Abstract In the process to form a plastic flat bottle by blowing air into an injection molded parison having a bottom, the injection blow molding method of the invention is characterized in that the thicknesses of the portions of the parison to form the front and rear faces of the flat bottle are made larger than the thicknesses of the portions of the parison to form the side end faces of the flat bottle, thereby enlarging the heat capacity in the former portions of the parison to form the front and rear faces than that of the portions of the parison to form the side end faces of the flat bottle so as to make the former portions of the parison to be expanded more easily.

Inventors

  • 👤 Katashi Aoki

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 03:31
CPC Classifications
B; B29; B29C; B29C49/00; B29C49/071; B29C2949/00; B29C2949/07; B29C2949/0715; B29C2949/072; B29C2949/0721; B29C2949/0724; B29C2949/0725; B29C2949/076; B29C2949/0761; B29C2949/0765; B29C2949/0768; B29C2949/0769; B29C2949/077; B29C2949/0772; B29C2949/0773; B29C2949/081; B29C2949/0811; B29C2949/082; B29C2949/20; B29C2949/22; B29C2949/24; B29C2949/26; B29C2949/28; B29C49/02; B29C49/06

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 223 words
A method for producing non-circular plastic bottles by injection blow molding in a non-circular mold having mold walls wherein opposing portions of said mold wall are closer to each other than other opposing portions of said mold walls, including the steps of: injection molding a parison of uniform temperature, said parison having a circular outer contour, a bottom, and a said wall wherein opposing portions of the wall of the parison have a greater wall thickness than other opposing portions of the parison wall, said thicker wall portions having a greater capacity to store heat than said thinner wall portions; positioning the parison in said blow mold so that upon expansion of the parison during blow molding, the opposing portions of the parison having greater wall thickness will contact the opposing portions of the blow mold wall closest to each other before the opposing portions of the parison having a lesser wall thickness contact the remainder of the blow mold walls; and blowing the parison so positioned into a finished bottle whereby, the thicker wall portions of the parison having more heat than the thinner wall portions will permit the remainder of the parison to extend into the remainder of the blow mold and contact the remainder of the blow mold walls to form a finished bottle having a relatively uniform wall thickness.
Claim 2
Independent Claim 223 words
A method for producing non-circular plastic bottles by injection blow molding in a non-circular mold having mold walls wherein opposing portions of said mold wall are closer to each other than other opposing portions of said mold walls, including the steps of: injection molding a parison of uniform temperature, said parison having a circular outer contour, a bottom, and a said wall wherein opposing portions of the wall of the parison have a greater wall thickness than other opposing portions of the parison wall, said thicker wall portions having a greater capacity to store heat than said thinner wall portions; positioning the parison in said blow mold so that upon expansion of the parison during blow molding, the opposing portions of the parison having greater wall thickness will contact the opposing portions of the blow mold wall closest to each other before the opposing portions of the parison having a lesser wall thickness contact the remainder of the blow mold walls; and blowing the parison so positioned into a finished bottle whereby, the thicker wall portions of the parison having more heat than the thinner wall portions will permit the remainder of the parison to extend into the remainder of the blow mold and contact the remainder of the blow mold walls to form a finished bottle having a relatively uniform wall thickness.
Claim 3
Dependent Claim 25 words
The method as claimed in claim 1 wherein said non-circular bottle is generally flat and has a cross-section generally in the shape of an ellipse.
Claim 4
Dependent Claim 25 words
The method as claimed in claim 1 wherein said non-circular bottle is generally flat and has a cross-section generally in the shape of a rectangle.
Claim 5
Independent Claim 61 words
The method as claimed in claims 2 or 3, wherein the thickness of the opposing portions of said parison to form the front and rear faces of said generally flat bottle is made larger by about 0.1 to 0.5 mm than the thickness of the opposing portions of said parison to form the side end faces of said generally flat bottle.

References Cited (Backward Citations)

US2750625A Cited
US2789312A Cited
US2792593A Cited
US3294883A Cited
US3137748A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-02-08 1991-08-10 1992-02-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-02-08 1995-08-10 1996-02-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-02-08 1999-08-10 2000-02-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag