Patent US4714627A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4714627A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of gold deposition using volatile organogold complexes

Assignee: Idea Corp Canada
•
Filing: 1985-12-17
•
Granted: 1987-12-22
•
Expires: 2005-12-17
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method is described for depositing gold onto a target surface using volatile organogold(I) and organogold(III) complexes. The method requires the vaporization of the organogold complex under high vacuum and moderate temperature and introduction of the vaporized complex into contact with the target surface heated to a temperature at or above the decomposition temperature for the complex, so that the complex decomposes upon contacting the surface thereby depositing gold thereon. A number of new organogold complexes are described for use in the method.

Inventors

  • 👤 Richard J. Puddephatt
  • 👤 Ilse Treurnicht

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 05:55
CPC Classifications
C; C23; C23C; C23C16/00; C23C16/06; C23C16/18

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 177 words
A method for depositing gold onto a target surface, comprising: vaporizing an organogold complex under conditions of a dynamic vacuum of at least about 10 -2 mbar and moderate heating in the range of about 30° C. to about 80° C., said complex having the formula: R--Au.sup.(I) ←L or R.sub.3 Au.sup.(III) ←L wherein R may be an alkyl, alkenyl, alkynyl, aryl or aralkyl group having up to 12 carbon atoms; and L may be --CNR' or --PR" 3 wherein R' is a C 1-6 alkyl, or an aryl or aralkyl group having up to 10 carbon atoms, and R" is a C 1-3 alkyl, or aryl; heating the target surface also under a dynamic vacuum of at least about 10 -2 mbar to at least the temperature of decomposition for the organogold complex, said heating being in the range of about 100° C. to about 250° C.; and introducing the vaporized complex into contact with the heated target surface while maintaining the vacuum thereby causing decomposition of the complex and deposition of gold onto the target surface.
Claim 2
Independent Claim 177 words
A method for depositing gold onto a target surface, comprising: vaporizing an organogold complex under conditions of a dynamic vacuum of at least about 10 -2 mbar and moderate heating in the range of about 30° C. to about 80° C., said complex having the formula: R--Au.sup.(I) ←L or R.sub.3 Au.sup.(III) ←L wherein R may be an alkyl, alkenyl, alkynyl, aryl or aralkyl group having up to 12 carbon atoms; and L may be --CNR' or --PR" 3 wherein R' is a C 1-6 alkyl, or an aryl or aralkyl group having up to 10 carbon atoms, and R" is a C 1-3 alkyl, or aryl; heating the target surface also under a dynamic vacuum of at least about 10 -2 mbar to at least the temperature of decomposition for the organogold complex, said heating being in the range of about 100° C. to about 250° C.; and introducing the vaporized complex into contact with the heated target surface while maintaining the vacuum thereby causing decomposition of the complex and deposition of gold onto the target surface.
Claim 3
Dependent Claim 19 words
A method as claimed in claim 1, wherein the target surface is heated by means of a laser beam.
Claim 4
Dependent Claim 13 words
A method as claimed in claim 1, wherein the organogold complex is methyl(isocyanomethyl)gold(I).
Claim 5
Dependent Claim 13 words
A method as claimed in claim 1, wherein the organogold complex is 3,3-dimethyl-1-butynyl(isocyanomethyl)gold(I).
Claim 6
Dependent Claim 13 words
A method as claimed in claim 1, wherein the organogold complex is 1-propynyl(trimethylphosphine)gold(I).
Claim 7
Dependent Claim 13 words
A method as claimed in claim 1, wherein the organogold complex is trimethyl(trimethylphosphine)gold(III).
Claim 8
Dependent Claim 13 words
A method as claimed in claim 1, wherein the organogold complex is methyl(trimethylphosphine)gold(I).
Claim 9
Dependent Claim 13 words
A method as claimed in claim 1, wherein the organogold complex is 3,3-dimethyl-1-butynyl(trimethylphosphine)gold(I).
Claim 10
Dependent Claim 13 words
A method as claimed in claim 1, wherein the organogold complex is 1-propynyl(isocyanomethyl)gold(I).
Claim 11
Dependent Claim 41 words
A method as claimed in claim 1, wherein the organogold complex is vaporized under a dynamic vacuum of about 10 -3 mbar, with heating thereof in the range 40°-70° C., and the target surface being heated in the range 150°-200° C.
Claim 12
Dependent Claim 13 words
A method as claimed in claim 1, wherein the organogold complex is methyl(isocyanocyclohexyl)gold(I).
Claim 13
Dependent Claim 13 words
A method as claimed in claim 1, wherein the organogold complex is vinyl(isocyanomethyl)gold(I).
Claim 14
Dependent Claim 13 words
A method as claimed in claim 1, wherein the organogold complex is vinyl(isocyanotert-butyl)gold(I).

References Cited (Backward Citations)

US3657296A Cited
US3661959A Cited
US3775157A Cited
US4009297A Cited
US4526807A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-12-21 1991-06-22 1991-12-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-12-21 1995-06-22 1995-12-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-12-21 1999-06-22 1999-12-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag