Abstract

Abstract In order to provide a structure which is not susceptible to the so called "peel-off" phenomenon which tends to occur with arrangements wherein electroluminescent layers are arranged one over the top of each other in discrete overlapping layers, and to avoid the use of yeild reducing etchants which readily attack the electroluminescent material through the inevitable pin holes and cracks which appear in the insulating layers covering the elements during the production of the panel, the light emitting elements are formed in side by side or non-overlapping relationships via a lift off technique. This obviates both the peel-off phenomenon and use of corrosive etchants.

Inventors

  • 👤 Satoshi Tanimoto

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 01:35
CPC Classifications
H; H10; H10H; H10H20/00; H10H20/80; H10H20/81; H10H20/822; H10H20/823; H10H20/8232

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 77 words
In a method of producing a polychromatic luminous panel having a plurality of electrodes and a transparent substrate, the first steps of: forming a first light emitting element that emits light of a first color on said transparent substrate using a lift off technique; and forming a second light emitting element that emits light of a second color on said transparent substrate in a non-overlapping relationship with said first light emitting element using a lift off technique.
Claim 2
Dependent Claim 77 words
In a method of producing a polychromatic luminous panel having a plurality of electrodes and a transparent substrate, the first steps of: forming a first light emitting element that emits light of a first color on said transparent substrate using a lift off technique; and forming a second light emitting element that emits light of a second color on said transparent substrate in a non-overlapping relationship with said first light emitting element using a lift off technique.
Claim 3
Dependent Claim 240 words
In a method of forming an electroluminescent panel the steps of: forming a first transparent electrode on a transparent substrate; forming a first temporary layer over said substrate; forming a first shaped aperture in said temporary layer so that the shadow of said first aperture falls on said first electrode; filling said first aperture with a first electroluminescent material that emits light of a first color; removing said first temporary layer using a lift off technique so that a first clearly defined light emitting element having the shape of said first aperture remains; forming a second temporary layer which covers at least said first light emitting element and an area surrounding same; forming a second shaped aperture in said second temporary layer in a manner that the shadow thereof falls on said first electrode in close proximity to and in a non-overlapping relationship with the shadow of said first light emitting element; filling said second aperture with a second electroluminescent material that emits light of a second color; removing said second temporary layer using a lift off technique in a manner to leave a second clearly defined light emitting element having the shape of said second aperture in close proximity to and in a side-by-side non-overlapping relationship with said first light emitting element; and forming second and third electrodes so that said second electrode overlays said first light emitting element and said third electrode overlays said second light emitting element.
Claim 4
Dependent Claim 240 words
In a method of forming an electroluminescent panel the steps of: forming a first transparent electrode on a transparent substrate; forming a first temporary layer over said substrate; forming a first shaped aperture in said temporary layer so that the shadow of said first aperture falls on said first electrode; filling said first aperture with a first electroluminescent material that emits light of a first color; removing said first temporary layer using a lift off technique so that a first clearly defined light emitting element having the shape of said first aperture remains; forming a second temporary layer which covers at least said first light emitting element and an area surrounding same; forming a second shaped aperture in said second temporary layer in a manner that the shadow thereof falls on said first electrode in close proximity to and in a non-overlapping relationship with the shadow of said first light emitting element; filling said second aperture with a second electroluminescent material that emits light of a second color; removing said second temporary layer using a lift off technique in a manner to leave a second clearly defined light emitting element having the shape of said second aperture in close proximity to and in a side-by-side non-overlapping relationship with said first light emitting element; and forming second and third electrodes so that said second electrode overlays said first light emitting element and said third electrode overlays said second light emitting element.
Claim 5
Dependent Claim 35 words
A method as claimed in claim 2, futher comprising the step of: forming a transparent insulating layer on said substrate which partially covers said first electrode before said step of forming said first temporary layer.
Claim 6
Dependent Claim 32 words
A method as claimed in claim 2, further comprising the step of: forming a transparent insulating layer over said first and second light emitting elements before forming said second and third electrodes.
Claim 7
Dependent Claim 271 words
In a method of forming an electroluminescent panel the steps of: forming a first transparent electrode on a transparent substrate; forming a first temporary layer over said substrate; forming a first shaped aperture in said temporary layer so that the shadow of said first aperture falls on said first electrode; filling said first aperture with a first electroluminescent material that emits light of a first color; removing said temporary layer using a lift off technique so that a first clearly defined light emitting element having the shape of said first aperture remains; forming an insulating layer which covers said first light emitting element and which partially covers said first electrode; forming a second temporary layer which extends at least over said first light emitting element and an area surrounding same; forming a second shaped aperture in said second temporary layer which has a shadow which falls on said first electrode in close proximity to and in a non-overlapping relationship with the shadow of said first light emitting element; filling said second aperture with a second electroluminescent material that emits light of a second color; removing said second temporary layer using a lift off technique in a manner to leave a second clearly defined light emitting element on said insulating layer which has the shape of said second aperture and which has a shadow which falls in close proximity to and in a non-overlapping relationship with the shadow of said first light emitting element; forming a second electrode on said insulating layer so as to overlay said first light emitting element; and forming a third electrode on said second light emitting element.
Claim 8
Dependent Claim 271 words
In a method of forming an electroluminescent panel the steps of: forming a first transparent electrode on a transparent substrate; forming a first temporary layer over said substrate; forming a first shaped aperture in said temporary layer so that the shadow of said first aperture falls on said first electrode; filling said first aperture with a first electroluminescent material that emits light of a first color; removing said temporary layer using a lift off technique so that a first clearly defined light emitting element having the shape of said first aperture remains; forming an insulating layer which covers said first light emitting element and which partially covers said first electrode; forming a second temporary layer which extends at least over said first light emitting element and an area surrounding same; forming a second shaped aperture in said second temporary layer which has a shadow which falls on said first electrode in close proximity to and in a non-overlapping relationship with the shadow of said first light emitting element; filling said second aperture with a second electroluminescent material that emits light of a second color; removing said second temporary layer using a lift off technique in a manner to leave a second clearly defined light emitting element on said insulating layer which has the shape of said second aperture and which has a shadow which falls in close proximity to and in a non-overlapping relationship with the shadow of said first light emitting element; forming a second electrode on said insulating layer so as to overlay said first light emitting element; and forming a third electrode on said second light emitting element.
Claim 9
Dependent Claim 259 words
In a method of forming an electroluminescent panel the steps of: forming a first transparent electrode on a transparent substrate; selecting a resist material having a thermal resistance in excess of 150° C.; forming a first temporary layer of said resist over said substrate and said transparent electrode; heating said substrate to approximately 150° C.; forming a first shaped aperture in said temporary layer so that the shadow of said first aperture falls on said first electrode; maintaining said substrate at approximately 150° C.; filling said first aperture with a first electroluminescent material that emits light of a first color; removing said temporary layer using a solution which dissolves the resist material; forming a second temporary layer of said resist which covers at least said first light emitting element and an area surrounding the same; heating said substrate to approximately 150° C.; forming a second shaped aperture in said second temporary layer in a manner that the shadow thereof falls on said first electrode in close proximity to and in a non-overlapping relationship with the shadow of said first light emitting element; maintaining said substrate at approximately 150° C.; filling said second aperture with a second electroluminescent material that emits light of a second color; removing said second temporary layer using a solution which dissolves the resist material; forming a transparent insulating layer over said first and second light emitting elements; and forming second and third electrodes so that said second electrode overlays said first light emitting element and said second third element overlays said second light emitting element.
Claim 10
Dependent Claim 259 words
In a method of forming an electroluminescent panel the steps of: forming a first transparent electrode on a transparent substrate; selecting a resist material having a thermal resistance in excess of 150° C.; forming a first temporary layer of said resist over said substrate and said transparent electrode; heating said substrate to approximately 150° C.; forming a first shaped aperture in said temporary layer so that the shadow of said first aperture falls on said first electrode; maintaining said substrate at approximately 150° C.; filling said first aperture with a first electroluminescent material that emits light of a first color; removing said temporary layer using a solution which dissolves the resist material; forming a second temporary layer of said resist which covers at least said first light emitting element and an area surrounding the same; heating said substrate to approximately 150° C.; forming a second shaped aperture in said second temporary layer in a manner that the shadow thereof falls on said first electrode in close proximity to and in a non-overlapping relationship with the shadow of said first light emitting element; maintaining said substrate at approximately 150° C.; filling said second aperture with a second electroluminescent material that emits light of a second color; removing said second temporary layer using a solution which dissolves the resist material; forming a transparent insulating layer over said first and second light emitting elements; and forming second and third electrodes so that said second electrode overlays said first light emitting element and said second third element overlays said second light emitting element.
Claim 11
Dependent Claim 261 words
In a method of forming an electroluminescent panel the steps of: forming a first transparent electrode on a transparent substrate; selecting a resist material having a thermal resistance in excess of 150° C.; forming a first temporary layer of said resist over said substrate and said transparent electrode; heating said substrate to 150° C.; forming a first shaped aperture in said temporary layer so that the shadow of said first aperture falls on said first electrode; maintaining said substrate at 150° C.; filling said first aperture with a first electroluminescent material that emits light of a first color; removing said first temporary layer using a solution which dissolves the resist material; forming an insulative layer which covers said first light emitting element and which partially covers said first electrode; forming a second temporary layer of said resist which covers at least said first light emitting element and an area surrounding the same; heating said substrate to 150° C.; forming a second shaped aperture in said second temporary layer in a manner that the shadow thereof falls on said first electrode in close proximity to and in a non-overlapping relationship with the shadow of said first light emitting element; maintaining said substrate at 150° C.; filling said second aperture with a second electroluminescent material that emits light of a second color; removing said second temporary layer using a solution which dissolves the resist material; forming a second electrode on said insulating layer so as to overlay said first light emitting element; and forming a third electrode on said second light emitting element.
Claim 12
Dependent Claim 261 words
In a method of forming an electroluminescent panel the steps of: forming a first transparent electrode on a transparent substrate; selecting a resist material having a thermal resistance in excess of 150° C.; forming a first temporary layer of said resist over said substrate and said transparent electrode; heating said substrate to 150° C.; forming a first shaped aperture in said temporary layer so that the shadow of said first aperture falls on said first electrode; maintaining said substrate at 150° C.; filling said first aperture with a first electroluminescent material that emits light of a first color; removing said first temporary layer using a solution which dissolves the resist material; forming an insulative layer which covers said first light emitting element and which partially covers said first electrode; forming a second temporary layer of said resist which covers at least said first light emitting element and an area surrounding the same; heating said substrate to 150° C.; forming a second shaped aperture in said second temporary layer in a manner that the shadow thereof falls on said first electrode in close proximity to and in a non-overlapping relationship with the shadow of said first light emitting element; maintaining said substrate at 150° C.; filling said second aperture with a second electroluminescent material that emits light of a second color; removing said second temporary layer using a solution which dissolves the resist material; forming a second electrode on said insulating layer so as to overlay said first light emitting element; and forming a third electrode on said second light emitting element.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-03-01 1991-08-31 1992-03-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-03-01 1995-08-31 1996-03-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-03-01 1999-08-31 2000-03-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags