manner that the thickness of the resultant coating is constant.
Claim 2
Independent Claim 168 words
A method of reducing the reflectance of a transparent viewing screen comprising first mechanically roughening the outer surface of the screen until the roughness parameters of the resultant roughened outer surface satisfies the following requirements 25 nm<R a <200 nm 50 nm<R q <250 nm 25 nm<R tm <1500 nm 25 μm<S m <100 μm wherein R a is the arithmetic average of the absolute difference between the surface profile and the average surface level measured along a line, R q is the square root of the average difference squared between the surface profile and the average surface level measured along a line, R tm is the peak-to-valley height difference of the surface profile averaged over a number of line intervals, and S m is the average distance between positive crossings of the surface profile and the average surface level measured along a line and then providing an anti-reflective coating on the roughened outer surface in such a manner that the thickness of the resultant coating is constant.
Claim 3
Dependent Claim 21 words
A method as claimed in claim 1, characterized in that the inner surface of the viewing screen is also roughened mechanically.
Claim 4
Dependent Claim 24 words
A method as claimed in claim 2, characterized in that the roughening is effected by means of loose grains on a flexible polishing base.
Claim 5
Dependent Claim 23 words
A method as claimed in claim 3, characterized in that the anti-reflective coating is formed by vapour-deposition or sputtering in a vacuum system.
Claim 6
Dependent Claim 49 words
A method as claimed in claim 4, characterized in that on the roughened outer surface of the screen a layer of magnesium-fluoride is vapour-deposited as anti-reflective coating, the vapour-deposition flow towards said outer surface being directed at an angle smaller than 15° to the normal to said outer surface.
Claim 7
Dependent Claim 28 words
A method as claimed in claim 5, characterized in that during vapour-deposition the outer surface of the viewing screen is brought at a temperature of approximately 300° C.
Claim 8
Dependent Claim 44 words
A method as claimed in claim 5, characterized in that prior to vapour-deposition the outer surface of the screen is chemically activated by subjecting it to a glow-discharge for at least 15 minutes and during vapour-deposition this outer surface is maintained at room temperature.
Claim 9
Dependent Claim 162 words
A viewing screen whose outer surface is provided with an anti-reflective coating, characterized in that at least the outer surface of the viewing screen is mechanically roughened, the roughness parameters satisfying the following requirements: 25 nm>R a >200 nm 50 nm<R q <250 nm 250 nm<R tm <1500 nm 25 μm<S m <100 μm wherein R a is the arithmetic average of the absolute difference between the surface profile and the average surface level measured along a line, R q is the square root of the average difference squared between the surface profile and the average surface level measured along a line, R tm is the peak-to-valley height difference of the surface profile averaged over a number of line intervals, and S m is the average distance between positive crossings of the surface profile and the average surface level measured along a line the anti-reflective coating on the roughened outer surface having a constant thickness and following the surface profile after roughening.
Claim 10
Dependent Claim 162 words
A viewing screen whose outer surface is provided with an anti-reflective coating, characterized in that at least the outer surface of the viewing screen is mechanically roughened, the roughness parameters satisfying the following requirements: 25 nm>R a >200 nm 50 nm<R q <250 nm 250 nm<R tm <1500 nm 25 μm<S m <100 μm wherein R a is the arithmetic average of the absolute difference between the surface profile and the average surface level measured along a line, R q is the square root of the average difference squared between the surface profile and the average surface level measured along a line, R tm is the peak-to-valley height difference of the surface profile averaged over a number of line intervals, and S m is the average distance between positive crossings of the surface profile and the average surface level measured along a line the anti-reflective coating on the roughened outer surface having a constant thickness and following the surface profile after roughening.
Claim 11
Dependent Claim 21 words
A viewing screen as claimed in claim 8, characterized in that the inner surface of the screen is also mechanically roughened.
Claim 12
Dependent Claim 54 words
A picture screen as claimed in claim 8, characterized in that the anti-reflective coating comprises a single layer whose refractive index is smaller than that of the viewing-screen material and whose optical thickness is equal to a quarter of a reference wavelength for the range of wavelengths for which the reflectance must be reduced.
Claim 13
Dependent Claim 14 words
A television picture tube provided with a viewing screen as claimed in claim 8.
Claim 14
Dependent Claim 24 words
A method as claimed in claim 2, characterized in that the roughening is effected by means of loose grains on a flexible polishing base.
Claim 15
Dependent Claim 23 words
A method as claimed in claim 2, characterized in that the anti-reflective coating is formed by vapour-deposition or sputtering in a vacuum system.
Claim 16
Dependent Claim 24 words
A method as claimed in claim 4, characterized in that the roughening is effected by means of loose grains on a flexible polishing base.
Claim 17
Dependent Claim 54 words
A picture screen as claimed in claim 9, characterized in that the anti-reflective coating comprises a single layer whose refractive index is smaller than that of the viewing-screen material and whose optical thickness is equal to a quarter of a reference wavelength for the range of wavelengths for which the reflectance must be reduced.
Claim 18
Dependent Claim 14 words
A television picture tube provided with a viewing screen as claimed in claim 9.
Claim 19
Dependent Claim 14 words
A television picture tube provided with a viewing screen as claimed in claim 10.

References Cited (Backward Citations)

US2044350A Cited
US2612611A Cited
US3504212A Cited
DE2321349A1 Cited
JPS54129873A Cited
US4410310A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-03-15 1991-09-14 1992-03-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-03-15 1995-09-14 1996-03-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-03-15 1999-09-14 2000-03-15 $7700.00 Window Closed / Lapsed