US4728178A Expired / Lapsed US ⏱️ 0.0 years remaining

Faceted magneto-optical garnet layer and light modulator using the same

Assignee: Honeywell International Inc
•
Filing: 1986-02-20
•
Granted: 1988-03-01
•
Expires: 2006-02-20
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A magneto-optical element comprises a magnetic garnet layer on a crystalline substrate. The garnet layer has a faceted structure, which provides high Faraday rotation and controlled coercivity. The faceted structure is preferably formed by depositing the layer onto a substrate whose lattice constant is sufficiently smaller than that of the layer. The resulting elements find application in light modulators, such as switches and displays, where they permit high resolution without having to be cut into an array of small cells.

Inventors

  • 👤 Devlin M. Gualtieri
  • 👤 Paul F. Tumelty

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 20:53
CPC Classifications
G; G02; G02F; G02F1/00; G02F1/0009; G02F1/0036; H; H01; H01F; H01F10/00; H01F10/08; H01F10/10; H01F10/18; H01F10/20; H01F10/24; H01F10/245; Y; Y10; Y10S; Y10S428/00; Y10S428/90

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 86 words
A magneto-optical element comprising a magnetic garnet layer on a crystalline substrate, characterized in that the lattice constant of said garnet layer exceeds the lattice constant of the substrate by a least about 0.5%, and wherein the thickness of said garnet layer is such that the lattice constant mismatch is effective to produce stress between the substrate and said garnet layer that exceeds the critical stress whereby stress no longer increases linearly with said garnet layer thickness and garnet layer deformation becoming plastic with facets forming.
Claim 2
Dependent Claim 86 words
A magneto-optical element comprising a magnetic garnet layer on a crystalline substrate, characterized in that the lattice constant of said garnet layer exceeds the lattice constant of the substrate by a least about 0.5%, and wherein the thickness of said garnet layer is such that the lattice constant mismatch is effective to produce stress between the substrate and said garnet layer that exceeds the critical stress whereby stress no longer increases linearly with said garnet layer thickness and garnet layer deformation becoming plastic with facets forming.
Claim 3
Dependent Claim 64 words
The element of claim 1 in which the garnet layer has a composition nominally represented by the formula R 3-d (Ca, Sr) d (Fe, Ni, Co, Ga) 5-d (Si, Ge) d O 12 , where R is at least 1 element of the group consisting of Bi, Y, and the elements having atomic number from 57-71, and d is from 0 to about 1.5.
Claim 4
Dependent Claim 21 words
The element of claim 2 in which the garnet is (Bi, Y, Tm, Gd) 3 (Fe, Ga) 5 O 12 .
Claim 5
Dependent Claim 11 words
The element of claim 1 in which the substrate is GGG.
Claim 6
Dependent Claim 17 words
The element of claim 4 in which the garnet layer is on the (111) face of GGG.
Claim 7
Dependent Claim 26 words
The element of claim 1 in which the lattice constant of the garnet layer exceeds the lattice constant of the substrate by less than about 2%.
Claim 8
Dependent Claim 68 words
A light modulator comprising The magneto-optical element of claim 1 placed so that a beam of polarized light is incident on, and passes through, the layer, an analyzer placed so that the beam, after passing through the element, is incident on the analyzer, means for applying a magnetic field to the layer, and means for adjusting the magnetic field to control the light transmitted by the light modulator.
Claim 9
Dependent Claim 97 words
A process for preparing a magneto-optical element comprising depositing by liquid phase epitaxy a magnetic garnet on a crystalline substrate characterized in that the lattice constant of said garnet layer exceeds the lattice constant of the substrate by at least about 0.5%, and the deposition being conducted to a thickness of said garnet layer such that the lattice constant mismatch is effective to produce stress between the substrate and said garnet layer that exceeds the critical stress whereby stress no longer increases linearly with said garnet layer thickness and garnet layer deformation becoming plastic with facets forming.
Claim 10
Dependent Claim 97 words
A process for preparing a magneto-optical element comprising depositing by liquid phase epitaxy a magnetic garnet on a crystalline substrate characterized in that the lattice constant of said garnet layer exceeds the lattice constant of the substrate by at least about 0.5%, and the deposition being conducted to a thickness of said garnet layer such that the lattice constant mismatch is effective to produce stress between the substrate and said garnet layer that exceeds the critical stress whereby stress no longer increases linearly with said garnet layer thickness and garnet layer deformation becoming plastic with facets forming.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-03-01 1991-08-31 1992-03-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-03-01 1995-08-31 1996-03-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-03-01 1999-08-31 2000-03-01 $7700.00 Window Closed / Lapsed