← Back to Patent Explorer
US4717399A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for adsorbing mercury from natural gas

Assignee: Mobil Oil AS
•
Filing: 1986-12-22
•
Granted: 1988-01-05
•
Expires: 2006-12-22
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Hydrocarbon gases containing trace quantities of mercury are treated to remove the mercury by contacting the gases with a porous bed of aluminum which has been activated by contacting it with an aqueous solution of a soluble mercuric salt and subsequent drying of the activated bed in a non-oxidizing atmosphere.

Inventors

  • 👤 Costandi A. Audeh

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 22:23
CPC Classifications
C; C07; C07C; C07C7/00; C07C7/148; C07C7/14833; C07C7/14841; B; B01; B01D; B01D53/00; B01D53/34; B01D53/46; B01D53/64

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 81 words
A process for removing trace quantities of mercury from a hydrocarbon gas containing said trace quantities comprising: (a) contacting a porous mass of aluminum metal with an aqueous solution of a soluble mercuric salt; (b) drying said porous mass with a non-oxidizing gas at a temperature between about 45° and about 95° C.; and (c) subsequently contacting said porous mass with said hydrocarbon gas containing trace quantities of mercury, thereby absorbing or amalgamating said mercury onto said mass of aluminum metal.
Claim 2
Dependent Claim 81 words
A process for removing trace quantities of mercury from a hydrocarbon gas containing said trace quantities comprising: (a) contacting a porous mass of aluminum metal with an aqueous solution of a soluble mercuric salt; (b) drying said porous mass with a non-oxidizing gas at a temperature between about 45° and about 95° C.; and (c) subsequently contacting said porous mass with said hydrocarbon gas containing trace quantities of mercury, thereby absorbing or amalgamating said mercury onto said mass of aluminum metal.
Claim 3
Dependent Claim 28 words
The process of claim 1 in which the concentration of the soluble mercuric salt in the aqueous solution is between about 0.001 and about 0.5 grams per liter.
Claim 4
Dependent Claim 45 words
The process of claim 1 wherein the porous mass of aluminum metal is contacted with said aqueous solution for a period of between about 0.25 and about 1 hour at a temperature between about 65° and about 180° F. and a pressure of one atmosphere.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-01-04 1991-07-06 1992-01-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-01-04 1995-07-06 1996-01-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-01-04 1999-07-06 2000-01-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag