← Back to Patent Explorer
US4713262A Expired / Lapsed US ⏱️ 0.0 years remaining

Manufacturing method for a magnetic recording medium

Assignee: Fujifilm Holdings Corp
•
Filing: 1986-10-02
•
Granted: 1987-12-15
•
Expires: 2006-10-02
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for manufacturing a magnetic recording medium, comprising evaporating a magnetic metal material from an evaporation source to form a vapor stream of the magnetic metal material, vapor-depositing the magnetic metal material on a tape-shaped substrate moving along a cooling can such that the incident angle (θ) of the vapor stream which is incident upon the substrate changes continuously from a high incident angle (θmax) to a low incident angle (θmin), and at the same time introducing one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas, and nitrogen oxide gas, or a mixed gas composed of oxygen gas and one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas and nitrogen oxide gas from a gas inlet part disposed at a position in the vicinity of the substrate and near the vapor stream at a low incident angle (θmin) upon the substrate, thereby providing a ferromagnetic metal film on the substrate.

Inventors

  • 👤 Tadashi Yasunaga
  • 👤 Ryuji Shirahata

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 00:27
CPC Classifications
G; G11; G11B; G11B5/00; G11B5/84; G11B5/85

Claims Analysis

Total Claims: 20
Claim 1
Independent Claim 268 words
A method for manufacturing a magnetic recording medium, comprising evaporating a magnetic metal material from an evaporation source to form a vapor stream of the magnetic metal material in a vacuum vessel, vapor-depositing the magnetic metal material on a tape-shaped substrate moving along a cooling can such that the incident angle (θ) of the vapor stream which is incident upon the substrate changes continuously from a high incident angle (θmax) to a low incident angle (θmin), and at the same time introducing one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas, and nitrogen oxide gas, or a mixed gas composed of oxygen gas and one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas and nitrogen oxide gas from a gas inlet nozzle disposed at a position in the vicinity of the substrate and near the vapor stream at a low incident angle (θmin) upon the substrate, thereby providing a ferromagnetic metal film on the substrate, wherein the gas inlet nozzle is disposed so that the ratio (R/r) of a distance (R) from the center of said cooling can to said gas inlet nozzle to the radius (r) of said cooling can is within the range of 1.10 or less, wherein a mask is disposed between the evaporation source and the tape-shaped substrate, which mask is separate from the gas inlet nozzle and which mask controls the incident angle (θ) of the vapor stream so that only vapor stream of the desired incident angle (θ) contacts the tape-shaped substrate.
Claim 2
Independent Claim 268 words
A method for manufacturing a magnetic recording medium, comprising evaporating a magnetic metal material from an evaporation source to form a vapor stream of the magnetic metal material in a vacuum vessel, vapor-depositing the magnetic metal material on a tape-shaped substrate moving along a cooling can such that the incident angle (θ) of the vapor stream which is incident upon the substrate changes continuously from a high incident angle (θmax) to a low incident angle (θmin), and at the same time introducing one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas, and nitrogen oxide gas, or a mixed gas composed of oxygen gas and one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas and nitrogen oxide gas from a gas inlet nozzle disposed at a position in the vicinity of the substrate and near the vapor stream at a low incident angle (θmin) upon the substrate, thereby providing a ferromagnetic metal film on the substrate, wherein the gas inlet nozzle is disposed so that the ratio (R/r) of a distance (R) from the center of said cooling can to said gas inlet nozzle to the radius (r) of said cooling can is within the range of 1.10 or less, wherein a mask is disposed between the evaporation source and the tape-shaped substrate, which mask is separate from the gas inlet nozzle and which mask controls the incident angle (θ) of the vapor stream so that only vapor stream of the desired incident angle (θ) contacts the tape-shaped substrate.
Claim 3
Dependent Claim 53 words
A method for manufcturing magnetic recording medium as claimed in claim 1, wherein the introduced gas comprises a gas other than oxygen gas or the gas other than oxygen gas containing oxygen gas in a mixing ratio of the oxygen gas to the other than oxygen gas of 2.0 or less by volume.
Claim 4
Dependent Claim 57 words
A method for manufacturing magnetic recording medium as claimed in claim 2, wherein the introduced gas comprises a gas other than oxygen gas or the gas other than oxygen gas containing oxygen gas in a mixing ratio of the oxygen gas to the other than oxygen gas in the range of from 0.5 to 2.0 by volume.
Claim 5
Dependent Claim 38 words
A method for manufacturing magnetic recording medium as claimed in claim 1, wherein the introduced gas is selected from the group consisting of a rare gas or a mixed gas composed of oxygen gas and a rare gas.
Claim 6
Dependent Claim 40 words
A method for manufacturing magnetic recording medium as claimed in claim 4, wherein the introduced gas is selected from the group consisting of Ar or Ne gas or a mixed gas composed of oxygen gas and Ar or Ne gas.
Claim 7
Dependent Claim 38 words
A method for manufacturing magnetic recording medium as claimed in claim 1, wherein the introduced gas is selected from the group consisting of CO 2 gas or a mixed gas composed of oxygen gas and CO 2 gas.
Claim 8
Dependent Claim 48 words
A method for manufacturing magnetic recording medium as claimed in claim 1, wherein the introduced gas is selected from the group consisting of N 2 gas or a nitrogen oxide gas, or a mixed gas composed of oxygen gas and N 2 gas or a nitrogen oxide gas.
Claim 9
Dependent Claim 40 words
A method for manufacturing magnetic recording medium as claimed in claim 7, wherein the introduced gas is selected from the group consisting of N 2 O gas, or a mixed gas composed of oxygen gas and N 2 O gas.
Claim 10
Dependent Claim 30 words
A method for manufacturing a magnetic recording medium as claimed in claim 1, wherein the gas inlet nozzle is disposed at a position nearer the cooling can than the mask.
Claim 11
Dependent Claim 57 words
A method for manufacturing magnetic recording medium as claimed in claim 1, wherein the gas inlet part is disposed so that the ratio (R/r) of a distance (R) from the center of said cooling can to said gas inlet part to the radius (r) of said cooling can is within the range of from 1.0 to 1.10.
Claim 12
Dependent Claim 53 words
A method for manufacturing a magnetic recording medium as claimed in claim 1, wherein the vapor stream passes the mask after issuing from the evaporation source, the incident angle (θ) of the vapor stream thereby being controlled by the mask, whereafter the one or more gases are introduced from the gas inlet nozzle.
Claim 13
Dependent Claim 37 words
A method for manufacturing a magnetic recording medium as claimed in claim 11, wherein the gas inlet nozzle is substantially at the point where the vapor stream is at the low incident angle (θ) upon the substrate.
Claim 14
Dependent Claim 86 words
A method for manufacturing a magnetic recording medium as claimed in claim 11, wherein the one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas and nitrogen oxide gas or a mixed gas composed of oxygen gas and one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas and nitrogen oxide gas are argon and oxygen at a mixing ratio of oxygen to argon of 0.5 to 2.0.
Claim 15
Dependent Claim 86 words
A method for manufacturing a magnetic recording medium as claimed in claim 11, wherein the one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas and nitrogen oxide gas or a mixed gas composed of oxygen gas and one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas and nitrogen oxide gas are helium and oxygen at a mixing ratio of oxygen to helium of 0.5 to 2.0.
Claim 16
Dependent Claim 88 words
A method for manufacturing a magnetic recording medium as claimed in claim 11, wherein the one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas and nitrogen oxide gas or a mixed gas composed of oxygen gas and one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas and nitrogen oxide gas are carbon dioxide and oxygen at a mixing ratio of oxygen to carbon dioxide of 0.5 to 2.0.
Claim 17
Dependent Claim 86 words
A method for manufacturing a magnetic recording medium as claimed in claim 11, wherein the one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas and nitrogen oxide gas or a mixed gas composed of oxygen gas and one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas and nitrogen oxide gas are nitrogen and oxygen at a mixing ratio of oxygen to nitrogen of 0.5 to 2.0.
Claim 18
Dependent Claim 88 words
A method for manufacturing a magnetic recording medium as claimed in claim 11, wherein the one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas and nitrogen oxide gas or a mixed gas composed of oxygen gas and one or more gases selected from the group consisting of a rare gas, CO 2 gas, N 2 gas and nitrogen oxide gas are NO 2 and oxygen at a mixing ratio of oxygen to NO 2 of 0.5 to 2.0.
Claim 19
Dependent Claim 32 words
A method for manufacturing a magnetic recording medium as claimed in claim 1, which further comprises applying a lubricant to the thus formed ferromagnetic metal film to form a lubricant layer thereon.
Claim 20
Dependent Claim 53 words
A method for manufacturing a magnetic recording medium as claimed in claim 1, wherein the gas inlet nozzle is disposed at a position in the vicinity of the substrate after the vapor stream is contacted with the tape-shaped substrate and the tape-shaped substrate is passing from a delivery roll to a wind-up roll.

References Cited (Backward Citations)

US4450186A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-12-14 1991-06-15 1991-12-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-12-14 1995-06-15 1995-12-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-12-14 1999-06-15 1999-12-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.