Abstract

Abstract A light-sensitive silver halide photographic material for X-ray photography characterized in that the material has the characteristic curve whose gamma between optical densities of 0.50 and 1.50 is 2.7 to 3.3 and gamma between optical densities of 2.00 and 3.00 is 1.5 to 2.5, when processed by use of the following developer: ______________________________________ Potassium sulfite 55.0 g Hydroquinone 25.0 g 1-Phenyl-3-pyrazolidone 1.2 g Boric acid 10.0 g Potassium hydroxide 21.0 g Triethylene glycol 17.5 g 5-Methylbenztriazole 0.04 g 5-Nitrobenzimidazole 0.11 g 1-Phenyl-5-mercaptotetrazole 0.015 g Glacial acetic acid 16.0 g Potassium bromide 4.0 g Add water to make up one liter. ______________________________________

Inventors

  • 👤 Akio Suzuki
  • 👤 Masatoshi Iwata
  • 👤 Katsutoshi Machida
  • 👤 Chika Honda

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 22:32
CPC Classifications
G; G03; G03C; G03C1/00; G03C1/005; G03C5/00; G03C5/16; G03C2200/00; G03C2200/58; Y; Y10; Y10S; Y10S430/00; Y10S430/167; Y10S430/168

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 180 words
A method for preparing a light-sensitive silver halide photographic material for X-ray photography comprising chemically sensitizing a monodispersed silver halide emulsion and chemically sensitizing a polydispersed silver halide emulsion, said monodispersed emulsion containing grains of a larger mean grain size than the grains of said polydispersed emulsion and then mixing said monodispersed emulsion with said polydispersed emulsion, the mean grain sizes of said polydispersed emulsion and said monodispersed emulsion are from 0.3 to 1.35 μm and the ratio of the former to the latter is 1:1.2 to 1:2.4, thereby preparing a light-sensitive silver halide photographic material having a characteristic curve whose gamma between optical densities of 0.50 and 1.50 is 2.7 to 3.3 and gamma between optical densities of 2.00 and 3.00 is 1.5 to 2.5 when processed by the following Developer-I: ______________________________________ Potassium sulfite 55.0 g Hydroquinone 25.0 g 1-Phenyl-3-pyrazolidone 1.2 g Boric acid 10.0 g Potassium hydroxide 21.0 g Triethylene glycol 17.5 g 5-Methylbenztriazole 0.04 g 5-Nitrobenzimidazole 0.11 g 1-Phenyl-5-mercaptotetrazole 0.015 g Glacial acetic acid 16.0 g Potassium bromide 4.0 g Water to make up one liter. ______________________________________
Claim 2
Independent Claim 180 words
A method for preparing a light-sensitive silver halide photographic material for X-ray photography comprising chemically sensitizing a monodispersed silver halide emulsion and chemically sensitizing a polydispersed silver halide emulsion, said monodispersed emulsion containing grains of a larger mean grain size than the grains of said polydispersed emulsion and then mixing said monodispersed emulsion with said polydispersed emulsion, the mean grain sizes of said polydispersed emulsion and said monodispersed emulsion are from 0.3 to 1.35 μm and the ratio of the former to the latter is 1:1.2 to 1:2.4, thereby preparing a light-sensitive silver halide photographic material having a characteristic curve whose gamma between optical densities of 0.50 and 1.50 is 2.7 to 3.3 and gamma between optical densities of 2.00 and 3.00 is 1.5 to 2.5 when processed by the following Developer-I: ______________________________________ Potassium sulfite 55.0 g Hydroquinone 25.0 g 1-Phenyl-3-pyrazolidone 1.2 g Boric acid 10.0 g Potassium hydroxide 21.0 g Triethylene glycol 17.5 g 5-Methylbenztriazole 0.04 g 5-Nitrobenzimidazole 0.11 g 1-Phenyl-5-mercaptotetrazole 0.015 g Glacial acetic acid 16.0 g Potassium bromide 4.0 g Water to make up one liter. ______________________________________
Claim 3
Dependent Claim 30 words
The method of claim 1, wherein the sensitized monodispersed emulsion and the sensitized polydispersed emulsion are mixed in the ratio of 2:1 to 5:1 as molar ratio of silver halide.
Claim 4
Dependent Claim 30 words
The method of claim 2, wherein the sensitized monodispersed emulsion and the sensitized polydispersed emulsion are mixed in the ratio of 3:1 to 4:1 as molar ratio of silver halide.
Claim 5
Independent Claim 162 words
A method for preparing a light-sensitive silver halide photographic material for X-ray photography comprising chemically sensitizing a monodispersed silver halide emulsion of a mean grain size of 1.15 to 1.35 μm and chemically sensitizing a polydispersed silver halide emulsion of a mean grain size of 0.55 to 0.75 μm, and mixing said sensitized monodispersed emulsion with said polydispersed emulsion in the ratio of 3:1 to 4:1 as molar ratio of silver halide, thereby preparing a light-sensitive silver halide photographic material whose gamma between optical densities of 0.50 and 1.50 is 2.7 to 3.3 and gamma between optical densities of 2.00 and 3.00 is 1.5 to 2.5, when processed by use of the following Developer-I: ______________________________________ Potassium sulfite 55.0 g Hydroquinone 25.0 g 1-Phenyl-3-pyrazolidone 1.2 g Boric acid 10.0 g Potassium hydroxide 21.0 g Triethylene glycol 17.5 g 5-Methylbenztriazole 0.04 g 5-Nitrobenzimidazole 0.11 g 1-Phenyl-5-mercaptotetrazole 0.015 g Glacial acetic acid 16.0 g Potassium bromide 4.0 g Water to make up one liter. ______________________________________
Claim 6
Independent Claim 162 words
A method for preparing a light-sensitive silver halide photographic material for X-ray photography comprising chemically sensitizing a monodispersed silver halide emulsion of a mean grain size of 1.15 to 1.35 μm and chemically sensitizing a polydispersed silver halide emulsion of a mean grain size of 0.55 to 0.75 μm, and mixing said sensitized monodispersed emulsion with said polydispersed emulsion in the ratio of 3:1 to 4:1 as molar ratio of silver halide, thereby preparing a light-sensitive silver halide photographic material whose gamma between optical densities of 0.50 and 1.50 is 2.7 to 3.3 and gamma between optical densities of 2.00 and 3.00 is 1.5 to 2.5, when processed by use of the following Developer-I: ______________________________________ Potassium sulfite 55.0 g Hydroquinone 25.0 g 1-Phenyl-3-pyrazolidone 1.2 g Boric acid 10.0 g Potassium hydroxide 21.0 g Triethylene glycol 17.5 g 5-Methylbenztriazole 0.04 g 5-Nitrobenzimidazole 0.11 g 1-Phenyl-5-mercaptotetrazole 0.015 g Glacial acetic acid 16.0 g Potassium bromide 4.0 g Water to make up one liter. ______________________________________
Claim 7
Dependent Claim 43 words
The light-sensitive silver halide photographic material for X-ray photography prepared by the process of claim 4 which has wide exposure latitude at the high density portion of said exposure and is capable of producing images of high sharpness which have high diagnostic utility.
Claim 8
Dependent Claim 35 words
The method of X-ray photography comprising imagewise exposing the light-sensitive silver halide photographic material of claim 5 to X-ray radiation to expose said material and then developing said exposed material to produce sharp photographic images.

References Cited (Backward Citations)

US3942986A Cited
US3989527A Cited
US4222777A Cited
US4446228A Cited
US4414304A Cited
US4521507A Cited
US4425426A Cited
US4425426B1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-03-15 1991-09-14 1992-03-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-03-15 1995-09-14 1996-03-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-03-15 1999-09-14 2000-03-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag